Search NASA⌕ Search

Engineering topics

Schelhas, Laura T.

Publications and source records attributed to Schelhas, Laura T..

At least 37 records · Page 2

Thermochromic Halide Perovskite Windows with Ideal Transition Temperatures

Abstract Urban centers across the globe are responsible for a significant fraction of energy consumption and CO 2 emission. As urban centers continue to grow, the popularity of glass as cladding material in urban buildings is an alarming trend. Dynamic windows reduce heating and cooling loads in buildings by passive heating in cold seasons and mitigating solar heat gain in hot seasons. Here, reduced energy consumption in highly glazed buildings in a mesoscopic building energy model is demonstrated when thermochromic windows are employed. Savings are realized across eight disparate climate zones of the United States. The model is used to determine ideal critical transition temperatures of 20–27.5 °C for thermochromic windows based on metal halide perovskite materials. Ideal transition temperatures are realized experimentally in composite metal halide perovskite films composed of perovskite crystals and an adjacent reservoir phase. The transition temperature is controlled by cointercalating methanol, instead of water, with methylammonium iodide and tailoring the hydrogen‐bonding chemistry of the reservoir phase. Thermochromic windows based on metal halide perovskites represent a clear opportunity to mitigate the effects of energy‐hungry buildings.

14 SOLAR ENERGY↗

Compositional texture engineering for highly stable wide-bandgap perovskite solar cells

The development of highly stable and efficient wide-bandgap (WBG) perovskite solar cells (PSCs) based on bromine-iodine (Br–I) mixed-halide perovskite (with Br greater than 20%) is critical to create tandem solar cells. However, issues with Br–I phase segregation under solar cell operational conditions (such as light and heat) limit the device voltage and operational stability. This challenge is often exacerbated by the ready defect formation associated with the rapid crystallization of Br-rich perovskite chemistry with antisolvent processes. We combined the rapid Br crystallization with a gentle gas-quench method to prepare highly textured columnar 1.75–electron volt Br–I mixed WBG perovskite films with reduced defect density. Here, with this approach, we obtained 1.75–electron volt WBG PSCs with greater than 20% power conversion efficiency, approximately 1.33-volt open-circuit voltage (V oc ), and excellent operational stability (less than 5% degradation over 1100 hours of operation under 1.2 sun at 65°C). When further integrated with 1.25–electron volt narrow-bandgap PSC, we obtained a 27.1% efficient, all-perovskite, two-terminal tandem device with a high V oc of 2.2 volts.

14 SOLAR ENERGY↗

Intermediate-phase engineering via dimethylammonium cation additive for stable perovskite solar cells

Achieving the long-term stability of perovskite solar cells is arguably the most important challenge required to enable widespread commercialization. Understanding the perovskite crystallization process and its direct impact on device stability is critical to achieving this goal. The commonly employed dimethyl-formamide/dimethyl-sulfoxide solvent preparation method results in a poor crystal quality and microstructure of the polycrystalline perovskite films. In this work, we introduce a high-temperature dimethyl-sulfoxide-free processing method that utilizes dimethylammonium chloride as an additive to control the perovskite intermediate precursor phases. By controlling the crystallization sequence, we tune the grain size, texturing, orientation (corner-up versus face-up) and crystallinity of the formamidinium (FA)/caesium (FA) y Cs 1-y Pb(I x Br 1-x )3 perovskite system. A population of encapsulated devices showed improved operational stability, with a median T80 lifetime (the time over which the device power conversion efficiency decreases to 80% of its initial value) for the steady-state power conversion efficiency of 1,190 hours, and a champion device showed a T80 of 1,410 hours, under simulated sunlight at 65 degrees C in air, under open-circuit conditions. In conclusion, this work highlights the importance of material quality in achieving the long-term operational stability of perovskite optoelectronic devices.

