Comparison of Residual Stress in SRS and LANL-welded 3013 Inner Containers
Explore the source record for details and available documents.
Engineering topics
Publications and source records attributed to Stroud, Mary Ann.
Explore the source record for details and available documents.
A high-purity fuel-grade plutonium dioxide material from the Material Identification and Surveillance (MIS) Program inventory has been studied with regard to gas generation and corrosion in a storage environment. Sample PBO-47-09-012-023 originated from the Hanford continuous oxalate precipitation and calcination process and represents plutonium oxides from multiple processes currently stored in 3013 containers. After calcination to 950°C, the material contained 87.5% plutonium/americium with no major impurities. This study followed over time the gas pressure of a sample with nominally 0.5 wt% water in a sealed container with an internal volume scaled to 1/400 th of the volume of a 3013 container. Gas compositions were measured periodically over a three year period. The maximum observed gas pressure was 96 kPa. The increase over the initial pressure was primarily due to generation of hydrogen (5.7 kPa) and nitrogen (2 kPa) gas. Oxygen was a minor component of the initial headspace gas and was depleted. At the completion of the study, the internal components of the sealed container did not show significant signs of corrosion.
A high-purity uranium/plutonium mixed oxide material from the Material Identification and Surveillance (MIS) Program inventory has been studied with regard to gas generation and corrosion in a storage environment. Sample 5501579 represents process plutonium oxides from high purity mixed oxides and mixed oxides from alloy oxidation at Hanford, hydride oxide from Rocky Flats, and mixed oxides from alloy oxidation and scrap mixed oxides at Savannah River that are currently stored in 3013 containers. This study followed over time the gas pressure of two samples of this material with nominally 0.5 wt% water in a sealed container with an internal volume scaled to 1/500th of the volume of a 3013 container. The first experiment studied a mixture of 60% as-received material (AR) and 40% material that had been calcined at 950 °C. The mixture contained 66% weapons grade plutonium and 11% uranium, with approximately 7.3% impurities and the remainder principally oxygen. A second experiment studied material calcined at 950 °C which contained approximately 4.3% impurities and similar uranium and plutonium content. Gas compositions were measured periodically over approximately 3.5 years in the first container and 20 months for the second container, which was terminated early due to an inadvertent container pumpdown. The maximum observed gas pressures were 152 kPa and 161 kPa, respectively. The increase over the initial pressures of 82 kPa and 88 kPa, respectively, was primarily due to generation of carbon dioxide and nitrogen gases. In the container with the AR/calcined mixture, a small amount of hydrogen and oxygen was generated and was consumed. In the container with calcined material only, hydrogen partial pressure of 18.9 kPa was measured. A small amount of oxygen was generated and was consumed. At the completion of the study, the internal components of both sealed containers showed signs of corrosion
A high purity plutonium dioxide material from the Material Identification and Surveillance (MIS) Program inventory has been studied with regard to gas generation and corrosion in a storage environment. Sample MT1490 represents process plutonium oxides from several metal oxidation operations that are currently stored in 3013 containers. This study followed over time, the gas pressure of a sample with nominally 0.5 weight percent water in a sealed container with an internal volume scaled to 1/500 th of the volume of a 3013 container. The sample was a mixture of as-received material, material calcined at 800°C and material calcined at 950°C. This material contained 87% plutonium with no major impurities. Gas compositions were measured periodically over a nine year period. The maximum observed gas pressure of 118 kPa was reached during the ninth year. The increase over the initial pressure of 95 kPa was primarily due to generation of nitrogen and hydrogen gas. Oxygen was a minor component of the headspace gas. At the completion of the study, the inner bucket showed signs of corrosion, including pitting, in the container material contact region.
