Search NASA⌕ Search

Engineering topics

Schmid, A. W.

Publications and source records attributed to Schmid, A. W..

Stress compensation in hafnia/silica optical coatings by inclusion of alumina layers

Hafnium dioxide films deposited using electron-beam evaporation tend to exhibit high tensile stresses, particularly when deposited on low-thermal-expansion substrates for use in a low-relative-humidity environment. Hafnia has been shown to be a critical material, however, for use in high-peak-power laser coatings, providing exceptional deposition control and laser-damage resistance. To correct for tensile thin-film stresses in hafnia/silica multilayer coatings, alumina compensation layers were incorporated in the multilayer design. Determination of the stresses resulting from alumina layers in different coating designs has led to the realization of the influence of water diffusion and the diffusion-barrier properties of alumina that must be considered. The inclusion of alumina layers in a hafnia/silica multilayer provides the ability to produce low-compressive-stress, high-laser-damage-threshold coatings.

36 MATERIALS SCIENCE↗

In situ detection and analysis of laser-induced damage on a 15-m multilayer-dielectric grating compressor for high-energy, petawatt-class laser systems

A grating-inspection system and a damage-analysis method have been developed to measure in situ laser-induced damage on a 1.5-m tiled-grating assembly of the OMEGA EP pulse compressor during a 15-ps, 2.2-kJ energy ramp. The beam fluence at which significant damage growth occurred was determined. This is the first report on beam fluence versus laser-induced-damage growth of meter-sized multilayer-dielectric-diffraction gratings. This result was correlated to the damage-probability measurement conducted on a small grating sample and is consistent with the fluence, corresponding to 100% damage probability.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Optimizing a cleaning process for multilayer-dielectric- (MLD) diffraction gratings

An essential component for the OMEGA EP short-pulse petawatt laser system is the grating compressor chamber (GCC). This large (12,375 ft 3 ) vacuum chamber contains critical optics where laser-pulse compression is performed at the output of the system on two 40-cm-sq-aperture, IR (1054-nm) laser beams. Critical to this compression, within the GCC, are four sets of tiled multilayer-dielectric- (MLD) diffraction gratings that provide the capability for producing 2.6-kJ output IR energy per beam at 10 ps. The primary requirements for these large-aperture (43-cm × 47-cm) gratings are diffraction efficiencies greater than 95%, peak-to-valley wavefront quality of less than λ/10 waves, and laser-induced-damage thresholds greater than 2.7 J/cm 2 at 10-ps measured beam normal. Degradation of the grating laser-damage threshold due to adsorption of contaminants from the manufacturing process must be prevented to maintain system performance. In this paper we discuss an optimized cleaning process to achieve the OMEGA EP requirements. The fabrication of MLD gratings involves processes that utilize a wide variety of both organic materials (photoresist processes) and inorganic materials (metals and metal oxides) that can affect the final cleaning process. Finally, a number of these materials have significant optical absorbance; therefore, incomplete cleaning of these residues may result in the MLD gratings experiencing laser damage.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