Charge Transport and Space-Charge Formation in Cd 1 - x Zn x Te 1 - y Se y Radiation Detectors

The electron- and hole-transport properties in cadmium zinc telluride selenide (CZTS) crystals are studied using a laser-induced transient-current technique with pulsed and dc bias. The internal electric field profile and velocity of surface recombination are determined by Monte Carlo simulations of electron and hole transient currents combined with a numerical solution of the drift-diffusion equation coupled with Poisson’s equation. Electron and hole drift mobilities of μe = 830 cm 2 /Vs and μh = 40 cm 2 /Vs, respectively, are determined. We also develop a simple technique for evaluating surface recombination directly from measured current waveforms without the need for numerical simulation. The good quality of the prepared detector at pulsed bias, with electron- and hole-mobility-lifetime products of (μτ)e = 1.9 × 10 -3 cm 2 /V and (μτ)h = 1.4 × 10 -4 cm 2 /V, respectively, are observed. The formation of a positive space charge, originating from hole injection combined with a recombination level, is found. We observe a significant position dependence of the lifetime of electrons and holes in dc bias due to hole injection. The experiment is successfully fitted by a simple model dominated by a single deep recombination level with an energy of E t =E C -0.73eV; concentration of 7.3 × 10 11 cm -3 ; and electron- and hole-capture cross sections of 3.5 × 10 -14 cm 2 and 6.5 × 10 -14 cm 2 , respectively.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

New Scintillator Materials (K2CeBr5) and (Cs2CeBr5)

Cesium cerium bromide (Cs2CeBr5) and potassium cerium bromide (K2CeBr5) are new scintillator materials for X-ray and gamma ray detector applications. Recently halide scintillator materials, such as Ce doped lanthanum bromide has been proved to be very important material for the same purpose. These materials are highly hygroscopic; a search for high light yield non-hygroscopic materials was highly desirable to advance the scintillator technology. In this paper, we are reporting the crystal growth of novel scintillator materials, cesium cerium bromide (Cs2CeBr5) and potassium cerium bromide (K2CeBr5). Crystals were successfully grown from the melt using the vertical Bridgman-Stockbarger technique, in a comparison with the high performance LaBr3 or LaCl3 crystals, cerium based alkali halides crystals, (Cs2CeBr5) and (K2CeBr5) have similar scintillation properties, while being much less hygroscopic. Furthermore, cesium based compounds will not suffer from the self-activity present in potassium and lanthanum compounds. However the Cs2CeBr5 crystals did not grow properly probably due to non-congruent melting or to some phase transition during cooling. Keywords." Scintillator materials; Ce3+; Energy resolution; Light yield; K2CeBr5

Hawrami, R.↗

Photoluminescence of CdTe Crystals Grown by Physical-Vapor Transport

High-quality CdTe crystals with resistivities higher than 10(exp 8) omega cm were grown by the physical-vapor transport (PVT) technique. Indium, aluminum, and the transition-metal scandium were introduced at the nominal level of about 6 ppm to the source material. Low-temperature photoluminescence (PL) has been employed to identify the origins of PL emissions of the crystals. The emission peaks at 1.584 eV and 1.581 eV were found only in the In-doped crystal. The result suggests that the luminescence line at 1.584 eV is associated with Cd-vacancy/In complex. The intensity of the broadband centered at 1.43 eV decreases strongly with introduction of Sc.

Palosz, W.↗

Photoluminescence of CdTe Crystals Grown by Contactless PVT Method

High quality CdTe crystals with resistivities higher than 10(exp 8) Omega cm were grown by the 'contactless' PVT (physical vapor transport) technique. Group III elements In and Al, and the transition metal Sc were introduced at the nominal level of about 6 ppm to the source material. Low-temperature photoluminescence (PL) has been employed to identify the origins of PL emissions of the crystals. It was found that the emission peaks at 1.584 eV and 1.581 eV exist only in the In-doped crystal. The result suggests that the luminescence line at 1.584 eV is associated with Cd-vacancy/indium complex. The intensity of the broadband centered at 1.43 eV decreases dramatically with introduction of Sc.

Palosz, W.↗

Photoluminescence of CdTe Crystals Grown by Physical Vapor Transport

High quality CdTe crystals with resistivities higher than 10(exp 8) omega cm were grown by the physical vapor transport technique. Indium, Aluminum, and the transition metal Scandium were introduced at the nominal level of about 6 ppm to the source material. Low-temperature photoluminescence (PL) has been employed to identify the origins of PL emissions of the crystals. The emission peaks at 1.584 eV and 1.581 eV were found only in the In-doped crystal. The result suggests that the luminescence line at 1.584 eV is associated with Cd-vacancy/indium complex. The intensity of the broadband centered at 1.43 eV decreases strongly with introduction of Sc.

Curreri, Peter A.↗

Photoluminescence of CdTe Crystals Grown by Physical Vapor Transport

High quality CdTe crystals with resistivities higher than 10(exp 8) omega cm were grown by the physical vapor transport technique. Indium, Aluminum, and the transition metal Scandium were introduced at the nominal level of about 6 ppm to the source material. Low-temperature photoluminescence (PL) has been employed to identify the origins of PL emissions of the crystals. The emission peaks at 1.584 eV and 1.581 eV were found only in the In-doped crystal. The result suggests that the luminescence line at 1.584 eV is associated with Cd-vacancy/indium complex. The intensity of the broadband centered at 1.43 eV decreases strongly with introduction of Sc.

Palosz, W.↗