A high-purity uranium/plutonium mixed oxide material from the Material Identification and Surveillance (MIS) Program inventory has been studied with regard to gas generation and corrosion in a storage environment. Sample SCP711-56 represents process plutonium oxides from mixed oxides at the Hanford Site, byproduct plutonium/uranium mixed oxides at the Rocky Flats Plant, Hanford Site mixed oxides at Savannah River, mixed oxides from alloy oxidation at Savannah River, scrap mixed oxides at Savannah River and plutonium/uranium oxide at Los Alamos National Laboratory that are currently stored in 3013 containers. After calcination to 950°C the material contains 17% fuel grade plutonium and 68% uranium with approximately 1.5% impurities and the remainder principally oxygen. This study followed over time the gas pressure of a sample with nominally 0.1 wt% water in a sealed container with an internal volume scaled to 1/500th of the volume of a 3013 container. Gas compositions were measured periodically over approximately 4 years. The maximum observed gas pressure was 115 kPa. The increase over the initial pressure of 83 kPa was primarily due to generation of carbon dioxide and nitrogen gases. A small amount of hydrogen was generated and oxygen was consumed. At the completion of the study, the internal components of the sealed container showed signs of corrosion, including pitting.
A high-purity, reactor-grade plutonium dioxide material from the Material Identification and Surveillance (MIS) Program inventory has been studied with regard to gas generation and corrosion in a storage environment. BLO-39-11-14-004 is a high specific power oxide that represents Hanford process plutonium oxides from oxalate process product, oxalate precipitation of impure plutonium and pure mixed uranium/plutonium nitrate solutions, PFP NDA and impure and scrap plutonium oxides 80-85% from PFP and the 300 area. It also represents plutonium oxides from oxalate precipitation at LANL and Savannah River. After calcination to 950 °C, the material contained 80% plutonium and 7% americium with no major impurities. This study followed over time the gas pressure of a sample with nominally 0.5 wt% water in a sealed container with an internal volume scaled to 1/500th of the volume of a 3013 container. A leak occurred in the original reactor (SSR132) which was terminated after 3 years. The sample was reloaded (SSR132A) and an additional set of data was collected. Results from both loadings are discussed. Gas compositions were measured periodically over three (SSR132) and four and a half (SSR132A) year periods. The maximum observed gas pressures were 93 kPa and 94 kPa, respectively. The increase over the initial pressure was primarily due to generation of nitrogen gas. For SSR132, the maximum observed gas pressure for hydrogen was 1.2 kPa and oxygen was 9.3 kPa (includes oxygen from leak). For SSR132A, the maximum observed gas pressure for hydrogen was 5.5 kPa and oxygen was 0.9 kPa. At the completion of the study, the internal components of the sealed container showed limited signs of corrosion.
Surveillance of vented, stainless-steel Hagan and SAVY-4000 storage containers with some plutonium materials have revealed evidence of corrosion inside the container. There are ∼3000 items stored in Hagan containers and ∼600 items currently stored in SAVY-4000 containers at TA-55. The Hagan is made of 304L steel while the SAVY is made of 316L and should be less susceptible to corrosion. Given the relatively thin body wall of these containers (nominally 0.762 millimeters), it is essential to understand the effects of corrosion on the lifetime of the containers to ensure worker safety. Studies are being conducted on both container types to determine the relative susceptibility of the two containers to corrosion. This paper will describe the potential cause of the corrosion, the extent of corrosion, the types of corrosion observed, along with the results of accelerating aging experiments. The combined results of the surveillance and lifetime extension studies will be used to predict the container lifetime. (authors)
Surveillance of vented, stainless-steel Hagan and SAVY-4000 storage containers with some plutonium materials has revealed evidence of corrosion inside the container. There are ~3000 items stored in Hagan containers and ~600 items currently stored in SAVY-4000 containers at TA -55. The Hagan is made of 304L steel, while the SAVY-4000 is made of 316L and should be less susceptible to corrosion. Given the relatively thin body wall of these containers (nominally 0.762 millimeters), it is essential to understand the effects of corrosion on the lifetime of the containers to ensure worker safety. Studies are being conducted on both container types to determine the relative susceptibility of the two containers to corrosion. This paper describes the potential cause of corrosion, the extent of corrosion, and types of corrosion observed, along with the results of accelerated aging experiments. The combined results of the surveillance and lifetime extension studies establish a technical basis for extending the design life of the stainless steel components of the SAVY-4000 container from 5 years to 15 years.
