Search NASA⌕ Search

Engineering topics

Rudisill, T

Publications and source records attributed to Rudisill, T.

DECONTAMINATION OF ZIRCALOY CLADDING HULLS FROM SPENT NUCLEAR FUEL

The feasibility of decontaminating spent fuel cladding hulls using hydrofluoric acid (HF) was investigated as part of the Global Energy Nuclear Partnership (GNEP) Separations Campaign. The concentrations of the fission product and transuranic (TRU) isotopes in the decontaminated hulls were compared to the limits for determining the low level waste (LLW) classification in the United States (US). The {sup 90}Sr and {sup 137}Cs concentrations met the disposal criteria for a Class C LLW; although, in a number of experiments the criteria for disposal as a Class B LLW were met. The TRU concentration in the hulls generally exceeded the Class C LLW limit by at least an order of magnitude. The concentration decreased sharply as the initial 30-40 {micro}m of the cladding hull surface were removed. At depths beyond this point, the TRU activity remained relatively constant, well above the Class C limit. Reprocessing of spent nuclear fuel generates a cladding waste which would likely require disposal as a Greater than Class C LLW in the US. If the cladding hulls could be treated to remove a majority of the actinide and fission product contamination, the hulls could potentially meet acceptance criteria for disposal as a LLW or allow recycle of the Zr metal. Discard of the hulls as a LLW would result in significant cost savings compared to disposal as a Greater than Class C waste which currently has no disposition path. During fuel irradiation and reprocessing, radioactive materials are produced and deposited in the Zircaloy cladding. Due to short depths of penetration, the majority of the fission products and actinide elements are located in the ZrO{sub 2} layer which forms on the surface of the cladding during fuel irradiation. Therefore, if the oxide layer is removed, the majority of the contamination should also be removed. It is very difficult, if not impossible to remove all of the activity from spent fuel cladding since traces of U and Th in the unirradiated Zircaloy adsorb neutrons generating higher actinides in the bulk material. During fuel irradiation, {sup 92}Zr is also converted to radioactive {sup 93}Zr by neutron adsorption. Methods for decontaminating and conditioning irradiated Zircaloy cladding hulls have been investigated in Europe, Japan, and the US during the last 35 years; however, a method to decontaminate the hulls to an activity level which meets US acceptance criteria for disposal as a LLW was not deployed on a commercial scale. The feasibility of decontaminating spent fuel cladding hulls was investigated as part of the GNEP Separations Campaign. Small-scale experiments were used to demonstrate the removal of the ZrO{sub 2} layer from Zircaloy coupons using dilute solutions ({le}1.0 M) of HF. The most effective conditions resulted in dissolution rates which were less than approximately 2 mg/cm{sup 2}-min. With dissolution rates in this range, uniform removal of the oxide layer was obtained and a minimal amount of Zircaloy metal was dissolved. To test the HF decontamination process, experiments were subsequently performed using actual spent fuel cladding hulls. Decontamination experiments were performed to measure the fission product and actinide concentrations as a function of the depth of the surface removed from the cladding hull. The experimental methods used to perform these experiments and a discussion of the results and observations are presented in the following sections.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

