Search NASA⌕ Search

Engineering topics

Rigatti, Amy

Publications and source records attributed to Rigatti, Amy.

Broadband 920-nm mirror thin film damage competition

The 2023 Laser Damage conference thin-film damage competition was devoted to a survey on the state-of-the-art broadband near-IR multilayer dielectric (MLD) mirrors designed for ultra-short pulsed laser applications. The requirements for the coatings were a minimum reflection of 99.5% at 45-deg incidence angle for S-polarization from 830 nm to 1010 nm and group delay dispersion (GDD) < ± 50fs 2 . The participants were allowed to select the coating materials, coating design, and coating deposition method. Samples were damage tested at a single testing facility to enable direct comparison among the participants using a 25 ± 5 fs optical parametric chirped-pulse amplification (OPCPA) laser system operating at 5 Hz. The testing results from this set of 37 samples showed that dense coatings by ion-beam sputtering (IBS), magnetron sputtering (MS), and electron-beam ion assisted deposition (e-beam IAD) exhibited highest damage initiation onset (laser-induced damage threshold or LIDT) while e-beam coatings were low performers. In addition, multilayer coatings using tantala and/or hafnia as high index materials were top performers. Furthermore, this competition included for the first time the measurement of the damage growth onset (laser-induced damage growth threshold or LDGT). This latter performance metric plays an important role in establishing the safe operational conditions for larger aperture ultrashort pulsed lasers. Information pertaining to the morphology of the damage sites and their evolution under subsequent exposure to different laser fluences leading to damage growth is presented. Finally, not all coating samples in the survey met the GDD requirements stated above and associated measurements are discussed in the context of the present and past thin-film damage competitions focused on similar broadband near-IR MLD coatings.

23 broadband high reflectors↗

Broadband, 920-nm mirror thin film damage competition

This year’s competition proposed to survey the state-of-the-art broadband, near-IR multilayer dielectric (MLD) mirrors designed for ultra-short, pulsed laser applications. The requirements for the coatings were a minimum reflection of 99.5% at 45-degree incidence angle for S-polarization from 830 nm to 1010 nm and group delay dispersion (GDD) < ± 50 fs 2 . The participants in this effort selected the coating materials, coating design, and deposition method. Samples were damage tested at a single testing facility to enable direct comparison among the participants using a 25 ± 5 fs OPCPA laser system operating at 5 Hz. A double blind test assured sample and submitter anonymity. The damage performance results, sample rankings, details of the deposition processes, coating materials and substrate cleaning methods are shared here. We found that multilayer coatings using tantala and/or hafnia as high index materials were top performers within several coating deposition groups. Specifically, dense coatings by ion-beam sputtering (IBS), magnetron sputtering (MS), and electron-beam ion assisted deposition (e-beam IAD) exhibited highest damage initiation onset (LIDT) while e-beam coatings were low performers. In addition, damage growth onset (LDGT) was also examined and the results are reported here for all samples as this performance metric plays an important role in establishing the safe operational conditions for larger aperture, ultrashort pulsed lasers. As a result, not all coating samples in the survey met the GDD requirements stated above and associated measurements are discussed in the context of the present and past competitions focused on similar broadband, near-IR MLD coatings.

42 ENGINEERING↗

Power balancing a multibeam laser

Multibeam lasers often require an output beam balance that specifies the degree of simultaneity of the laser output energy, instantaneous power, or instantaneous irradiance (power per unit area). Here, this work describes the general problem of balancing a multibeam laser. Specific techniques used to balance the output power of the 60-beam pulsed OMEGA Laser System are discussed along with a measured reduction of beam-to-beam imbalance. In particular, the square-pulse distortion induced by a simple saturating amplifier operating with its output at some fraction of its saturation fluence is derived, and a method to exchange gain between saturated amplifiers in a single beam that have different saturation fluences to adjust balance is described.

47 OTHER INSTRUMENTATION↗

Power balance on a multibeam laser

Inertial confinement fusion (ICF) cryogenic experiments on the 60-beam OMEGA laser have strict requirements for the laser energy delivered on target to be power balanced in order to maximize target-irradiation uniformity. For OMEGA, this quantity (power balance) is inferred from measurements of the time-integrated energy and time-resolved, spatially integrated temporal profile of each of the 60 beams at the output of the laser. The work presented here proposes a general definition of power balance as measured at the laser output and discusses the conditions that are fundamental to achieving laser power balance. Power balance necessitates equal gain across all stages of amplification, equal net losses across each amplifier stage, equal frequency conversion (from 1053 nm to 351 nm) of all 60 beams, and equal beam path lengths (beam timing). Typical OMEGA ICF laser pulse shapes consist of one or more short (100-ps) “pickets” followed by a shaped “drive” pulse of 1 to 2 ns. For these experiments, power balance is assessed for the pickets and the drive independently, with the ultimate goal of achieving root-mean-square (rms) imbalance across all 60 beams of less than 2% rms on both. Our work presents a comprehensive summary of laser shot campaigns conducted to significantly improve laser power balance from typical rms values of 4.7% and 5.2%, respectively, to the 3% level for both features along with a discussion of future work required to further reduce the rms power imbalance of the laser system.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Shape dependence of laser–particle interaction-induced damage on the protective capping layer of 1 ω high reflector mirror coatings

The response of a potential candidate protective capping layer (SiO 2 or Al 2 O 3 ) to laser exposure of 1 ω (1053 nm) to high-reflector silica-hafnia multilayer coatings in the presence of variously shaped Ti particles is investigated by combining laser damage testing and numerical modeling. Each sample is exposed to a single oblique angle (45°) laser shot (p-polarization, ~10 J/cm 2 , 14 ns) in the presence of spherically or irregularly shaped Ti particles on the surface. The two capping layers show markedly different responses. For the spherical particles, the Al 2 O 3 cap layer exhibits severe damage, with the capping layer becoming completely delaminated at the particle locations. The SiO 2 capping layer is only mildly modified by a shallow depression, likely due to plasma erosion. The different response of the capping layer is attributed to the large difference in the thermal expansion coefficient of the materials, with that of the Al 2 O 3 about 15 times greater than that of the SiO 2 layer. For the irregular particles, the Al 2 O 3 capping layer displays minimal to no damage while the SiO 2 capping layer is significantly damaged. In conclusion, the difference is due to the disparity in mechanical strength with Al 2 O 3 possessing approximately 10 times higher fracture toughness.

1053 nm↗