In Situ Study on Fracture Behavior of Thick-Section Friction Stir-Welded AA 5083 Alloy

Friction stir welding (FSW) produces a gradient microstructure with distinct metallurgical zones. Here, the present study focuses on characterizing the fracture behavior during uniaxial loading across thick-section FSW joint in nonheat-treatable 5083 aluminum alloy. The hardness variation is linked to microstructural features across the weld zones through correlative microscopy. Notably, the heat-affected zone (HAZ) exhibits a lower hardness of 75 HV, while the thermomechanically affected zone (TMAZ) and stir zones (SZ) display a hardness of around 79HV. A marginal difference in hardness in HAZ prompts strain localization in HAZ on the advancing side of the weld, resulting in offset in fracture from the SZ, which is captured through in situ monitoring of the tensile test. Further, the postdeformation analysis reveals crack propagation along the maximum shear stress plane due to the coalescence of microvoids resulting from the fracturing and debonding of second-phase particles. Overall, this study provides valuable insight for optimizing the FSW process of AA 5083 alloy for thick-section applications.

36 MATERIALS SCIENCE↗

FY2022 Status Report: Cold Spray for Canister SCC Mitigation and Repair

This progress report describes work performed during FY22 at Sandia National Laboratories (SNL) to assess the corrosion performance of cold spray coatings to enable optimization of cold spray for the purposes of mitigation and/or repair of potentially susceptible regions, corrosion, or stress corrosion cracking (SCC) in austenitic stainless steel for spent nuclear fuel (SNF) storage. Of particular concern is SCC, by which a through-wall crack could potentially form in a canister outer wall over time intervals that may be shorter than possible dry storage times. In FY21, initial corrosion explorations of cold spray coating were evaluated and in FY22, an expanded set of cold spray coatings with in-depth analysis of post-exposure accelerated testing was explored. Additionally, relevant atmospheric exposure testing was carried out and initial results are presented herein. The corrosion attack from the accelerated testing and more realistic atmospheric exposures environments were compared to identify potentially deleterious factors for corrosion as well as help to understand the applicability of accelerated testing for cold spray optimization. This initial analysis will help to enable optimization of the corrosion resistance cold spray, one of the more promising coating and repair techniques, for potential application in an SNF environment. Learnings from both are summarized, and implications and future work are presented in this report.

36 MATERIALS SCIENCE↗

Microstructure, hardness and cavitation erosion resistance of different cold spray coatings on stainless steel 316 for hydropower applications

There is an urgent need for repair of hydropower components that have undergone damage due to cavitation. Conventional repair methods involve melting of materials and can deteriorate material properties and cause distortion. This study investigated the relevant properties of different materials using solid phase processing—cold spray technology. Stainless steel (SS) 316, Inconel 625 and CrC-NiCr materials were cold spray deposited onto base metal SS 316, respectively. Cold spray achieved dense uniform deposits with low level porosity, and intimate contact between the deposit and the base metal was observed. Severe plastic deformation imparted during the cold spray process resulted in significant grain size refinement, nanostructured regions were observed in the deposits across the interfacial area. Cold sprayed deposits exhibited elevated hardness in contrast to that of the base metal SS 316. The cavitation erosion resistance of the deposits was evaluated with a cavitation erosion jet adhering to ASTM G134. Both SS 316 and Inconel 625 achieved better cavitation erosion resistance when compared to that of the SS 316 base metal, with the former exhibiting close to a 4 times improvement.

Jiang, Xiujuan↗

Cold Spray Deposition of 304L Stainless Steel to Mitigate Chloride-Induced Stress Corrosion Cracking in Canisters for Used Nuclear Fuel Storage

A feasibility study of the cold spray deposition process of 304L stainless steel on 304L stainless steel substrates as a mitigation method for chloride-induced stress corrosion cracking (CISCC) has been investigated under various substrate conditions. The study is aimed at the application of this technology to mitigate CISCC that may potentially occur in or nearthe fusion welded regions of stainless steel canisters in Dry Cask Storage System (DCSS) for used nuclear fuels. Spherical gas-atomized 304L stainless steel powder, in the size range of 25 µm to 44 µm, was used as a feedstock powder for the cold spray process. The powder was deposited on four types of 304L substrates with various surface conditions: as-polished, oxidized, cold-rolled, plates with prototypical CISCC. The effects of cold spray parameters on quality of cold spray coatings were investigated. Thickness, porosity, and phases in the as-deposited materials were evaluated using scanning electron microscopy (SEM) and X-ray diffraction (XRD), and correlated with microhardness and adhesion strength measured via micro-indentation and ASTM C633 pulling test, respectively. XRD analysis of the coatings was also conducted to examine the effects of cold spray condition on residual stress state in the coating. Detailed cross-sectional examination of coating/substrate interfaces was performed with transmission electron microscopy (TEM) equipped with energy dispersive spectroscopy (EDS). Dense and continuous coatings with good adhesion strength and hardness were produced for the various substrate conditions by adjusting cold spray parameters. The results demonstrate that cold spray stainless steel coating is a viable option to provide a physical barrier against CISCC in fusion weld regions of stainless steel in corrosive chloride salt-bearing environments.

