Impact of Crystalline Phases on Low-Activity Waste Glass Durability: Insights from PCT and VHT

During vitrification of nuclear wastes, slow cooling along the container centerline promotes crystalline phase formation, which can alter residual glass composition and reduce chemical durability. This study investigates the effects of crystalline phases on the chemical durability of low-activity waste (LAW) borosilicate glasses using the product consistency test (PCT) and vapor hydration test (VHT) on container centerline cooled (CCC) samples. A preliminary model (R2 = 0.88) was developed to predict CCC PCT responses based on glass composition, PCT data from quenched glasses, and measured crystal fractions. Using the latest LAW glass dataset, the feasibility of predictive modeling is evaluated, limitations in current data and methods are identified, and challenges for improving model accuracy are discussed to guide future data collection and model development.

borosilicate glass↗

Low Activity Waste Glass Optimization with Property Models from Machine Learning, Part 2: Experimental Validation and Active Learning

The United States Department of Energy is responsible for managing legacy nuclear waste stored in underground tanks at the Hanford Site. To treat the waste, it is planned as the current baseline to separately vitrify low-activity waste (LAW) and high-level waste fractions. Previously, machine learning (ML) based glass property models (e.g., chemical durability, viscosity, electrical conductivity and SO3 solubility) were developed with prediction uncertainties. A waste glass optimization approach was then established to enable the capability of using these ML models in LAW glass formulation. In this study, the previous ML models were first experimentally validated, and the results were incorporated back into the database to update the ML models. The updated models and formulations showed increased waste loading while reducing the failure rate, demonstrating improved predictive accuracy, reduced uncertainties, and the effectiveness of active learning in guiding high-dimensional, nonlinear LAW glass design. This represents the first experimental validation of ML based LAW glass formulation, with practical benefits such as higher waste loading, shorter mission duration, and lower operational risk.

Lu, Xiaonan (ORCID:0000000179708148)↗

Glass formulation and lab-scale testing of glasses designed for in-can Melter and in-container Vitrification of high-assay low-enriched uranium aqueous polishing Raffinate waste

Glasses were designed for processing a nuclear waste from aqueous polishing of high-assay low-enriched uranium using either In-Can Melter (ICM) or GeoMelt® In-Container Vitrification™ (ICV) technologies, which operate at temperatures of T p ≤ 1100 °C and T p ≤ 1450 °C, respectively. Due to the different operating conditions, the melt and glass properties were optimized differently for each technology. Each glass was designed to optimize for maximum waste loading while simultaneously satisfying processing (e.g., crystallization, viscosity, and conductivity) and product quality (e.g., durability, hazard characteristic, and crystal content) constraints. Here, the raffinate waste contains high nitric acid (4 M) and low total solids (9 g·L -1 ) concentrations. Feed preparation processes were tested to facilitate concentration and nitrate destruction/removal while controlling redox of the melter feed. A successful feed process including sugar addition and spray-drying was performed to generate an adequate melter feed for ICV processing.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Durability testing of actual Hanford waste glasses and their non-radioactive simulant glasses

The low-activity waste (LAW) fraction of Hanford tank waste will be converted to glass at the Waste Treatment and Immobilization Plant (WTP) and disposed on the Hanford site. The chemical durability of LAW glasses has been researched for decades to satisfy contract requirements. Most LAW glass durability data has been generated on non-radioactive simulant glasses fabricated via crucible melts. These non-radioactive glasses were chosen due to safety and cost reasons with confidence that radioactive waste glasses would exhibit similar behavior. To reduce the risk of significant differences in laboratory test response data between WTP melter waste glass and simulant glass, Product Consistency Tests (PCT, i.e., ASTM C1285-21) and Environmental Protection Agency (EPA) 1313 durability tests were performed on actual and simulant LAW glasses fabricated using laboratory-scaled melters. Actual and simulant glass durability test results are presented and statistically compared. Finally, differences in test responses were found to be within experimental uncertainty.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

ISG-2: properties of the second International Simple Glass

Given the importance of glass materials to society, their durability when exposed to aqueous solutions is a critical area for research, particularly for vitrified radioactive wastes. This spurred an international team to fabricate a standardized composition based on waste immobilization glass called the International Simple Glass (ISG), which has been the subject of numerous experimental and computational studies focused on aqueous corrosion resistance. With the original batch of ISG nearly depleted, the international team designed and fabricated a standard glass material, ISG-2, where half the Ca in the original composition was replaced with Mg by mole. This paper presents information on both the ISG-2 composition and a new batch with the same nominal composition as the original ISG, designated ISG-1, including their homogeneity, their physical and thermal properties. The results of static alteration experiments are presented as well to provide a baseline for future aqueous corrosion performance investigations.

