Search NASA⌕ Search

Engineering topics

Samukawa, Seiji

Publications and source records attributed to Samukawa, Seiji.

Al and Ge simultaneous oxidation using neutral beam post-oxidation for formation of gate stack structures

To obtain a high-quality Germanium (Ge) metal–oxide–semiconductor structure, a Ge gate stacked structure was fabricated using neutral beam post-oxidation. After deposition of a 1-nm-thick Al metal film on a Ge substrate, simultaneous oxidation of Al and Ge was carried out at 300 °C, and a Ge oxide film with 29% GeO{sub 2} content was obtained by controlling the acceleration bias power of the neutral oxygen beam. In addition, the fabricated AlO{sub x}/GeO{sub x}/Ge structure achieved a low interface state density of less than 1 × 10{sup 11 }cm{sup −2 }eV{sup −1} near the midgap.

36 MATERIALS SCIENCE↗

Resistive switching in a few nanometers thick tantalum oxide film formed by a metal oxidation

Resistive switching in a Cu/Ta{sub 2}O{sub 5}/Pt structure that consisted of a few nanometer-thick Ta{sub 2}O{sub 5} film was demonstrated. The Ta{sub 2}O{sub 5} film with thicknesses of 2–5 nm was formed with a combination of Ta metal film deposition and neutral oxygen particle irradiation at room temperature. The device exhibited a bipolar resistive switching with a threshold voltage of 0.2 V and multilevel switching operation.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Impact of artificial lateral quantum confinement on exciton-spin relaxation in a two-dimensional GaAs electronic system

We demonstrate the effect of artificial lateral quantum confinement on exciton-spin relaxation in a GaAs electronic system. GaAs nanodisks (NDs) were fabricated from a quantum well (QW) by top-down nanotechnology using neutral-beam etching aided by protein-engineered bio-nano-templates. The exciton-spin relaxation time was 1.4 ns due to ND formation, significantly extended compared to 0.44 ns for the original QW, which is attributed to weakening of the hole-state mixing in addition to freezing of the carrier momentum. The temperature dependence of the spin-relaxation time depends on the ND thickness, reflecting the degree of quantum confinement.

36 MATERIALS SCIENCE↗

Photoluminescence from GaAs nanodisks fabricated by using combination of neutral beam etching and atomic hydrogen-assisted molecular beam epitaxy regrowth

We have fabricated GaAs nanodisk (ND) structures by using a combination of neutral beam etching process and atomic hydrogen-assisted molecular beam epitaxy regrowth. We have observed clear photoluminescence (PL) emissions from GaAs NDs. The peak energy showed a blueshift due to the quantum confinement in three spatial dimensions, and it agreed with the theoretically estimated transition energy. The PL results also showed that the cap-layer disks act as radiative recombination centers. We have confirmed that the PL emission originates from the GaAs NDs, and our approach is effective for the fabrication of high quality ND structures.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

200-mm-diameter neutral beam source based on inductively coupled plasma etcher and silicon etching

The authors developed a neutral beam source consisting of a 200-mm-diameter inductively coupled plasma etcher and a graphite neutralization aperture plate based on the design of a neutral beam source that Samukawa et al. [Jpn. J. Appl. Phys., Part 2 40, L779 (2001)] developed. They measured flux and energy of neutral particles, ions, and photons using a silicon wafer with a thermocouple and a Faraday cup and calculated the neutralization efficiency. An Ar neutral beam flux of more than 1 mA/cm{sup 2} in equivalent current density and a neutralization efficiency of more than 99% were obtained. The spatial uniformity of the neutral beam flux was within {+-}6% within a 100 mm diameter. Silicon etching using a F{sub 2}-based neutral beam was done at an etch rate of about 47 nm/min, while Cl{sub 2}-based neutral beam realized completely no undercut. The uniformity of etch rate was less than {+-}5% within the area. The etch rate increased by applying bias power to the neutralization aperture plate, which shows that accelerated neutral beam was successfully obtained. These results indicate that the neutral beam source is scalable, making it possible to obtain a large-diameter and uniform neutral beam, which is inevitable for application to mass production.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Prediction of UV spectra and UV-radiation damage in actual plasma etching processes using on-wafer monitoring technique

