Irradiation performance of a U-7Mo in Al-Si matrix dispersion full-size fuel plate assembly

The Korea Atomic Energy Research Institute (KAERI) is leading the Ki-Jang Research Reactor (KJRR) project with the intent to develop a new reactor for medical isotope production and other nuclear research purposes. The KJRR core is designed to use high density fuel system where uranium alloyed with 7 wt% molybdenum (U-7Mo) particles are dispersed in a matrix of aluminum alloyed with 5 wt% silicon (Al-5Si) and clad in aluminum alloy 6061 (Al-6061) to form fuel plates. KAERI developed a fabrication facility to construct KJRR fuel assemblies and partnered with the Idaho National Laboratory (INL) to irradiate a full-size fuel assembly, with 21 total fuel plates, in the Advanced Test Reactor (ATR). Irradiation testing and subsequent Post Irradiation Exam (PIE) campaigns were performed successfully over a multi-year project. Monte Carlo neutronic calculations, coupling with a depletion code, were performed based on ATR’s as-run power history which showed that the highest power plate (plate 20) reached 83.1 % end-of-life (EOL) local burnup based on initial 235 U content. Additionally, finite element thermal modeling was performed based as-run power history which showed a beginning-of-life (BOL) peak local heat flux of 184 W/cm 2 . No anomalous fuel performance was observed during the irradiation and target test conditions were achieved. PIE showed favorable performance of the fuel assembly regarding all important phenomena. This paper describes the KJRR fuel assembly irradiation conditions and PIE data to support the conclusion that it performed well, without evidence of unexpected or problematic fuel performance, within an irradiation test designed to bound the KJRR design environment.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Contributions to the mechanistic understanding of the microstructural evolution in irradiated U-Mo dispersion fuel

Here, advanced microstructural characterization techniques, such as scanning electron microscopy (SEM) and scanning transmission electron microscopy - energy dispersive x-ray spectroscopy (STEM-EDS), were used to interpret the fuel microstructure evolution and fission products behavior in U-Mo dispersion fuel irradiated in the Advanced Test Reactor (ATR) as part of the European Mini-Plate Irradiation Experiment (EMPIrE) test. The larger as-fabricated fuel grain size achieved by heat-treating the U-Mo powder resulted in slower high burnup structure (HBS) development and reduced fission gas porosity. Slower HBS kinetics was observed at the fuel kernels’ periphery, which contained smaller and less fission gas bubbles at all fission densities (FDs) investigated and was attributed to a locally reduced damage density and fission products concentration, as corroborated with Monte Carlo simulations. The non-refined grains at the fuel kernel periphery hosted a perfectly ordered fission Gas Bubble Superlattice (GBS) up to 6.3 × 10 21 fissions/cm 3 . Nano-scale STEM-EDS analysis presented in this study provided useful information on the GBS characteristic morphology and evolution in U-Mo fuel. The concentration of fission gas in the GBS progressively increased with FD, pointing to an evolution of the nanobubble pressure status with irradiation. A possible connection between the GBS collapse and HBS onset is proposed for which there exists a threshold in the misorientation of the refined sub-grains above which the GBS stability during irradiation is no longer preserved, resulting in the GBS collapse.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Evidence of Xe-incorporation in the bubble superlattice in irradiated U-Mo fuel

For years, researchers have reported competing ideas on the formation of fission gas bubble super lattices in metallic fuels, which was postulated to be comprised of elemental xenon (Xe) atoms. However, the chemical and physical arrangement of these elements within this gas bubble superlattice has not been verified. In this contribution, Xe was chemically profiled using atomic resolution scanning transmission electron microscopy (STEM) and atom probe tomography (APT) techniques in irradiated uranium-molybdenum (U-Mo) fuels. These complementary techniques provide conclusive evidence of Xe presence in bubble superlattice up to fission densities of 4.5×10 21 fissions/cm 3 and provide quantitative assessment of Xe content within the bubble superlattice. Based on the results of simultaneous imaging and spectroscopy using STEM, the chemical composition of the Xe bubble superlattice present in fission densities less than 4.5x10 21 fissions/cm 3 in U-Mo fuel was measured and found to be up to 8±1.3 atomic %. APT data complements STEM findings on Xe distribution in irradiated U-Mo fuel sample. APT showed a chemical composition of 0.7±0.1 atomic%. Finally, this study concludes by providing conclusive evidence that Xe is not only present within an atomically arranged bubble superlattice but provides fundamental insight the physical state of Xe in low enriched U-Mo monolithic fuel.