36 MATERIALS SCIENCE↗

The effect of metals on zeolite crystallization kinetics with relevance to nuclear waste glass corrosion

Abstract Geologic disposal of vitrified radioactive material is planned in several countries, but there are remaining uncertainties related to the long-term stability of glass exposed to groundwater. Specifically, the crystallization of aluminosilicate zeolite minerals can accelerate the rate at which glass corrodes and radioactive material is released into the biosphere. In this study, we identify elemental species that may accelerate or suppress zeolite formation using a protocol to examine their effects on zeolite synthesis over a three-day duration. Our results are consistent with previous works demonstrating glass corrosion acceleration in the presence of calcium. Furthermore, we identify two elements—tin and lithium—as inhibitors of zeolite P2 (gismondine, or GIS type) nucleation and, thus, promising components for promoting the long-term durability of glass waste forms.

36 MATERIALS SCIENCE↗

Predicting initial dissolution rates using structural features from molecular dynamics simulations

Predicting chemical durability of glass materials is important for various applications from daily life such as drink glass and kitchen ware to advanced technologies such as nuclear waste disposal and biomedicine. In this work, we explored prediction of initial dissolution rate through structural features from molecular dynamics (MD) simulations for a wide range of glass compositions (total 28) including borosilicate and aluminosilicate glasses, ZrO 2 -containing and V 2 O 5 -containing boroaluminosilicate glasses. The initial dissolution rates (r 0 ) measured experimentally at 90 °C with varying solution conditions were correlated with structural features (e.g., polyhedral linkages and non-bridging oxygen species) obtained from MD simulations, either from this study or from literature. Since hydrolysis of the glass network through breaking of the network former linkages (e.g., Si-O-Si, Si-O-Al, etc.) is a critical step of network glass dissolution, the statistics of these linkages obtained from MD were correlated to r0 through linear regression, where the coefficient of determination (R 2 ) and root mean square error are found to be 0.949 and 0.681, respectively. This model was compared and discussed with existing models developed by various approaches including machine learning, the kinetic rate equation, topological constraint theory, and other descriptors from MD simulations. The discussion provides insights on future model improvements to predict glass dissolution. In addition, the impact of V 2 O 5 on the glass dissolution was examined in detail, implicating that the impact is not the same across all glass compositions and test conditions.

36 MATERIALS SCIENCE↗

Effects of Al:Si and (Al+Na):Si ratios on the static corrosion of sodium‐boroaluminosilicate glasses

Abstract Understanding alteration mechanisms of borosilicate glasses in aqueous media is essential to nuclear waste performance assessments to ensure radioisotopes are contained for extended durations. Aluminum is typically added to glass compositions to reduce the extent of alteration. However, previous work on 7‐day durability tests has suggested that Al has a nonlinear relationship with extent of alteration. The effects of Al:Si and (Al+Na):Si substitutions on glass durability were evaluated using series of glasses based on the International Simple Glass corroded in static conditions up to 13 months in deionized water at 90°C. The alteration behavior was determined by measurement of element release in solution. The ⁓7‐day alteration trends across the series were consistent with predicted trends. The 13‐month results indicated overall alteration decreased as Al:Si ratios increased and was unaffected by changes in (Al+Na):Si except for the glass with the highest (Al+Na):Si ratio (ISG‐A23N), which completely altered within 14 days. Frequent sampling and in situ Raman measurements of solutions revealed ISG‐A23N experienced several distinguishable alteration rate regimes within 7 days, forming a ⁓100 µm alteration layer and a NaSiAlO 4 zeolite.

