Modeling the hydrodynamic impact on the tool influence function during hemispherical subaperture optical polishing

To fabricate high-precision and accurate optics relative to the optical design surface, a high level of deterministic control of material removal (i.e., the tool influence function, TIF) during subaperture tool polishing is required. In this study, a detailed analysis of the pressure distribution, which is a key component of the TIF, has been performed using finite element analysis to couple together solid mechanics and fluid dynamics. Modeling experimental parameters of recently published work reveals that, when considering tool deformation, which in turn influences the fluid film thickness between the tool and workpiece, the effective pressure profile has a flat-top distribution. This flat-top pressure profile differs from the parabolic pressure distributions predicted by Hertzian mechanics. Furthermore, the shear contribution is shown here to be a key contributor to material removal, inducing the removal at the periphery of the contact edge and even outside the generally accepted contact area. Finally, the simulated fluid velocities provide evidence of mixed-mode contact polishing, supporting recent experimental findings that also suggest that onset of hydroplaning contributions lead to material removal drop-off.

36 MATERIALS SCIENCE↗

Nanoplastic removal function and the mechanical nature of colloidal silica slurry polishing

The nanomechanical deformations on a broad range of optical material surfaces (single crystals of Al 2 O 3 [sapphire], SiC, Y 3 Al 5 O 12 [YAG], CaF 2 , and LiB 3 O 5 [LBO]; a SiO 2 –Al 2 O 3 –P 2 O 5 –Li 2 O glass-ceramics [Zerodur]; and glasses of SiO 2 :TiO 2 [ULE], SiO 2 [fused silica], and P 2 O 5 –Al 2 O 3 –K 2 O–BaO [Phosphate]) near the elastic-plastic load boundary have been measured by nanoindentation and nanoscratching to mimic the nanoplastic removal caused by a single slurry particle during polishing. Nanoindenation in air was performed to determine the workpiece hardness at various loads using a commercial nanoindenter with a Berkovich tip. Similarly, an atomic force microscope (AFM) with a stiff diamond coated tip (150 nm radius) was used to produce nanoplastic scratches in air and aqueous environments over a range of applied loads (~20-170 μN). The resulting nanoplastic deformation of the nanoscratches were used to calculate the removal function (i.e., depth per pass) which ranged from 0.18 to 3.6 nm per pass for these materials. A linear correlation between the nanoplastic removal function and the polishing rate (using a fixed polishing process with colloidal silica slurry on a polyurethane pad) of these materials was observed implying that: (a) the polishing mechanism using colloidal silica slurry can be dominated by mechanical rather than chemical interactions; and (b) the nanoplastic removal function, as opposed to interface particle interactions, is the controlling factor for the polishing material removal rate. Furthermore, this correlation is consistent with the Ensemble Hertzian Multi-Gap (EHMG) microscopic material removal rate model described previously. The nanoplastic removal depth was also found to correlate to the measured nanoindentation hardness (H1) of the optical material, scaling as H 1 -3.5 . Two-dimensional (2D) finite element analysis simulations of nanoindentation showed a similar nonlinear dependence of plastic deformation with the workpiece material hardness. The findings of this study are used to determine an effective Preston coefficient for the material removal rate expression and enhance the predictive nature of the nanoplastic polishing rate for various materials utilizing their material properties.

36 MATERIALS SCIENCE↗

Relationship between surface μ‐roughness and interface slurry particle spatial distribution during glass polishing

Abstract During optical glass polishing, a number of interactions between the workpiece (i.e., glass), polishing slurry, and pad can influence the resulting workpiece roughness at different spatial scale lengths. In our previous studies, the particle size distribution of the slurry, the pad topography, and the amount of material removed by a single particle on the workpiece were shown to strongly correlate with roughness at AFM scale lengths (nm‐μm) and weakly at μ‐roughness scale lengths (μm‐mm). In this study, the polishing slurry pH and the generation of glass removal products are shown to influence the slurry particle spatial and height distribution at the polishing interface and the resulting μ‐roughness of the glass workpiece. A series of fused silica and phosphate glass samples were polished with various ceria and colloidal silica slurries over a range of slurry pH , and the resulting AFM roughness and μ‐roughness were measured. The AFM roughness was largely invariant with pH , suggesting that the removal function of a single particle is unchanged with pH . However, the μ‐roughness changed significantly, increasing linearly with pH for phosphate glass and having a maximum at an intermediate pH for fused silica. In addition, the spatial and height distribution of slurry particles on the pad (as measured by laser confocal microscopy) was determined to be distinctly different at low and high pH during phosphate glass polishing. Also, the zeta potential as a function of pH was measured for the workpiece, slurry, and pad with and without surrogate glass products (K 3 PO 4 for phosphate glass and Si( OH ) 4 for silica) to assess the role of interfacial charge during polishing. The addition of K 3 PO 4 significantly raised the zeta potential, whereas addition of Si( OH ) 4 had little effect on the zeta potential. An electrostatic DLVO three‐body force model, using the measured zeta potentials, was used to calculate the particle–particle, particle–workpiece, and particle–pad attractive and repulsive forces as a function of pH and the incorporation of glass products at the interface. The model predicted an increase in particle–pad attraction with an increase in pH and phosphate glass products consistent with the measured slurry distribution on the pads during phosphate glass polishing. Finally, a slurry “island” distribution gap ( IDG ) model has been formulated which utilizes the measured interface slurry distributions and a load balance to determine the interface gap, the contact area fraction, and the load on each slurry “island”. The IDG model was then used to simulate the workpiece surface topography and μ‐roughness; the results show an increase in roughness with pH similar to that observed experimentally.