36 MATERIALS SCIENCE↗

An investigation of the failure modes in U-10Mo monolithic fuel irradiated to high burnup

Here, this study investigated possible failure mode sequences in U-10Mo monolithic fuel irradiated to very-high-burnup. The U-Mo fuel plate used in this study was characterized using scanning electron microscopy (SEM), wavelength dispersive spectroscopy (WDS), and image analysis techniques to investigate how microstructural features may initiate crack formation and propagation through the microstructure, potentially leading to blistering. Distinctly large fission gas pores (FGPs) were observed to preferentially align 5-15µm away from the U-10Mo/Zr interface, parallel to the Zr diffusion barrier. Preferential growth, alignment, and interconnection of FGP could initiate blistering in the fuel plate by creating a fission gas channel, parallel to the U-Mo/Zr interface. FGP alignment in the fuel phase near the U-Mo/Zr interface is believed to be one of the precursors to crack and Type 2 blister formation in monolithic U-Mo fuels. The chemical maps revealed differences in fission product behavior near the U-Mo/Zr interface such that Nd remains in the fuel matrix at the FGP sites. On the other hand, other fission products like Xe and Cs can get trapped in FGPs by Nd in the fuel phase and/or diffuse toward the Zr diffusion barrier.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Non-destructive analysis of swelling in the EMPIrE fuel test

The European Mini-Plate Irradiation Experiment (EMPIrE) was designed to support the development and testing of a coated uranium-molybdenum (U-Mo) dispersion fuel for the conversion of select high-performance research reactors (HPRRs) to utilize low-enriched uranium (LEU). To aid in the development of the coated fuel form, the EMPIrE test included several plate designs and irradiated them in the Idaho National Laboratory (INL) Advanced Test Reactor (ATR) at a high meat power density (~21 kW/cm 3 ) and to high fuel particle fission densities (~6.4 × 10 21 fissions/cm 3 ). These conditions mimic the bounding conditions of the BR-2 reactor in Belgium, where a concurrent irradiation experiment was performed, and exceed those previously explored in dispersion U-Mo fuel plates. A local fuel swelling analysis, as determined through high-fidelity, post-irradiation mini-plate profilometry, was used along with statistical methods to non-destructively evaluate the overall performance and separate the effects of convoluted fabrication variables. While some effects observed with this non-destructive analysis were subtle, others had more significant, and possibly competing, effects on the fuel swelling behavior. In closing, these observations will be examined further with destructive examinations to more fully assess them as the fuel design is developed and qualified.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microstructural characterization of as-fabricated monolithic plates with boron carbide, aluminum boride, and zirconium boride burnable absorbers

The use of burnable absorbers can be beneficial for nuclear reactors by extending the fuel’s operational cycle, providing additional criticality control, and flattening the power profile. In this work, three burnable absorber materials (boron carbide, aluminum boride, and zirconium boride) embedded in aluminum have been fabricated into foils and clad in AA-6061 for potential use in high performance research reactors. The as-fabricated boron-containing phases were determined using transmission electron microscopy to be AlB2, B4C, and ZrB2. TEM also revealed weak bonding at the B4C-matrix interface. SEM showed a relatively uniform spatial distribution of boron-containing phases for all the candidate materials. Higher porosity was observed in the foil containing ZrB2 in its as-rolled condition. The porosity in the ZrB2 foil was reduced by hot isostatic pressing. The size and shape distributions of the boron-containing phases were analyzed on the criteria of cross-sectional area, perimeter, roundness, circularity, and aspect ratio. A method of converting the 2D burnable absorber dispersoids seen in cross-sectional microscopy images into 3D volumes was derived using both spherical and ellipsoidal geometry models. The difference in calculated burnable absorber dispersoid average volume between the two models ranges from 20% to 100%, which could impact burnable absorber burnout rates due to differences in neutron self-shielding.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

The use of U3Si2/Al dispersion fuel for high power research reactors

In order to investigate the irradiation performance of U3Si2/Al dispersion fuel at relatively aggressive reactor conditions, compared to how this fuel is typically used in a research or test reactor, post irradiation examination was performed on two fuel plates that were irradiated at ~270 W/cm2 average surface heat flux and to a maximum local burnup greater than 8 × 1021 fissions/cm3 in the Advanced Test Reactor as part of the RERTR-8 experiment. As part of the non-destructive examinations that were performed on both fuel plates, detailed thickness measurements using a high-fidelity measurement bench were performed on one fuel plate and a segment of the second fuel plate. This paper provides the first reported results of such high-resolution thickness measurements for U3Si2/Al dispersion fuel plates, containing primarily the U3Si2 fuel phase, irradiated at such power levels to high burnup. For destructive examination using optical metallography, samples were generated from both irradiated plates. Localized regions of high swelling (characteristic of internal blistering) were observed on the surface of both fuel plates, suggesting that the performance limits had been reached for each plate. Destructive examinations showed that the fuel particles that are primarily U3Si2, which become amorphous during irradiation, in both plates contained relatively large fission gas bubbles with evidence of fission gas bubble interconnection.