Reiser, Joelle T.↗

Effects of Al:Si and (Al+Na):Si Ratios on the Properties of the International Simple Glass, Part II: Structure

High-alumina containing high-level waste (HLW) will be vitrified at the Waste Treatment Plant at the Hanford Site. The resulting glasses, high in alumina, will have distinct composition-structure-property (C-S-P) relationships compared to previously studied HLW glasses. These C-S-P relationships determine the processability and product durability of glasses and therefore must be understood. The main purpose of this study is to understand the detailed structural changes caused by Al:Si and (Al+Na):Si substitutions in a simplified nuclear waste model glass (ISG, International Simple Glass) by combining experimental structural characterizations and molecular dynamics (MD) simulations. The structures of these two series of glasses were characterized by neutron total scattering and 27Al, 23Na, 29Si, and 11B solid-state nuclear magnetic resonance (NMR) spectroscopy. Additionally, MD simulations were used to generate atomistic structural models of the borosilicate glasses and simulation results were validated by the experimental structural data. Short-range (e.g., bond distance, coordination number, etc.) and medium-range (e.g., oxygen speciation, network connectivity, polyhedral linkages) structural features of the borosilicate glasses were systematically investigated as a function of the degree of substitution. The results show that bond distance and coordination number of the cation-oxygen pairs are relatively insensitive to Al:Si and (Al+Na):Si substitutions with the exception of the B-O pair. Additionally, the Al:Si substitution results in an increase of tri-bridging oxygen species, while (Al+Na):Si substitution creates non-bridging oxygen species. Charge compensator preferences were found for Si-[NBO] (Na+), [3]B-[NBO] (Na+), [4]B (mostly Ca2+), [4]Al (nearly equally split Na+ and Ca2+), and [6]Zr (mostly Ca2+). The network former-BO-network former linkages preferences were also tabulated; Si-O-Al and Al-O-Al were preferred at the expense of lower Si-O-[3]B and [3]B-O-[3]B linkages. These results provide insights on the structural origins of property changes such as glass transition temperature caused by the substitutions, providing a basis for future improvements of theoretical and computer simulation models.

Lu, Xiaonan↗

Effects of Al:Si and (Al + Na):Si ratios on the properties of the international simple glass, part I: Physical properties

Understanding composition-structure-property relationships of high-alumina nuclear waste glasses are important for vitrification of nuclear waste at the Hanford Site. Two series of glasses were designed, one with varying Al:Si ratios and the other with (Al+Na):Si ratios based on the International Simple Glass (ISG, a simplified nuclear waste model glass), with Al2O3 ranging from 0 to 23 mol % (0 to 32 wt. %). The glasses were synthesized and characterized using electron probe microanalysis, X-ray photoelectron spectroscopy, small angle X-ray scattering, high temperature oxide melt solution calorimetry, and infrared spectroscopy. Glasses were crystal free, and the lowest Na2O and Al2O3 glass formed an immiscible glass phase. Evolution of various properties - glass transition temperature, percentage of 4-coordinated B, enthalpy of glass formation - and infrared spectroscopy results indicate that structural effects differ based on the glass series.

Nuclear Waste Glass↗

Acceleration of Glass Alteration Rates Induced by Zeolite Seeds at Controlled pH

As the glass-water reaction proceeds, certain glass compositions undergo a delayed acceleration in the alteration rate – a phenomenon that is commonly referred to as Stage III behavior – which generally coincides with zeolite formation. However, studying Stage III in the laboratory is difficult because the time scale required to observe Stage III behavior can vary from months to several years, and the solution conditions that initiate this acceleration remain poorly understood. Consequently, the development of a corrosion test method capable of quantifying Stage III rates in a timely manner would be of great benefit to both the scientific community and policy makers concerned with nuclear waste disposal. In this work, we induced and measured the acceleration in the corrosion rate of the AFCI glass by seeding static corrosion tests with zeolite Na-P2 at fixed pH90°C values ranging from 9.5 to 11.5. The induced Stage III rates increased linearly with increasing pH and were measured to be between the forward and residual rates of AFCI. Tests designed to compare induced Stage III rates obtained for different seeding times showed that the induced Stage III rates were faster in the absence of an alteration layer. In summary, the use of the seeded test method allows for a conservative quantification of Stage III rates in a relatively short, one-month time period.

Neeway, James J.↗