14 SOLAR ENERGY↗

Arrhenius Analysis of the Degradation Modes in Emerging Photovoltaic Backsheets

With increasingly large-scale deployments of photovoltaic (PV) modules to meet global energy demands, interest in better establishing modules' lifespans is growing. We report on the performance of co-extruded polyolefin- (PO)-based backsheets as environmentally friendly alternatives to fluoropolymer-reinforced polyethylene-terephthalate (PET)-based backsheets using three hygrometric accelerated test conditions. After completing cumulative 4000 hours of aging, we analyzed data from electrical performance (I-V), surface roughness (gloss), and appearance (L, a*, b* color) characterizations to quantify degradation rates, quantify the corresponding activation energy, and cross-correlate between the characteristics examined, thereby providing insights into the relationship between physical characteristics and operating performance.

BackFLIP↗

Development of Fixtures and Methods to Assess the Durability of Balance of Systems Components

The degradation of photovoltaic (PV) balance of systems (BoS) components is not well studied, but the consequences include offline modules, strings, and inverters; system shutdown; arc faults; and fires. A utility provider experienced a ~30% failure rate in their power transfer chain, originally attributed to branch connectors. Field-failed specimen assemblies were, therefore, examined, consisting of cable connector, branch connector, and discrete fuse components. In this study, unused field-vintage specimens are examined using a benchtop prototype fixture to identify the most influential environmental stressors on BoS components as well as the effect of external mechanical perturbation. The prototype fixture was used to develop a perturbation capability for future use in the combined-accelerated stress testing chamber. The benchtop experiments were also used to develop the in-situ data acquisition of specimen current, voltage, and temperature. A significant increase in operating temperature (~100 °C from ~40 °C) and a different failure mode (arcing at the metal pins rather than overheating of the fuse filament) were observed promptly once periodic mechanical perturbation was applied. The current at failure was decreased from 35 A (measured for static specimens, with failure occurring in the fuses) to 15 A (for tests with mechanical perturbation, with failure at the male/female metal pin connection). After initial examination using X-ray computed tomography, the external plastic was machined away from failed specimens to allow for failure analysis, including the extraction of the internal convolute springs for morphological examination (optical and electron microscopy). Chemical composition analysis included energy-dispersive X-ray spectroscopy, differential scanning calorimetry, and Fourier transform infrared spectroscopy.

14 SOLAR ENERGY↗

Evaluating the Durability of Balance of Systems Components Using Combined-Accelerated Stress Testing

The degradation of photovoltaic (PV) balance of systems (BoS) components is not well-studied, but the consequences include: offline-modules, -strings, -inverters; system shutdown; arc-faults; and fires. A utility provider experienced a ~30% failure rate in their power transfer chain, attributed to branch connectors. Field-failed specimen assemblies were therefore examined, consisting of cable connector, branch connector and discrete fuse components. Unused field-vintage specimens are presently being examined using combined-accelerated stress testing (C-AST) to clarify the most influential environmental stressors as well as the effect of external mechanical perturbation. A benchtop prototype fixture was used to develop the perturbation capability for C-AST. The benchtop experiments were also used to develop the in-situ data acquisition of specimen: current, voltage, and temperature. A significant increase in operating temperature, ~100 deg C from ~40 deg C, and a different failure mode was observed immediately once periodic mechanical perturbation was applied. The current at failure was decreased from 35 A (with failure occurring in the fuses) to 15 A (failure at the male/female metal pin connection). After initial examination using X-ray computed tomography, the external plastic was machined away from failed specimens to allow failure analysis, including the extraction of the internal convolute springs for morphological examination (optical- and electron-microscopy). Chemical composition analysis included: energy-dispersive X-ray spectroscopy, differential scanning calorimetry, and Fourier transform infrared spectroscopy.

