Silicon PM Radiation Hardness
Detailed measurements have been made of 9 mm 2 SiPMs from Hamamatsu (MPPC) and Zecotek (MAPD) after room temperature annealing after exposure to fluences of 10 12 to 10 13 cm -2 . The data was used to complete the final ADR report.
46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