Explore the source record for details and available documents.
A high-purity plutonium dioxide material from the Material Identification and Surveillance (MIS) Program inventory has been studied with regard to gas generation and corrosion in a storage environment. Sample 5501579 represents process plutonium oxides from hydride oxide from Rocky Flats that are currently stored in 3013 containers. After calcination to 950°C, the material contained 87.42% plutonium with no major impurities. This study followed over time, the gas pressure of a sample with nominally 0.5 wt% water in a sealed container with an internal volume scaled to 1/500th of the volume of a 3013 container. Gas compositions were measured periodically over a six year period. The maximum observed gas pressure was 124 kPa. The increase over the initial pressure of 70 kPa was primarily due to generation of nitrogen and carbon dioxide gas. Hydrogen and oxygen were minor components of the headspace gas. At the completion of the study, the internal components of the sealed container showed signs of corrosion.
A set of six long-term, full-scale experiments were initiated to determine the type and extent of corrosion that occurs in 3013 containers packaged with chloride-bearing plutonium oxide materials. The materials were exposed to a high relative humidity environment representative of actual packaging conditions for the materials in storage. The materials were sealed in instrumented, inner 3013 containers with corrosion specimens designed to test the corrosiveness of the environment inside the containers under various conditions. This report focuses on initial loading conditions that are used to establish a baseline to show how the conditions change throughout the storage lifetime of the containers.
Chloride-induced stress corrosion cracking (SCC) has been investigated as a potential failure mechanism for the SAVY 4000 and the Hagan containers used to store plutonium-bearing materials at Los Alamos National Laboratory. This report discusses the regions of the container bodies most susceptible to SCC and the magnitude of the residual stresses in those regions. Boiling MgCl2 testing indicated that for both containers the region near the top weld was most susceptible to SCC. The Hagan showed through wall cracking after 22-24 hours of exposure both parallel (axial stresses) and perpendicular (hoop stresses) to the weld. The SAVY 4000 container showed significant cracking above and below the weld after 47 hours of exposure but there was no visual evidence of a through wall crack and the cracks did not leak water. Two through wall holes formed in the bottom of the SAVY 4000 container after 44-46 hours of exposure. For both containers, average “through wall” residual stresses were determined from hole drilling data 4 mm below the weld. In the Hagan body, average tensile hoop stresses were 194 MPa and average compressive axial stresses were -120 MPa. In the SAVY 4000 body, average compressive hoop stresses were 11 MPa and average tensile axial stresses were 25 MPa. Results suggest that because the Hagan container exhibited through wall cracking in a shorter time in boiling MgCl2 and had the higher average tensile stress, 194 MPa hoop stress, it is more susceptible to SCC than the SAVY 4000 container.