PLUTONIUM SOLUBILITY IN SIMULATED SAVANNAH RIVER SITE WASTE SOLUTIONS

To address the accelerated disposition of the supernate and salt portions of Savannah River Site (SRS) high level waste (HLW), solubility experiments were performed to develop a predictive capability for plutonium (Pu) solubility. A statistically designed experiment was used to measure the solubility of Pu in simulated solutions with salt concentrations and temperatures which bounded those observed in SRS HLW solutions. Constituents of the simulated waste solutions included: hydroxide (OH{sup -}), aluminate (Al(OH){sub 4}{sup -}), sulfate (SO{sub 4}{sup 2-}), carbonate (CO{sub 3}{sup 2-}), nitrate (NO{sub 3}{sup -}), and nitrite (NO{sub 2}{sup -}) anions. Each anion was added to the waste solution in the sodium form. The solubilities were measured at 25 and 80 C. Five sets of samples were analyzed over a six month period and a partial sample set was analyzed after nominally fifteen months of equilibration. No discernable time dependence of the measured Pu concentrations was observed except for two salt solutions equilibrated at 80 C which contained OH{sup -} concentrations >5 mol/L. In these solutions, the Pu solubility increased with time. This observation was attributed to the air oxidation of a portion of the Pu from Pu(IV) to the more soluble Pu(V) or Pu(VI) valence states. A data driven approach was subsequently used to develop a modified response surface model for Pu solubility. Solubility data from this study and historical data from the literature were used to fit the model. The model predicted the Pu solubility of the solutions from this study within the 95% confidence interval for individual predictions and the analysis of variance indicated no statistically significant lack of fit. The Savannah River National Laboratory (SRNL) model was compared with predicted values from the Aqueous Electrolyte (AQ) model developed by OLI Systems, Inc. and a solubility prediction equation developed by Delegard and Gallagher for Hanford tank waste. The agreement between measured or values predicted by the SRNL model and values predicted by the OLI AG model was very poor. The much higher predicted concentrations by the OLI AQ model appears to be the result of the model predicting the predominate Pu oxidation state is Pu(V) which is reported as unstable below sodium hydroxide (NaOH) concentrations of 6 M. There was very good agreement between the predicted Pu concentrations using the SRNL model and the model developed by Delegard and Gallagher with the exception of solutions that had very high OH{sup -} (15 M) concentrations. The lower Pu solubilities in these solutions were attributed to the presence of NO{sub 3}{sup -} and NO{sub 2}{sup -} which limit the oxidation of Pu(IV) to Pu(V).

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

DISTRIBUTION OF ACTINIDES BETWEEN THE AQUEOUS AND ORGANIC PHASES IN THE TALSPEAK PROCESS

One objective of the US Department of Energy's Office of Nuclear Energy (DOE-NE) is the development of sustainable nuclear fuel cycles which improve uranium resource utilization, maximize energy generation, minimize waste generation, improve safety, and complement institutional measures limiting proliferation risks. Activities in progress which support this objective include the development of advanced separation technologies to recover the actinides from used nuclear fuels. With the increased interest in the development of technology to allow closure of the nuclear fuel cycle, the TALSPEAK process is being considered for the separation of Am and Cm from the lanthanide fission products in a next generation reprocessing plant. However, at this time, the level of understanding associated with the chemistry and the control of the process variables is not acceptable for deployment of the process on an industrial scale. To address this issue, DOE-NE is supporting basic scientific studies focused on the TALSPEAK process through its Fuel Cycle Research and Development (R&D) program. One aspect of these studies is an experimental program at the Savannah River National Laboratory (SRNL) in which temperature-dependent distribution coefficients for the extraction of actinide elements in the TALSPEAK process were measured. The data were subsequently used to calculate conditional enthalpies and entropies of extraction by van't Hoff analysis to better understand the thermodynamic driving forces for the TALSPEAK process. In the SRNL studies, the distribution of Pu(III) in the TALSPEAK process was of particular interest. A small amount of Pu(III) would be present in the feed due to process losses and valence adjustment in prior recovery operations. Actinide elements such as Np and Pu have multiple stable oxidation states in aqueous solutions; therefore the oxidation state for these elements must be controlled in the TALSPEAK process, as the extraction chemistry is dependent upon the actinide's valence. Since our plans included the measurement of Pu(III) distribution coefficients using a Np(V) solution containing small amounts of {sup 238}Pu, it was necessary to demonstrate that the desired oxidation states of Np and Pu are produced and could be stabilized in a buffered lactate solution containing diethylenetriaminepentaacetic (DTPA). The stability of Np(V) and Pu(III) in lactic acid/DTPA solutions was evaluated by ultraviolet-visible (UV-vis) spectroscopy. To perform the evaluation, Np and Pu were added to solutions containing either hydroxylamine nitrate (HAN) or ferrous sulfamate (FS) as the reductant and nominally 1.5 M lactic acid/0.05 M DTPA. The pH of the solution was subsequently adjusted to nominally 2.8 as would be performed in the TALSPEAK process. In the valence adjustment study, we found that it was necessary to reduce Pu to Pu(III) prior to combining with the lactic acid and DTPA. The Pu reduction was performed using either HAN or FS. When FS was used, Np was reduced to Np(IV). The spectroscopic studies showed that Np(V) and Pu(III) are not stable in lactic acid/DTPA solutions. The stability of Np(IV)- and Pu(IV)-DTPA complexes are much greater than the stability of the Np(V)- and Pu(III)-DTPA complexes, and as a result, Np is slowly reduced to Np(IV) and Pu is slowly oxidized to Pu(IV) due to the reduced activity of the more stable complexes. When Np(V) was added to a solution containing a 1.5 M lactic acid/ammonium lactate buffer and 0.05 M DTPA, approximately 50% of the Np was reduced to Np(IV) in the first day. The fraction of Np(V) in the solution continued to diminish with time and was essentially reduced to Np(IV) after one week. When Pu(III) was added to a lactic acid/DTPA solution of the same composition, the spectrum recorded following at least two days after preparation of the solution continued to show some sign of Pu(III). The Pu(III) was completely oxidized to Pu(IV) after 3-4 days. The UV-vis spectroscopy demonstrated that Np(V) and Pu(III) were the predominate valences in the lactic acid/DTPA solution for the better part of a day following solution preparation. Based on these results, we chose to initially add HAN to the actinide tracer solution prepared for the distribution coefficient measurements (to produce Pu(III)) prior to combining with lactic acid and DTPA. The distribution coefficient measurements were expected to be complete in 2-3 h; therefore, Np(V) and Pu(III) valences would predominate in the solution during this time. Prior to adding the HAN to the actinide tracers, we added sufficient Am(III) activity to allow the measurement of distribution coefficients during the extraction experiments. Protactinium (V) distribution coefficients were also measured using the activity which was in secular equilibrium with the {sup 237}Np. The actinide distribution coefficients were measured at pH 2.8 and 3.5 and covered a range of temperatures from nominally 20 to 60 C.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