UV radiation during plasma processing affects the surface of materials. Nevertheless, the interaction of UV photons with surface is not clearly understood because of the difficulty in monitoring photons during plasma processing. For this purpose, we have previously proposed an on-wafer monitoring technique for UV photons. For this study, using the combination of this on-wafer monitoring technique and a neural network, we established a relationship between the data obtained from the on-wafer monitoring technique and UV spectra. Also, we obtained absolute intensities of UV radiation by calibrating arbitrary units of UV intensity with a 126 nm excimer lamp. As a result, UV spectra and their absolute intensities could be predicted with the on-wafer monitoring. Furthermore, we developed a prediction system with the on-wafer monitoring technique to simulate UV-radiation damage in dielectric films during plasma etching. UV-induced damage in SiOC films was predicted in this study. Our prediction results of damage in SiOC films shows that UV spectra and their absolute intensities are the key cause of damage in SiOC films. In addition, UV-radiation damage in SiOC films strongly depends on the geometry of the etching structure. The on-wafer monitoring technique should be useful in understanding the interaction of UV radiation with surface and in optimizing plasma processing by controlling UV radiation.

36 MATERIALS SCIENCE↗

Controllable modification of self-assembled monolayer surface by using N{sub 2} neutral beam process

A novel technique of low-energy N{sub 2} neutral beam (NB) (<10 eV) irradiation was investigated as a means of controlling the surface nitridation of self-assembled monolayers (SAMs). This low-energy process without UV photons was able to nitride the surfaces of terphenyl SAMs. Furthermore, by varying the on/off period for irradiation, a pulse-time modulated NB process could be used to control the atomic ratio of nitrogen in terphenyl molecules. Time-of-flight secondary ion mass spectra revealed that one H in the terphenyl group was substituted by a NH{sub 2} group because of irradiation by the N{sub 2} beam. The data suggested that the low-energy NB technique caused less damage to modified surfaces than the conventional plasma process did. Therefore, we believe that it is a potential damage-free process for modifying the surfaces of soft organic materials and films.

36 MATERIALS SCIENCE↗

Mechanism for low-etching resistance and surface roughness of ArF photoresist during plasma irradiation

ArF excimer laser lithography was introduced to fabricate nanometer-scale devices and uses chemically amplified photoresist polymers including photoacid generators (PAGs). Because plasma-etching processes cause serious problems related to the use of ArF photoresists, such as line-edge roughness and low etching selectivity, we have to understand the interaction between plasma and ArF photoresist polymers. Investigating the effects of surface temperature and the irradiation species from plasma, we have found that ion irradiation by itself did not drastically increase the roughness or etching rate of ArF photoresist films unless it was combined with ultraviolet/vacuum ultraviolet (UV/VUV) photon irradiation. The structures of ArF photoresist polymers were largely unchanged by ion irradiation alone but were destroyed by combinations of ion and UV/VUV-photon irradiation. Our results suggested that PAG-mediated deprotection induced by UV/VUV-photon irradiation was amplified at surface temperatures above 100 deg. C. The etching rate and surface roughness of plasma-etched ArF photoresists are affected by the irradiation species and surface temperature during plasma etching. UV/VUV-photon irradiation plays a particularly important role in the interaction between plasma and ArF photoresist polymers.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

UV photon-induced defect and its control in plasma etching processes

We found that the use of pulse-time-modulated (TM) plasma reduces ultraviolet (UV) photon-induced defects in SiO{sub 2} films formed during plasma etching. The pulse timing of the radio-frequency power in the TM plasma was modulated at a few tens of microseconds. During the pulse-off period, UV photon radiation significantly decreased because of reduced electron energy in the plasma. As a result, the density of UV photon-induced defects, such as E{sup '} centers, in SiO{sub 2} films was reduced when the TM plasma was used compared with that when a continuous wave (CW) plasma was used. In addition, we found that the energy level of excitation states of the E{sup '} centers generated in the TM plasma was less than that generated when the CW plasma was used. Low-temperature annealing was needed to reduce the number of E{sup '} centers when the TM plasma was used; whereas higher-temperature annealing was needed when the CW plasma was used. These results showed that the energy level of excitation states of UV photon-induced defects in SiO{sub 2} films was reduced by using the TM plasma.