balance of systems↗

Value Proposition of UV-Absorbers in PV Module Encapsulation

Various common crystalline silicon cell technologies were exposed to UVA radiation (1.24 Wm-2 nm-1 at 340 nm peak) on the front and back faces at 45 degrees Celsius for periods up to 3000 h, representing about 3 y of solar exposure in Phoenix, Arizona, USA. The resulting degradation of the open-circuit voltage and short-circuit current is presented. Of the various cell types examined, significant levels of degradation were seen in all cases. Less degradation was generally found after UV irradiation of cell fronts and older cell types, whereas a bifacial PERC type exposed on the rear showed about 25% degradation in short circuit current, attributable to lack of a diffused surface field. Selected cells were exposed to UV irradiation with the addition of long pass UV filters to replicate UV-absorbers in encapsulants. Modern cell designs are sensitive to UV-ID because of reduced or eliminated front and back surface field and increased dependence on high quality surface passivation. Single transformation of the independent variable (t, kW h/m^2) could be used to achieve a linear model of the data to extrapolate to 50 y. Solar Advisor Model (SAM) shows appropriate filtering of UV-irradiation can improve LCOE and net present value of plant. Some advanced cell types are seen to be UV-resistant (cell level solutions also exist). Solutions therefore exist on the cell, glass, and encapsulant level. Changes over time in each of these would also need to be considered (solarization, encapsulant browning...).

ENGINEERING,SOLAR ENERGY↗

A study of degradation mechanisms in PVDF-based photovoltaic backsheets

Abstract Commercial backsheets based on polyvinylidene fluoride (PVDF) can experience premature field failures in the form of outer layer cracking. This work seeks to provide a better understanding of the changes in material properties that lead to crack formation and find appropriate accelerated tests to replicate them. The PVDF-based backsheet outer layer can have a different structure and composition, and is often blended with a poly(methyl methacrylate) (PMMA) polymer. We observed depletion of PMMA upon aging with sequential (MAST) and combined (C-AST) accelerated stress testing. In field-aged samples from Arizona and India, where PVDF crystallizes in its predominant α-phase, the degree of crystallinity greatly increased. MAST and C-AST protocols were, to some extent, able to replicate the increase in crystallinity seen in PVDF after ~ 7 years in the field, but no single-stress test condition (UV, damp heat, thermal cycling) resulted in significant changes in the material properties. The MAST regimen used here was too extreme to produce realistic degradation, but the test was useful in discovering weaknesses of the particular PVDF-based outer layer structure studied. No excessive β-phase formation was observed after aging with any test condition; however, the presence of β-phase was identified locally by Fourier transform infrared spectroscopy (FTIR). We conclude that both MAST and C-AST are relevant tests for screening outdoor failure mechanisms in PVDF backsheets, as they were successful in producing material degradation that led to cracking.

14 SOLAR ENERGY↗

Perovskite Photovoltaics: Venturing Outdoors

Metal halide perovskite solar cells have shown promising performance, but mainly on small-area devices and under laboratory conditions. Now, researchers have demonstrated the fabrication of large-area devices assembled and packaged into modules and reported on their operation outdoors.

field testing↗

UV‐induced degradation of high‐efficiency silicon PV modules with different cell architectures

Abstract Degradation from ultraviolet (UV) radiation has become prevalent in the front of solar cells due to the introduction of UV‐transmitting encapsulants in photovoltaic (PV) module construction. Here, we examine UV‐induced degradation (UVID) in various commercial, unencapsulated crystalline silicon cell technologies, including bifacial silicon heterojunction (HJ), interdigitated back contact (IBC), passivated emitter and rear contact (PERC), and passivated emitter rear totally diffused (PERT) solar cells. We performed UV exposure tests using UVA‐340 fluorescent lamps at 1.24 W·m −2 (at 340 nm) and 45°C through 4.02 MJ·m −2 (2000 h). Our results showed that modern cell architectures are more vulnerable to UVID, leading to a significant power decrease (−3.6% on average; −11.8% maximum) compared with the conventional aluminum back surface field (Al‐BSF) cells (<−1% on average). The power degradation is largely caused by the decrease in short‐circuit current and open‐circuit voltage. A greater power decrease is observed in bifacial cells with rear‐side exposure compared with those with front‐side exposure, indicating that the rear side is more susceptible to UV damage. Secondary ion mass spectroscopy (SIMS) confirmed an increase in hydrogen concentration near the Si/passivation interface in HJ and IBC cells after UV exposure; the excess of hydrogen could result in hydrogen‐induced degradation and subsequently cause higher recombination losses. Additionally, surface oxidation and hot‐carrier damage were identified in PERT cells. Using a spectral‐based analysis, we obtained an acceleration factor of 5× between unpackaged cells (containing a silicon nitride antireflective coating on the front) in the UV test and an encapsulated module (with the front glass and encapsulant blocking 90% of the UV at 294 nm and 353 nm, respectively) in outdoor conditions. From the analytical calculations, we show that a UV‐blocking encapsulant can reduce UV transmission in the module by an additional factor of ~50.

