Search NASA⌕ Search

Engineering topics

Sun, Yuanwei

Publications and source records attributed to Sun, Yuanwei.

A native oxide high-κ gate dielectric for two-dimensional electronics

Silicon-based transistors are approaching their physical limits and thus new high-mobility semiconductors are sought to replace silicon in the microelectronics industry. Both bulk materials (such as silicon-germanium and III–V semiconductors) and low-dimensional nanomaterials (such as one-dimensional carbon nanotubes and two-dimensional transition metal dichalcogenides) have been explored, but, unlike silicon, which uses silicon dioxide (SiO 2 ) as its gate dielectric, these materials suffer from the absence of a high-quality native oxide as a dielectric counterpart. This can lead to compatibility problems in practical devices. Here, we show that an atomically thin gate dielectric of bismuth selenite (Bi 2 SeO 5 ) can be conformally formed via layer-by-layer oxidization of an underlying high-mobility two-dimensional semiconductor, Bi 2 O 2 Se. Using this native oxide dielectric, high-performance Bi 2 O 2 Se field-effect transistors can be created, as well as inverter circuits that exhibit a large voltage gain (as high as 150). The high dielectric constant (~21) of Bi 2 SeO 5 allows its equivalent oxide thickness to be reduced to 0.9 nm while maintaining a gate leakage lower than thermal SiO 2 . The Bi 2 SeO 5 can also be selectively etched away by a wet chemical method that leaves the mobility of the underlying Bi 2 O 2 Se semiconductor almost unchanged.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Characterization of hot extrusion and heat treatment on mechanical properties in a spray formed ultra-high strength Al-Zn-Mg-Cu alloy

Highlights: • The spray forming technology was used to fabricate ultra-high strength aluminum alloy. • The alloy under RRA state obtained the highest ultimate tensile strength of 732 MPa. • The effects of dislocations, solutes and precipitates etc., on yield strength were calculated. • Precipitation was characterized as the main strengthening mechanism for aging states. - Abstract: To obtain the optimal mechanical properties, several processes including spray forming technology, two passes hot extrusion and substantial heating treatments were operated on an Al-Zn-Mg-Cu-Zr alloy. The characterization methods used in this study include tensile tests, X-ray diffraction, differential scanning calorimetry and microstructure observations by optical microscope, scanning and transmission electron microscopy. The typical characteristics were the refined grain, homogeneous precipitates and porosity in the as-deposited pre-forms. The ultimate tensile strength, yield strength, hardness and elongation improved significantly after two passes hot extrusion. A good combination of ultimate tensile strength at 704 MPa and elongation at 9.7% were achieved under peak-aged treatment. The best ultimate tensile strength was obtained at 732 MPa after re-aging and regression. It was main dimple fracture in the extruded and aging treated specimens while brittle fracture for the as-deposited. The secondary phases were main MgZn{sub 2} and Al{sub 3}Zr dispersoids throughout all the states. The contributions of grain boundaries, dislocations, solid-solution and precipitates on the yield strength were analyzed using a quantitative equation.

36 MATERIALS SCIENCE↗