Search NASA⌕ Search

Engineering topics

Shyam, Amit

Publications and source records attributed to Shyam, Amit.

At least 91 records · Page 5

Hypervelocity Impact of Additively Manufactured A356/316L Interpenetrating Phase Composites

We have examined the hypervelocity impact response of targets made from monolithic A356 and 316L, as well as an additively manufactured A356/316L interpenetrating phase composite. 1.9 mm diameter spherical projectiles made from 2017 aluminum were fired at velocities of 5.9-6.1 km/s, allowing for the observation of multiple types of macro- and microstructural damage within each target. The macroscopic cratering damage to the A356/316L composite resembles that of the A356, but observations of both the cross section and the microstructural damage suggest that the A356/316L composite may be more resistant to spalling than A356 shielding with the same areal density.

French, Matthew↗

The effects of microstructural stability on the compressive response of two cast aluminum alloys up to 300 °C

Here in this study, the high temperature compressive response of cast aluminum alloys 319 and RR350 is compared in light of their microstructures. The 319 alloy is widely used in thermally critical automotive applications and provides a baseline for comparison with the RR350 alloy, whose microstructural stability at high homologous temperatures was recently reported. Cylindrical compression samples from each alloy were tested at four temperatures up to 300 °C at a constant true strain rate that was varied over four orders of magnitude. Although both alloys are strengthened by metastable precipitates (nominally Al 2 Cu) in the as-aged condition, their mechanical response diverges at temperatures greater than 250 °C as the strengthening precipitates evolve in the 319 alloy and retain their as-aged morphology in the RR350 alloy. Deformation mechanisms of each alloy are examined using microstructural analysis and empirical activation energy calculations. The stability of the θ' phase in the RR350 alloy leads to effective precipitation hardening at homologous temperatures up to 0.6 and an extensive regime of grain boundary controlled deformation.

36 MATERIALS SCIENCE↗

Comparative evaluation of cast aluminum alloys for automotive cylinder heads: Part II: Mechanical and thermal properties

The first part of this study documented the as-aged microstructure of five cast aluminum alloys namely, 206, 319, 356, A356, and A356+0.5Cu, that are used for manufacturing automotive cylinder heads (Roy et al. in Metall Mater Trans A, 2016). In the present part, we report the mechanical response of these alloys after they have been subjected to various levels of thermal exposure. In addition, the thermophysical properties of these alloys are also reported over a wide temperature range. The hardness variation due to extended thermal exposure is related to the evolution of the nano-scale strengthening precipitates for different alloy systems (Al-Cu, Al-Si-Cu, and Al-Si). The effect of strengthening precipitates (size and number density) on the mechanical response is most obvious in the as-aged condition, which is quantitatively demonstrated by implementing a strength model. Significant coarsening of precipitates from long-term heat treatment removes the strengthening efficiency of the nano-scale precipitates for all these alloys systems. Thermal conductivity of the alloys evolve in an inverse manner with precipitate coarsening compared to the strength, and the implications of the same for the durability of cylinder heads are noted.

36 MATERIALS SCIENCE↗

Comparative evaluation of cast aluminum alloys for automotive cylinder heads: Part I Microstructure evolution

The present study stages a comparative evaluation of microstructure and associated mechanical and thermal response for common cast aluminum alloys that are used for manufacturing automotive cylinder heads. The systems considered are Al-Cu (206-T6), Al-Si-Cu (319-T7), and Al-Si (356-T6, A356-T6, and A356 + 0.5Cu-T6). The focus of the present manuscript is on the evaluation of microstructure at various length scales after aging, while the second manuscript will deal with the mechanical and thermal response of these alloys due to short-term (aging) and long-term (pre-conditioning) heat treatments. At the grain-scale, the Al-Cu alloy possessed an equiaxed microstructure as opposed to the dendritic structure for the Al-Si-Cu or Al-Si alloys which is related to the individual solidification conditions for these alloy systems. The composition and morphology of intermetallic precipitates within the grain and at the grain/dendritic boundary are dictated by the alloy chemistry, solidification, and heat treatment conditions. At the nanoscale, these alloys contain various metastable strengthening precipitates (GPI and θ''θ'' in Al-Cu alloy, θ'θ' in Al-Si-Cu alloy, and β'β' in Al-Si alloys) with varying size, morphology, coherency, and thermal stability.

36 MATERIALS SCIENCE↗

Engineered glass seals for solid-oxide fuel cells

A seal for a solid oxide fuel cell includes a glass matrix having glass percolation therethrough and having a glass transition temperature below 650.degree. C. A deformable second phase material is dispersed in the glass matrix. The second phase material can be a compliant material. The second phase material can be a crushable material. A solid oxide fuel cell, a precursor for forming a seal for a solid oxide fuel cell, and a method of making a seal for a solid oxide fuel cell are also disclosed.

30 DIRECT ENERGY CONVERSION↗

Hot-tearing of multicomponent Al-Cu alloys based on casting load measurements in a constrained permanent mold

Hot-tearing is a major casting defect that is often difficult to characterize, especially for multicomponent Al alloys used for cylinder head castings. The susceptibility of multicomponent Al-Cu alloys to hot-tearing during permanent mold casting was investigated using a constrained permanent mold in which the load and displacement was measured. The experimental results for hot tearing susceptibility are compared with those obtained from a hot-tearing criterion based temperature range evaluated at fraction solids of 0.87 and 0.94. The Cu composition was varied from approximately 5 to 8 pct. (weight). Casting experiments were conducted without grain refining. The measured load during casting can be used to indicate the severity of hot tearing. However, when small hot-tears are present, the load variation cannot be used to detect and assess hot-tearing susceptibility.