14 SOLAR ENERGY↗

Chemical and mechanical interfacial degradation in bifacial glass/glass and glass/transparent backsheet photovoltaic modules

Abstract Glass/glass (G/G) photovoltaic modules are quickly rising in popularity, but the durability of modern G/G packaging has not yet been established. In this work, we examine the interfacial degradation modes in G/G and glass/transparent backsheet modules under damp heat (DH) with and without system bias voltage, comparing emerging polyolefin elastomer (POE) and industry‐standard poly(ethylene‐co‐vinyl acetate) (EVA) encapsulants. We investigate the transport of ionic species at cell/encapsulant interfaces, demonstrating that POE limits both sodium and silver ion migration compared with EVA. Changes to the chemical structures of the encapsulants at the cell/encapsulant interfaces demonstrate that both POE and EVA are more susceptible to degradation in modules with a transparent backsheet than in the G/G configuration. Adhesion testing reveals that POE and EVA have comparable critical debond energies after the DH exposures regardless of system bias polarity. The results of this study indicate that the interfacial degradation mechanisms of G/G appear to be similar to those of conventional glass/backsheet modules. For emerging materials, our results demonstrate that POE offers advantages over EVA but that transparent backsheets may accelerate encapsulant degradation due to increased moisture ingress when compared with the G/G structure.

14 SOLAR ENERGY↗

Arrhenius Analysis of the Degradation Modes in BackFLIP Study of Emerging Photovoltaic Backsheets: Preprint

With increasingly large-scale deployments of photovoltaic (PV) modules to meet global energy demands, interest in better establishing module lifespans is growing. We report on the performance of co-extruded polyolefin- (PO) based backsheets as environmentally friendly alternatives to fluoropolymer-reinforced polyethylene-terephthalate- (PET)-based backsheets using three hygrometric accelerated test conditions. After completing 4000 cumulative hours of aging, we analyzed data from electrical performance (I-V), surface roughness (gloss), and appearance (L, a*, b* color) characterizations are analyzed to quantify degradation rates, quantify the corresponding activation energy, and cross-correlate between the characteristics examined, thereby providing insights into the relationship between physical characteristics and operating performance.

BackFLIP↗

Accurately Quantifying Stress during Metal Halide Perovskite Thin Film Formation

The role of strain in metal halide perovskite (MHP) solar cells is still under investigation, showing both beneficial and detrimental effects on the device performance and stability. One crucial component to elucidating the impact of strain in the MHP absorber is a robust method of quantifying the amount of strain in the material. In this work, we present a parametric refinement approach based on grazing incidence wide-angle X-ray scattering and demonstrate its use on quantifying strain during thermal annealing and subsequent cooling as a function of substrate and processing route. We use the analysis to reveal the impact of the cubic-to-tetragonal phase transition during cooling on the material's strain and discuss texture formation as a potential strain-relief mechanism. Thereby we present both a robust approach to quantify strain in MHPs and potential mechanisms to control strain in the film, opening the path for further investigations of strain in MHPs.