Wachs, Daniel M.↗

Effects of irradiation on the interface between U-Mo and zirconium diffusion barrier

Irradiated fuel plates were characterized by microscopy that focused on the interface between U–Mo and Zr. Before irradiation, there were three major sub-layers identified in the U–Mo/Zr interface, namely, UZr 2 , Mo 2 Zr, and U with low Mo. The typical total thickness of this U–Mo/Zr interaction is 2–3 microns. The UZr 2 sub-layer formed during fuel fabrication remains stable after irradiation, without large bubbles/porosity accumulation. However, this sub-layer becomes increasingly discontinuous as burnup increases. The low-Mo sub-layer exhibits numerous sub-micron bubbles/porosity at low burnup. Larger, interconnected porosity in this sub-layer was observed in a medium-burnup fuel specimen. However, at higher burnup, regions with the extra-large bubbles/porosity (i.e., larger than 5 ?m) were observed at least 5 microns away from the original location of this sub-layer. The mechanism for the formation of the extra-large bubbles/porosity is still unclear at this time. In general, the U–Mo/Zr interface in monolithic U–Mo fuels is relatively stable after irradiation. As a result, no large detrimental defects, such as large interfacial bubbles or cracks/delamination, were observed in the fuel plates characterized.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Microstructural characterization of an irradiated RERTR-6 U-7Mo/AA4043 alloy dispersion fuel plate specimen blister-tested to a final temperature of 500°C

The Material Management and Minimization (M3) Reactor Conversion Program, in the past called the Reduced Enrichment for Research and Test Reactor (RERTR) Program, is developing low-enriched uranium (LEU) fuels for application in research reactors. U–Mo alloy dispersion fuel is one type being developed. Blister testing has been performed on different fuel plate samples to determine the margin to failure for fuel plates irradiated to different fission densities. Microstructural characterization was performed using scanning electron microscopy and transmission electron microscopy on a sample taken from a U-7Mo/AA4043 matrix dispersion fuel plate irradiated in the RERTR-6 experiment that was blister-tested up to a final temperature of 500°C. The results indicated that two types of grain/cell boundaries were observed in the U- 7Mo fuel particles, one with a relatively low Mo content and fission gas bubbles and a second type enriched in Si, due to interdiffusion from the Si-containing matrix, with little evidence of fission gas bubbles. With respect to the behavior of the major fission gas Xe, a significant amount of the Xe was still observed within the U-7Mo fuel particle, along with microns into the AA4043 matrix. For the fuel/matrix interaction layers that form during fabrication and then grow during irradiation, they change from the as-irradiated amorphous structure to one that is crystalline after blister testing. In the AA4043 matrix, the original Si-rich precipitates, which are typically observed in as-irradiated U-Mo dispersion fuel, get consumed due to interdiffusion with the U-7Mo fuel particles during the blister test. Lastly, the fission gas bubbles that were originally around 2 nm in diameter and resided on a fission gas superlattice in the intragranular regions of as-irradiated U-7Mo fuel grew in size (up to ~20 nm diameter) during blister testing.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Monolithic U-10Mo Fuel Development for U.S. High Performance Research Reactors

To support the U.S Department of Energy (DOE), National Nuclear Security Administration (NNSA) mission to reduce the threat posed by the civilian use of highly enriched uranium (HEU) worldwide, the US High Performance Research Reactor (US HPRR) fuel development program is pursuing development and qualification of a new high-density monolithic U-Mo fuel to facilitate conversion of five higher power research reactors located in the U.S. (ATR, HFIR, NBSR, MIT and MURR) and one critical facility (ATR-C) from HEU to low enriched uranium (LEU). These reactors require higher uranium fuel density than is achievable with dispersion fuel systems used to convert lower power research reactors. The down selected fuel system consists of U-10Mo alloy fuel foils having a thin Zr diffusion barrier interlayer, clad in 6061 Al alloy by hot isostatic pressing. In order to support fabrication development, fuel performance evaluations, generic fuel qualification through the Nuclear Regulatory Commission (NRC), and eventual reactor licensing, a series of irradiation experiments and testing campaigns are being planned. The tests are designed to provide data needed for fabrication process down selection, to establish acceptable fuel performance under normal operating conditions and anticipated transients, and to demonstrate successful scale-up to prototypic reactor-specific fuel element designs. A comprehensive testing program is being executed as part of the US HPRR fuel development program to develop and qualify a new monolithic UMo fuel system to allow conversion of five high power research reactors and one critical facility within the US in support of the NNSA mission to convert research reactors worldwide from HEU to LEU fuels. A significant outcome of this program will be the qualification and eventual licensing of a new plate-type fuel system for use in research reactors through the NRC for the first time in nearly 3 decades. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

