Search NASA⌕ Search

Engineering topics

Sharafi, Asma

Publications and source records attributed to Sharafi, Asma.

System and method for treating the surface of solid electrolytes

Disclosed are electrochemical devices, such as lithium battery electrodes, lithium ion conducting solid state electrolytes, and solid-state lithium metal batteries including these electrodes and solid state electrolytes. In one embodiment, a method for forming an electrochemical device is disclosed in which a precursor electrolyte is heated to remove at least a portion of a resistive surface region of the precursor electrolyte.

Sakamoto, Junki↗

Interfacial Reactions and Performance of Li 7 La 3 Zr 2 O 12 -Stabilized Li–Sulfur Hybrid Cell

Herein, we report on the characterization of a Li–S hybrid cell containing a garnet solid electrolyte (Li 7 La 3 Zr 2 O 12 , LLZO) and conventional liquid electrolyte. While the liquid electrolyte provided ionically conductive pathways throughout the porous cathode, the LLZO acted as a physical barrier to protect the Li metal anode and prevent polysulfide shuttling during battery operation. This hybrid cell exhibited an initial capacity of 1000 mAh/g(S) and high Coulombic efficiency (>99%). The interface between the liquid electrolyte and LLZO was studied using electrochemical impedance spectroscopy and X-ray photoelectron spectroscopy (XPS). These results indicate that a spontaneous interfacial reaction layer formed between the LLZO and liquid electrolyte. XPS depth profiling experiments indicate that this layer consisted of Li-enriched phases near the surface (e.g., Li 2 CO 3 ) and intermediate Li–La–Zr oxides in subsurface regions. The reaction layer extended well beyond the LLZO surface, and bulk pristine LLZO was not observed even at the deepest sputtering depths used in this study (~90 nm). Overall, these results highlight that developing stable electrode/electrolyte interfaces is critical for solid-state batteries and their hybrids.

36 MATERIALS SCIENCE↗

Crystal Orientation-Dependent Reactivity of Oxide Surfaces in Contact with Lithium Metal

Understanding ionic transport across interfaces between dissimilar materials and the intrinsic chemical stability of such interfaces is a fundamental challenge spanning many disciplines and is of particular importance for designing conductive and stable solid electrolytes for solid-state Li-ion batteries. In this work, we establish a surface science-based approach for assessing the intrinsic stability of oxide materials in contact with Li metal. Through a combination of experimental and computational insights, using Nb-doped SrTiO3 (Nb/STO) single crystals as a model system, we were able to understand the impact of crystallographic orientation and surface morphology on the extent of the chemical reactions that take place between surface Nb, Ti, and Sr upon reaction with Li. By expanding our approach to investigate the intrinsic stability of the technologically relevant, polycrystalline Nb-doped lithium lanthanum zirconium oxide (Li6.5La3Zr1.5Nb0.5O12) system, we found that this material reacts with Li metal through the reduction of Nb, similar to that observed for Nb/STO. These results clearly demonstrate the feasibility of our approach to assess the intrinsic (in)stability of oxide materials for solid-state batteries and point to new strategies for understanding the performance of such systems.

36 MATERIALS SCIENCE↗

Impact of air exposure and surface chemistry on Li-Li 7 La 3 Zr 2 O 12 interfacial resistance

Li 7 La 3 Zr 2 O 12 (LLZO) is a promising solid-state electrolyte that could enable solid-state-batteries (SSB) employing metallic Li anodes. For a SSB to be viable, the stability and charge transfer kinetics at the Li–LLZO interface should foster facile plating and stripping of Li. Contrary to these goals, recent studies have reported high Li–LLZO interfacial resistance which was attributed to a contamination layer that forms upon exposure of LLZO to air. This study clarifies the mechanisms and consequences associated with air exposure of LLZO; additionally, strategies to minimize these effects are described. First-principles calculations reveal that LLZO readily reacts with humid air; the most favorable reaction pathway involves protonation of LLZO and formation of Li2CO3. X-ray photoelectron spectroscopy, scanning electron microscopy, Raman spectroscopy, and transmission electron microscopy were used to characterize the surface and subsurface chemistry of LLZO as a function of relative humidity and exposure time. Additionally, electrochemical impedance spectroscopy was used to measure the Li–LLZO interfacial resistance as a function of surface contamination. These data indicate that air exposure-induced contamination impacts the interfacial resistance significantly, when exposure time exceeds 24 h. The results of this study provide valuable insight into the sensitivity of LLZO to air and how the effects of air contamination can be reversed.

36 MATERIALS SCIENCE↗

Characterizing the Li–Li 7 La 3 Zr 2 O 12 interface stability and kinetics as a function of temperature and current density

The stability and kinetics of the Li–Li 7 La 3 Zr 2 O 12 (LLZO) interface were characterized as a function of temperature and current density. Polycrystalline LLZO was densified using a rapid hot-pressing technique achieving 97 ± 1% relative density, and <10% grain boundary resistance; effectively consisting of an ensemble of single LLZO crystals. It was determined that by heating to 175 °C, the room temperature Li-LLZO interface resistance decreases dramatically from 5822 (as-assembled) to 514 Ω cm 2 ; a > 10-fold decrease. In characterizing the maximum sustainable current density (or critical current density – CCD) of the Li-LLZO interface, several signs of degradation were observed. In DC cycling tests, significant deviation from Ohmic behavior was observed. In post-cycling tests, regions of metallic Li were observed; propagating parallel to the ionic current. For the cells cycled at 30, 70, 100, 130 and 160 °C, the CCD was determined to be 50, 200, 800, 3500, and 20000 μA cm –2 , respectively. As a result, the relationships and phenomena observed in this work can be used to better understand the Li-LLZO interface stability, enabling the use of batteries employing Li metal anodes.

36 MATERIALS SCIENCE↗