Sabau, Adrian S↗

DPF Durability ORNL-04-0692

A substantial amount of testing and analysis was performed over the 13-year-duration of this Cooperative Research and Development Agreement (CRADA) between Cummins Inc. and the Oak Ridge National Laboratory (ORNL). ORNL's work focused on developing fundamental understanding of the mechanical and physical properties and their relationship to the microstructure of Diesel Particulate Filter (DPF) materials (i.e., cordierite, aluminum titanate, Si-SiC). These materials exhibit significant strain tolerance owing to their highly porous and mircocracked microstructures. That is, while very weak, the porous and compliant microstructure could withstand large strains without failing catastrophically. Substantial knowledge was also gained with respect to preparation of test specimens for evaluation of mechanical properties and the care required. Once the role of the microstructure of the wall material on its mechanical response was understood, the DPF honeycombs themselves were re-examined, and the influence of the honeycomb structure was considered. Cummins s work focused mainly on the apparent strength of the DPF honeycomb structure and using the material properties generated at ORNL for input to their regeneration and performance-predictive models.

36 MATERIALS SCIENCE↗

Young’s modulus and Poisson’s ratio changes due to machining in porous microcracked cordierite

Microstructural changes in porous cordierite caused by machining were characterized using microtensile testing, X-ray computed tomography and scanning electron microscopy. Young s moduli and Poisson s ratios were determined on ~215-380 um thick machined samples by combining digital image correlation and microtensile loading. The results provide evidence for an increase in microcrack density due to machining of the thin samples extracted from diesel particulate filter honeycombs.

36 MATERIALS SCIENCE↗

Onset of Plasticity via Relaxation Analysis (OPRA)

In crystalline metals and alloys, plasticity occurs due to the movement of mobile dislocations and the yield stress for engineering applications is traditionally quantified based on strain. The onset of irreversible plasticity or “yielding” is generally identified by a deviation from linearity in the stress-strain plot or by some standard convention such as 0.2 % offset strain relative to the “linear elastic response”. In the present work, we introduce a new methodology for the determination of the true yield point based on stress relaxation. We show experimentally that this determination is self-consistent in nature and, as such, provides an objective observation of the very onset of plastic flow. Lastly, our designation for yielding is no longer related to the shape of the stress-strain curve but instead reflects the earliest signature of the activation of concerted irreversible dislocation motion in a test specimen under increasing load.

36 MATERIALS SCIENCE↗

Small scale mechanical characterization of thin foil materials via pin load microtesting

In situ scanning electron microscope (SEM) experiments, where small-scale mechanical tests are conducted on micro- and nanosized specimens, allow direct visualization of elastic and plastic responses over the entirety of the volume being deformed. This enables precise spatial and temporal correlation of slip events contributing to the plastic flow evidenced in a stress–strain curve. A new pin-loading methodology has been employed, in situ within the SEM, to conduct microtensile tests on thin polycrystalline metal foils. This approach can be tailored to a specific foil whose particular grain size may range from microns to tens of microns. Manufacture of the specialized pin grip was accomplished via silicon photolithography-based processing followed by subsequent focused ion beam finishing. Microtensile specimen preparation was achieved by combining a stencil mask methodology employing broad ion beam sputtering along with focused ion beam milling in the study of several metallic foil materials. Finite-element analyses were performed to characterize the stress and strain distributions in the pin grip and micro-specimen under load. Furthermore, under appropriately conceived test conditions, uniaxial stress–strain responses measured within these foils by pin-load microtensile testing exhibit properties consistent with larger scale tests.

36 MATERIALS SCIENCE↗

Fracture toughness of plasma-sprayed thermal barrier ceramics: Influence of processing, microstructure, and thermal aging

Fracture toughness has become one of the dominant design parameters that dictates the selection of materials and their microstructure to obtain durable thermal barrier coatings (TBCs). Much progress has been made in characterizing the fracture toughness of relevant TBC compositions in bulk form, and it has become apparent that this property is significantly affected by process-induced microstructural defects. In this investigation, a systematic study of the influence of coating microstructure on the fracture toughness of atmospheric plasma sprayed (APS) TBCs has been carried out. Yttria partially stabilized zirconia (YSZ) coatings were fabricated under different spray process conditions inducing different levels of porosity and interfacial defects. Fracture toughness was measured on free standing coatings in as-processed and thermally aged conditions using the double torsion technique. Results indicate significant variance in fracture toughness among coatings with different microstructures including changes induced by thermal aging. Comparative studies were also conducted on an alternative TBC composition, Gd 2 Zr 2 O 7 (GDZ), which as anticipated shows significantly lower fracture toughness compared to YSZ. Furthermore, the results from these studies not only point towards a need for process and microstructure optimization for enhanced TBC performance but also a framework for establishing performance metrics for promising new TBC compositions.

36 MATERIALS SCIENCE↗

The Uniaxial Tensile Response of Porous and Microcracked Ceramic Materials

The uniaxial tensile stress-strain behavior of three porous ceramic materials was determined at ambient conditions. Test specimens in the form of thin beams were obtained from the walls of diesel particulate filter honeycombs and tested using a microtesting system. A digital image correlation technique was used to obtain full-field 2D in-plane surface displacement maps during tensile loading, and in turn, the 2D strains obtained from displacement fields were used to determine the Secant modulus, Young s modulus and initial Poisson s ratio of the three porous ceramic materials. Successive unloading-reloading experiments were performed at different levels of stress to decouple the linear elastic, anelastic and inelastic response in these materials. It was found that the stress-strain response of these materials was non-linear and that the degree of nonlinearity is related to the initial microcrack density and evolution of damage in the material.

anelasticity↗