Since the late 1990’s, the Hagan container was used as the primary container for packaging of plutonium-bearing materials. The Hagan design consisted of a threaded closure, a Viton® ORing, a carbon-carbon filter, and a 304L stainless steel (SS) body. Over the years, Hagans have shown vulnerability in their design [1]. In 2008, The Department of Energy (DOE) issued DOE M 441.1-1, Nuclear Material Packaging Manual, which detailed an approach to obtain highconfidence in containers by including specific design requirements, material contents and an approach to determine life span from said contents, and surveillance techniques [2]. In response to both the vulnerability issues with the Hagan and DOE M 441.1-1, the SAVY 4000 container with its twist style closure, Viton® O-Ring, Fiberfrax-Gortex filter, and annealed 316L SS body, was designed as the replacement for Hagan containers, but only for a short term lifespan of 5 years [1]. However, both the Hagan and SAVY 4000 are being pushed to maintain a lifespan of 40 years. Therefore, proper confidence must be placed on each component of each container to last a minimum of 40 years. So far, the biggest concern found during surveillance of these containers is corrosion and the potential for failure by corrosion. One concern is that the containers fail due to stress corrosion cracking (SCC), especially around the weld between the collar and the body as welds leave residual stresses. One advantage the SAVY 4000 has is that the body is annealed, but its weld is still susceptible as it was welded after annealing [3, 4]. Moreover, 316L SS is known to have a higher pitting resistance (pits are a precursor to SCC and can also lead to extensive failure of the material), than 304L SS [4]. During recent surveillance activities, two SAVY 4000’s containing Solution Assay Instrument (SAI) solutions were opened. The SAI SAVY 4000’s contained plutonium (Pu) in 3M HCl solution in plastic volumetric flasks placed inside of polyethylene bags. Historically, a SAVY 4000 containing an SAI solution is packaged for 3 weeks, however, these particular containers were not reopened until 14 months later. When opened, brown-red corrosion product was found all over the inside of the container as shown in Figure 1.
Explore the source record for details and available documents.
A high-purity plutonium dioxide material from the Material Identification and Surveillance (MIS) Program inventory has been studied with regard to gas generation and corrosion in a storage environment. Sample TS707001 represents process plutonium oxides from several metal oxidation operations as well as impure and scrap plutonium from Hanford that are currently stored in 3013 containers. After calcination to 950°C, the material contained 86.98% plutonium with no major impurities. This study followed over time, the gas pressure of a sample with nominally 0.5 wt% water in a sealed container with an internal volume scaled to 1/500th of the volume of a 3013 container. Gas compositions were measured periodically over a six year period. The maximum observed gas pressure was 138 kPa. The increase over the initial pressure of 80 kPa was primarily due to generation of nitrogen and carbon dioxide gas in the first six months. Hydrogen and oxygen were minor components of the headspace gas. At the completion of the study, the internal components of the sealed container showed signs of corrosion, including pitting.
The Department of Energy’s 3013 Standard for packaging plutonium-bearing materials for storage up to fifty years specifies a minimum of two individually welded, nested containers herein referred to as the 3013 outer and the 3013 inner.1 Stress corrosion cracking (SCC) is a potential failure mechanism for 3013 inner containers.2,3 The bagless transfer container (BTC), a 3013 inner container used by Hanford and Savanna River Site (SRS) made from 304L stainless steel (SS), poses the greatest concern for SCC.4,5 The Surveillance and Monitoring Program (SMP) use stressed metal samples known as teardrops as screening tools in SCC studies to evaluate factors that could result in cracks in the 3013 containers.6,7 This report provides background information on the teardrops used in the Los Alamos National Laboratory (LANL) SMP studies including method of construction, composition and variability. In addition, the report discusses measurements of residual stresses in teardrops and compares the results with residual stresses in BTCs reported previously.4 Factors affecting residual stresses, including teardrop dimensions and surface finish, are also discussed.
A mixture of chlorine-containing, impure plutonium oxides has been produced and has been given the name Master Blend. This large quantity of well-characterized chlorinecontaining material is available for use in the Integrated Surveillance and Monitoring Program for shelf-life experiments. It is intended to be representative of materials packaged to meet DOE-STD-3013.1 The Master Blend contains a mixture of items produced in Los Alamos National Laboratory’s (LANL) electro-refining pyrochemical process in the late 1990s. Twenty items were crushed and sieved, calcined to 800ºC for four hours, and blended multiple times. This process resulted in four batches of Master Blend. Calorimetry and density data on material from the four batches indicate homogeneity.
This report is an assessment performed by LANL that examines packaging for plutonium-bearing materials and the resilience of its design. This report discusses residual stresses in the 3013 outer, the SRS/Hanford and RFETS/LLNL inner containers, and teardrop samples used in studies to assess the potential for SCC in 3013 containers. Residual tensile stresses in the heat affected zones of the closure welds are of particular concern.