REMOVAL OF SOLIDS FROM HIGHLY ENRICHED URANIUM SOLUTIONS USING THE H-CANYON CENTRIFUGE

Prior to the dissolution of Pu-containing materials in HB-Line, highly enriched uranium (HEU) solutions stored in Tanks 11.1 and 12.2 of H-Canyon must be transferred to provide storage space. The proposed plan is to centrifuge the solutions to remove solids which may present downstream criticality concerns or cause operational problems with the 1st Cycle solvent extraction due to the formation of stable emulsions. An evaluation of the efficiency of the H-Canyon centrifuge concluded that a sufficient amount (> 90%) of the solids in the Tank 11.1 and 12.2 solutions will be removed to prevent any problems. We based this conclusion on the particle size distribution of the solids isolated from samples of the solutions and the calculation of particle settling times in the centrifuge. The particle size distributions were calculated from images generated by scanning electron microscopy (SEM). The mean particle diameters for the distributions were 1-3 {micro}m. A significant fraction (30-50%) of the particles had diameters which were < 1 {micro}m; however, the mass of these solids is insignificant (< 1% of the total solids mass) when compared to particles with larger diameters. It is also probable that the number of submicron particles was overestimated by the software used to generate the particle distribution due to the morphology of the filter paper used to isolate the solids. The settling times calculated for the H-Canyon centrifuge showed that particles with diameters less than 1 to 0.5 {micro}m will not have sufficient time to settle. For this reason, we recommend the use of a gelatin strike to coagulate the submicron particles and facilitate their removal from the solution; although we have no experimental basis to estimate the level of improvement. Incomplete removal of particles with diameters < 1 {micro}m should not cause problems during purification of the HEU in the 1st Cycle solvent extraction. Particles with diameters > 1 {micro}m account for > 99% of the solid mass and will be efficiently removed by the centrifuge; therefore, the formation of emulsions during solvent extraction operations is not an issue. Under the current processing plan, the solutions from Tanks 11.1 and 12.2 will be transferred to the enriched uranium storage (EUS) tank following centrifugation. The solution from Tanks 11.1 and 12.2 may remain in the EUS tank for an extended time prior to purification. The effects of extended storage on the solution were not evaluated as part of this study.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

