On the kinetics of the pack - Aluminization process
An investigation has been made of the aluminization of unalloyed Ni in fluoride-activated packs of varying Al activity. In packs of low Al activity, in which the ratio of Al to Ni was less than 50 at. pct, the specimen surface quickly came to equilibrium with the pack and remained close to equilibrium for the duration of normal coating runs. In these packs the kinetics of aluminization was controlled by diffusion in the solid. In packs of higher Al activity the surface of the specimen did not come to equilibrium with the pack and the kinetics of the process was governed by a combination of solid and gas diffusion rates. Under most conditions however, the surface composition was time-invariant and a steady-state appeared to exist at the pack-coating interface. By combining Levine and Caves' model for gaseous diffusion in pure-Al packs with calculations of solid diffusion rates some success has been achieved in explaining the results.