Suratwala, Tayyab↗

Nanoscratching of Optical Glass Surfaces Near the Elastic–Plastic Load Boundary to Mimic the Mechanics of Polishing Particles

The nanomechanical deformations on glass surfaces near the elastic–plastic load boundary have been measured on various glasses by nanoscratching using an atomic force microscope (AFM) to mimic the mechanical interactions of polishing particles during optical polishing. Nanoscratches were created in air and aqueous environments using a 150-nm radius diamond-coated tip on polished fused silica, borosilicate, and phosphate glass surfaces; the topology of the nanoscratches were then characterized by AFM. Using load ranges expected on slurry particles during glass polishing (0.05–200 μN), plastic-type scratches were observed with depths in the nm range. Nanoscratching in air generally showed deeper & narrower scratches with more pileup compared to nanoscratching in water, especially on fused silica glass. The critical load needed to observe plastic deformation was determined to range from 0.2–1.2 μN for the three glasses. For phosphate glass, the load dependence of the removal depth was consistent with that expected from Hertzian mechanics. However, for fused silica and borosilicate glass in this load range, the deformation depth showed a weak dependence with load. Using a sub-Tg annealing technique, material relaxation was observed on the nanoscratches, suggesting that a significant fraction of the deformation was due to densification on fused silica and borosilicate glass. Repeated nanoscratching at the same location was utilized for determining the effective incremental plastic removal depth. The incremental removal depth decreased with increase in number of passes, stabilizing after ~10 passes. In water, the removal depths were determined as 0.3–0.55 nm/pass for fused silica, 0.85 nm/pass for borosilicate glass, and 2.4 nm/pass for phosphate glass. The combined nanoscratching results were utilized to define the composite removal function (i.e., removal depth) for a single polishing particle as a function of load, spanning the chemical to the plastic removal regimes. Finally, this removal function serves as an important set of parameters in understanding material removal during polishing and the resulting workpiece surface roughness.

47 OTHER INSTRUMENTATION↗

Chemistry and Formation of the Beilby Layer During Polishing of Fused Silica Glass

The chemical characteristics and the proposed formation mechanisms of the modified surface layer (called the Beilby layer) on polished fused silica glasses are described. Fused silica glass samples were polished using different slurries, polyurethane pads, and at different rotation rates. The concentration profiles of several key contaminants, such as Ce, K, and H, were measured in the near surface layer of the polished samples using Secondary Ion Mass Spectroscopy (SIMS). The penetration of K, originating from KOH used for pH control during polishing, decreased with increase in polishing material removal rate. In contrast, penetration of the Ce and H increased with increase in polishing removal rate. In addition, Ce penetration was largely independent of the other polishing parameters (e.g., particle size distribution and the properties of the polishing pad). The resulting K concentration depth profiles are described using a two-step diffusion process: (1) steady-state moving boundary diffusion (due to material removal during polishing) followed by (2) simple diffusion during ambient postpolishing storage. Using known alkali metal diffusion coefficients in fused silica glass, this diffusion model predicts concentration profiles that are consistent with the measured data at various polishing material removal rates. On the other hand, the observed Ce profiles are inconsistent with diffusion based transport. Rather we propose that Ce penetration is governed by the ratio of Ce–O–Si and Si–O–Si hydrolysis rates; where this ratio increases with interface temperature (which increases with polishing material removal rate) resulting in greater Ce penetration into the Beilby layer. Calculated Ce surface concentrations using this mechanism are in good agreement to the observed change in measured Ce surface concentrations with polishing material removal rate. In conclusion, these new insights into the chemistry of the Beilby layer, combined together with details of the single particle removal function during polishing, are used to develop a more detailed and quantitative picture of the polishing process and the formation of the Beilby layer.

36 MATERIALS SCIENCE↗