The Impact of Furnace-Testing on the Microstructure of an Irradiated U-Mo Fuel Plate

The Material Management and Minimization Program (formerly known as the Reduced Enrichment for Research and Test Reactor Program) is responsible for converting research reactors that use highly enriched uranium (HEU) fuels to ones that use low-enriched uranium (LEU) fuels. As part of the development of LEU fuels, a variety of irradiation experiments are being conducted using the Advanced Test Reactor. In addition to the reactor tests, there is interest in generating information about the transient behavior of irradiated fuel plates. For example, it is of interest to determine the temperature at which a blister will form on the surface of a fuel plate, due to fission gas release from the fuel meat, for a particular fuel plate design. Since in-pile testing to determine the 'blister threshold' (the temperature where a blister forms on the surface of a fuel plate) in plate-type fuel is very difficult and expensive and has historically been deemed impractical for fuel qualification testing, an out-of-pile 'blister test' has been developed and employed. This post-irradiation blister anneal test was developed as a conservative simulation of in-pile behavior and has been routinely used for many research reactor fuel designs currently in use. In this test, the irradiated fuel plate is inserted into a furnace at a given temperature, soaked for a period of time, and removed for inspection. If no visible blisters appear, the furnace temperature is increased, and the plate is soaked and inspected again. This process continues until blisters are observed. Recently, a section from an irradiated U-7Mo dispersion fuel plate with Al-4043 matrix, which has a nominal composition of 4.81Si-0.20Fe-0.14Ti-0.16Cu-0.01Cr 0.01Mn-bal Al, was tested in a furnace located in the Hot Fuel Examination Facility, located at the Idaho National Laboratory, up to 500 deg. C, at which point blisters were observed on the surface of the fuel plate section. A sample near the blistered region of the fuel plate section was then characterized using scanning electron (SEM) and transmission electron microscopy (TEM). This paper discusses the results of this characterization and how they compare to those generated for a similar sample characterized after fabrication but before irradiation and for a sample characterized after irradiation but before furnace testing. One goal of this work is to identify the changes in the microstructure during blister testing that contribute to the eventual release of fission gas that results in the development of blisters. SEM analysis of the furnace-tested sample showed that in some locations of the U-7Mo particles, Al-4043 matrix constituents (primarily Si) had penetrated the microstructure along grain boundaries. This provided potential pathways for increased fission gas migration in the fuel meat microstructure during the furnace heating process. Some attack of these boundaries was also observed in the as-fabricated U-7Mo/Al-4043 sample, but there appeared to be additional attack during the furnace annealing. Besides the changes observed in grain boundary features, the TEM analysis showed that the fission gas bubbles that are typically present in the intra-granular regions of the as-irradiated U-7Mo microstructure as a fission gas bubble superlattice had changed in size, morphology, and distribution. The result of this may be an increase in the mobility of the fission gas in intra-granular regions of the fuel. The complete implications of the changes in fission gas morphology and distribution in the fuel meat microstructure and their impact on blistering continues to be investigated. (authors)

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Scanning Electron Microscopy Analysis of Fuel/Matrix Interaction Layers in Highly-Irradiated U–Mo Dispersion Fuel Plates with Al and Al–Si Alloy Matrices

In order to investigate how the microstructure of fuel/matrix-interaction (FMI) layers change during irradiation, different U–7Mo dispersion fuel plates have been irradiated to high fission density and then characterized using scanning electron microscopy (SEM). Specifially, samples from irradiated U–7Mo dispersion fuel elements with pure Al, Al–2Si and AA4043 (~4.5 wt.%Si) matrices were SEM characterized using polished samples and samples that were prepared with a focused ion beam (FIB). Features not observable for the polished samples could be captured in SEM images taken of the FIB samples. For the Al matrix sample, a relatively large FMI layer develops, with enrichment of Xe at the FMI layer/Al matrix interface and evidence of debonding. Overall, a significant penetration of Si from the FMI layer into the U–7Mo fuel was observed for samples with Si in the Al matrix, which resulted in a change of the size (larger) and shape (round) of the fission-gas bubbles. Additionally, solid-fission-product phases were observed to nucleate and grow within these bubbles. These changes in the localized regions of the microstructure of the U–7Mo may contribute to changes observed in the macroscopic swelling of fuel plates with Al–Si matrices.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