14 SOLAR ENERGY↗

Dependence of adhesion on degradation mechanisms of ethylene co-vinyl acetate encapsulants over the lifetime of photovoltaic modules

The long-term reliability of encapsulation has a critical impact on the overall cost and effectiveness of photovoltaic modules. An often overlooked but important element of this reliability concerns adhesive degradation of the encapsulant, which results in delamination. This work critically examines the degradation mechanisms – deacetylation, β-scission, and hydrolytic depolymerization – primarily responsible for adhesion loss in ethylene co-vinyl acetate (EVA) encapsulants to provide evidence and clarity regarding the contribution of these mechanisms to the adhesive degradation over the lifetime of a module. EVA samples obtained from mini-modules exposed in two sets of controlled, accelerated conditions – with and without ultraviolet (UV) radiation – are characterized to find specific evidence for the proposed degradation mechanisms. The mini-modules were exposed up to 10,000 h, which represents up to 15–20 years in the field. Results affirm that initially, deacetylation dominates the degradation before scission takes over, followed by hydrolytic depolymerization. Additional analysis highlights the climacteric interdependency between deacetylation and hydrolytic depolymerization as it relates to eventual delamination, where deacetylation products catalyze interfacial hydrolysis reactions. Furthermore, effects occurring at a given interface are isolated, explicitly providing evidence for how these mechanisms are nonuniform throughout the thickness of the EVA. Results demonstrate that the EVA that interfaces with the glass as opposed to the cell experiences increased levels of degradation, explaining why this initially stronger interface becomes the preferential interface for delamination after longer periods of exposure. Additionally, elevated temperatures alone are shown to induce limited migration of sodium ions across the glass/EVA interface.

36 MATERIALS SCIENCE↗

Perovskite solar cells can take the heat

Solar panels must endure extreme conditions during their service lifetime. There are few other products, let alone pristine semiconductor electronics, that are manufactured today and expected to withstand decades of abuse from full exposure to outdoor elements, including harsh ultraviolet sunlight, rain and hail, and daily and seasonal thermal cycles. Over the past decade, a new class of semiconductors, known as metal halide perovskites, has emerged, which constitutes the light-absorbing material in solar panels and has made incredible advancements, potentially taking photovoltaics in new directions. Perovskite materials have been touted as a potential game changer for solar energy production.

14 SOLAR ENERGY↗

BACKFLIP: A Comparison of Emerging Non-Fluoropolymer-Based, Co-Extruded PV Backsheets to Industry-Benchmark Technologies

As the photovoltaic (PV) industry is rapidly expanding around the world, there has been an increasing interest in extending the lifespan of PV modules. Concern has also emerged regarding the recyclability of modules and their component materials, including fluoropolymer-based backsheets. Laminated polyethylene-terephthalate (PET) core backsheets have traditionally been used in the PV industry, but new, co-extruded polyolefin (PO) backsheets show promise as an improved alternative. Mini-module and coupon samples of seven different backsheets (made of layers including contemporary PET and fluoropolymers, novel PO, and polyamide (PA) materials) were run through hygrometric- or UV photolytic-accelerated aging to identify and better understand each material's degradation modes and the backsheets' field reliability. In addition to the artificial aging, the natural weathering methods used in this study are described. The comprehensive set of chemical, mechanical, and structural characterizations at intermittent read points in this study is presented, including: visual appearance and color; gloss; mechanical tensile testing; I-V performance; electroluminescence (EL) imaging; dielectric breakdown; FTIR-chemical structure; X-ray-polymer structure (WAXS); and DSC-crystalline content. After 4000 h of aging, a strong correlation occurs between initial physical characteristics (mechanical tensile test) and operating performance (EL and I-V characteristics). This presentation focuses on gloss, FTIR, and breakdown voltage measurements. Results for MiMo power, grayness from EL imaging, optical micrscopy, and specimen morphology (on extraction when cut from MiMos) is also presented.

backsheet↗