EVALUATION OF FLOWSHEET CHANGES FOR THE HIGHLY ENRICHED URANIUM BLENDDOWN PROGRAM

H Canyon is considering a flowsheet change for Plutonium (Pu) Contaminated Scrap (PuCS) material. The proposed change is to route dissolved PuCS material directly to a uranium (U) storage tank. As a result, the PuCS solution will bypass Head End and First U Cycle, and will be purified by solvent extraction in Second U Cycle. The PuCS solution contains appreciable amounts of boron (B) and fluoride (F{sup -}), which are currently at trace levels in the U storage tank. Though unlikely, if the B concentration in the U storage tank were to reach 1.8 g B/g U, the entire contents of the U storage tank would likely require a second pass through Second U Cycle to provide sufficient decontamination to meet the Tennessee Valley Authority (TVA) Blend Grade Highly Enriched Uranium (HEU) specification for B, which is 30 {micro}g/g U. In addition, Second U Cycle is expected to provide sufficient decontamination of F{sup -} and Pu regardless of the amount of PuCS solution sent to the storage tank. Though aluminum (Al) is not present in the PuCS solution, B can be credited as a complexant of F{sup -}. Both stability constants from the literature and Savannah River National Laboratory (SRNL) corrosion studies were documented to demonstrate that B complexation of F{sup -} in nitric acid solutions is sufficient to prevent excessive corrosion. Though B and Al complex F{sup -} to a similar degree, neither completely eliminates the presence of free F{sup -} in solution. Therefore, a limited amount of corrosion is expected even with complexed F{sup -} solutions. Tanks maintained at ambient temperature are not expected to experience significant corrosion. However, the Low Activity Waste (LAW) evaporators may be subjected to a corrosion rate of about 25 mils per year (mpy) as they reach their highest F{sup -} concentrations. The feed adjustment evaporator would only be subjected to the corrosion rate of about 25 mpy in the latter stages of the PuCS campaign. An issue that must be addressed as part of the proposed PuCS flowsheet change is that B has limited solubility in concentrated nitric acid solutions. As the proposed PuCS campaign progresses, the B concentration will increase in the U storage tank, in Second U Cycle feed, and in the 1DW stream sent to the LAW evaporators. Limitations on the B concentration in the LAW evaporators will be needed to prevent formation of boron-containing solids.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

DISSOLUTION OF PLUTONIUM METAL USING NITRIC ACID SOLUTIONS CONTAINING POTASSIUM FLUORIDE

The deinventory and deactivation of the Savannah River Site's (SRS's) FB-Line facility required the disposition of approximately 2000 items from the facility's vaults. Plutonium (Pu) scraps and residues which do not meet criteria for conversion to a mixed oxide fuel will be dissolved and the solution stored for subsequent disposition. Some of the items scheduled for dissolution are composite materials containing Pu and tantalum (Ta) metals. The preferred approach for handling this material is to dissolve the Pu metal, rinse the Ta metal with water to remove residual acid, and burn the Ta metal. The use of a 4 M nitric acid (HNO{sub 3}) solution containing 0.2 M potassium fluoride (KF) was initially recommended for the dissolution of approximately 500 g of Pu metal. However, prior to the use of the flowsheet in the SRS facility, a new processing plan was proposed in which the feed to the dissolver could contain up to 1250 g of Pu metal. To evaluate the use of a larger batch size and subsequent issues associated with the precipitation of plutonium-containing solids from the dissolving solution, scaled experiments were performed using Pu metal and samples of the composite material. In the initial experiment, incomplete dissolution of a Pu metal sample demonstrated that a 1250 g batch size was not feasible in the HB-Line dissolver. Approximately 45% of the Pu was solubilized in 4 h. The remaining Pu metal was converted to plutonium oxide (PuO{sub 2}). Based on this work, the dissolution of 500 g of Pu metal using a 4-6 h cycle time was recommended for the HB-Line facility. Three dissolution experiments were subsequently performed using samples of the Pu/Ta composite material to demonstrate conditions which reduced the risk of precipitating a double fluoride salt containing Pu and K from the dissolving solution. In these experiments, the KF concentration was reduced from 0.2 M to either 0.15 or 0.175 M. With the use of 4 M HNO{sub 3} and a reduction in the KF concentration to 0.175 M, the dissolution of 300 g of Pu metal is expected to be essentially complete in 6 h. The dissolution of larger batch sizes would result in the formation of PuO{sub 2} solids. Incomplete dissolution of the PuO{sub 2} formed from the metal is not a solubility limitation, but can be attributed to a combination of reduced acidity and complexation of fluoride which slows the dissolution kinetics and effectively limits the mass of Pu dissolved.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