Dry Cask Storage Systems, cold spray, 304L stainle↗

Numerical Simulation and Experimental Validation of Joint Performance in Aluminum-Steel Lap Welds Formed by Friction Stir Dovetailing

Friction stir dovetailing (FSD) is a new dissimilar material joining process that simultaneously forms a mechanical interlock and metallurgical bond at the dissimilar material interface. This work presents development of a modeling and simulation approach to predict mechanical performance of FSD thick section aluminum to steel joints. A finite element analysis (FEA) was carried out in order to predict the load-carrying capacity and failure location for aluminum thicknesses between 12.7 mm and 50.8 mm with different numbers of dovetails. The numerical results and corresponding experimental investigation are in agreement and suggest that the developed methods can be used effectively for design and analysis of FSD joints using standard FEA tools.

Friction stir dovetailing, Friction stir welding, ↗

In Situ Cold-Spray Repair of Environmental Mission Infrastructure for Component Life Extension - 19424

Cold spray offers a potential option for performing in situ repair of U.S. Department of Energy (DOE) complex infrastructure critical to the Office of Environmental Management cleanup mission. Application to the DOE complex has the potential to reduce cost, schedule, and safety risk impacts associated with component failures and would negate the need to procure and construct replacement infrastructure. A concept and technical basis are presented for developing remotely deployable cold-spray systems for performing in situ repairs in hazardous environments such as nuclear waste tanks, piping, and process vessels to extend component service life or return critical infrastructure to service. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Friction stir welding bobbin tool

A bobbin tool is disclosed that includes a top shoulder, a bottom shoulder, and an axial pin that extends between the top and bottom shoulders. The bottom shoulder has an annular shoulder end surface, a back surface opposite the annular shoulder end surface, and a side surface that joins the annular shoulder end surface and the back surface. One or more and radially-extending blades may be disposed on the side surface of the bottom shoulder and/or one or more axially-extending blades may be disposed on the back surface. The one or more blades provide the bobbin tool with an ability to friction stir weld a variable thickness workpiece assembly, axially plunged through the workpiece assembly along an axis of rotation of the bobbin tool, and/or be extracted through the workpiece assembly along an axis of rotation of the bobbin tool.

47 OTHER INSTRUMENTATION↗

Friction stir processing of dual certified 304/304L austenitic stainless steel for improved cavitation erosion resistance

Cavitation phenomenon is known to be prevalent in equipment in hydraulic environments. Understanding cavitation and improving the cavitation resistance of commonly used materials is of interest for both scientific and economic reasons. In this study, friction stir processing was employed to modify commercial dual certified AISI 304/304L austenitic stainless steel plates. The cavitation erosion resistance of the processed plates was evaluated and compared to that of the unprocessed steel. A temperature control algorithm was employed to maintain a target tool temperature during the processing. The cross sections of the processed nuggets were evaluated using optical microscopy, scanning electron microscopy and Vickers hardness testing. Cavitation testing was performed conforming to ASTM G134 on specimens cut out of the nuggets of the commercially unprocessed and the processed 304/304L steel. The tool temperature was found to affect the microstructure and the cavitation performance. Friction stir processed steel showed 3 times better cavitation resistance than the unprocessed 304/304L. Surface cavitation patterns and cavitation rates were characterized and the mechanisms of material removal were discussed.

Jiang, Xiujuan↗

Joining thick section aluminum to steel with suppressed FeAl intermetallic formation via friction stir dovetailing

A new solid-phase technique called friction stir dovetailing (FSD) has been developed for joining thick section aluminum to steel. In FSD, mechanical interlocks are formed at the aluminum-steel interface and are reinforced by metallurgical bonds where intermetallic growth has been uniquely suppressed. Lap shear testing shows superior strength and extension at failure compared to popular friction stir approaches where metallurgical bonding is the only joining mechanism. High resolution microscopy revealed the presence of a 40-70 nm interlayer having a composition of 76.4 at% Al, 18.4 at% Fe, and 5.2 at% Si, suggestive of limited FeAl3 intermetallic formation.

Friction stir dovetailing, Joining, Intermetallics↗