36 MATERIALS SCIENCE↗

Generation and reduction in SiO{sub 2}/Si interface state density during plasma etching processes

During plasma processes, the SiO{sub 2}/Si interface state is generated by UV photon irradiation. We measured P{sub b} centers (Si dangling bond at SiO{sub 2}/Si interface) in SiO{sub 2}/Si film by electron spin resonance spectroscopy. The density of P{sub b} centers increased with increasing UV photon energy. This result indicates that high-energy photons effectively generate P{sub b} centers because of the absorption at the SiO{sub 2}/Si interface. At the same time, we found that UV photon flux is also an important factor in increasing the density of P{sub b} centers. On the other hand, ion irradiations were not a significant factor in the generation of P{sub b} centers. Ions can penetrate only the surface (less than 5 nm) but they cannot induce a P{sub b} center at the SiO{sub 2}/Si interface. Furthermore, pulse-time-modulated plasmas were used to reduce the UV photon irradiation during the plasma processes. The reduction in UV photon irradiation could completely eliminate the P{sub b} centers compared with the use of a conventional continuous wave plasma.

36 MATERIALS SCIENCE↗

Low-damage low-k etching with an environmentally friendly CF{sub 3}I plasma

The feasibility of etching Cu/low-k interconnects by using a low global warming potential CF{sub 3}I plasma was studied. Low-damage etching was done and porous SiOC (p-SiOC, k<2.6) film with low roughness was produced. Exposing p-SiOC film to CF{sub 3}I plasma was found to suppress the decrease in the CH{sub 3} group and the increase in the k value compared to those of conventional CF{sub 4} and C{sub 4}F{sub 6} plasmas. These effects are due to the low UV intensity and small amount of F radicals of CF{sub 3}I plasma. The authors also found that the etching profile of CF{sub 3}I plasma was comparable with that of CF{sub 4} plasma. Since the etching selectivity (p-SiOC/ArF photoresist) of CF{sub 3}I plasma is higher than that of CF{sub 4} plasma, the remaining photoresist thickness increases after etching, thus suppressing line edge roughness (LER). The decreased LER mitigated degradation of IV and time dependent dielectric breakdown characteristics in Cu interconnects. They also found that the roughness on the bottom surface of the p-SiOC trench was reduced. These benefits are due to CF{sub 3}I plasma's low reactivity with the carbon in photoresists and p-SiOC films. Based on these findings, they believe that the environmentally friendly CF{sub 3}I gas has great promise as a p-SiOC etching material.

36 MATERIALS SCIENCE↗

Environmentally harmonized CF{sub 3}I plasma for low-damage and highly selective low-k etching

Low-damage, high-rate, and highly selective low-k etching can be simultaneously satisfied using a plasma with an environmentally harmonized gas chemistry (CF{sub 3}I). Such a CF{sub 3}I plasma can drastically reduce the irradiation damage by ultraviolet (UV) photons during low-k etching, because the intensity of UV in CF{sub 3}I plasma is much lower than that in conventional CF{sub 4} plasma. The etching selectivity of SiOCH to a photoresist can be drastically improved by using CF{sub 3}I plasma because of reducing F radical generation. In addition, pulse-time-modulated CF{sub 3}I plasma causes a drastic increase in the etching rate because a large amount of negative ions can be generated. These results show that CF{sub 3}I plasma is a very promising candidate for low-damage and highly selective low-k etching.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Real-time monitoring of successive sparks in high-density plasma chambers

Successive sparks in high-density plasma were analyzed using various real-time monitoring systems, such as electromagnetic field sensors and on-wafer sensors. Electron density decreases at the moment the sparking occurs because a large number of electrons flow to the chamber wall and the wafer surface. Due to the potential fluctuation of the plasma, other sparks occur successively during recovery to the stable plasma. The successive sparks sometimes continue for a few milliseconds. Based on these findings, the authors found that electromagnetic field sensors and on-wafer sensors are very effective tools for real-time monitoring of successive sparks.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

Plasma irradiation damages to magnetic tunneling junction devices

We exposed magnetic tunneling junction (MTJ) devices--fabricated using Ar-ion milling--to the reactive plasma commonly used in etching to determine the mechanism of the damage caused by the exposure. Exposing MTJ devices to the conventional continuous-wave (CW) plasma widely used in plasma etching significantly degrades their magnetic characteristics. However, exposure to a pulse-time-modulated (TM) plasma does not degrade the MTJ devices' magnetic characteristics. Analysis of transmission electron microscopy cross sections of the MTJ device structures revealed that the structure of the CoFe pinned layer was damaged in the MTJ devices exposed to a conventional CW plasma. This structural damage degraded the MTJ devices' magnetic characteristics. No damage to the structure of the MTJ devices was seen in those exposed to a TM plasma. Therefore, using the TM plasma offers an effective, damage-free method of etching MTJ devices as part of their manufacturing process.

36 MATERIALS SCIENCE↗