Electrochemical Redox Behavior of Li Ion Conducting Sulfide Solid Electrolytes
Not provided.
Engineering topics
Publications and source records attributed to Swamy, Tushar.
Not provided.
Mechanical and electrochemical phenomena are coupled in defining the battery reliability, particularly for solid-state batteries. Micro-cracks act as barriers to Li-ion diffusion in the electrolyte, increasing the average electrode’s tortuosity. In our previous work, we showed that solid electrolytes are likely to suffer from mechanical degradation if their fracture energy is lower than 4 J m -2 [G. Bucci, T. Swamy, Y.-M. Chiang, and W. C. Carter, J. Mater. Chem. A (2017)]. Here we study the effect of electrolyte micro-cracking on the effective conductivity of composite electrodes. Via random analyzes, we predict the average diffusivity of lithium in a solid-state electrode to decrease linearly with the extension of mechanical degradation. Furthermore, the statistical distribution of first passage times indicates that the microstructure becomes more and more heterogeneous as damage progresses. In addition to power and capacity loss, a non-uniform increase of the electrode tortuosity can lead to heterogeneous lithiation and further stress localization. Finally, the understanding of these phenomena at the mesoscale is essential to the implementation of safe high-energy solid-state batteries.
A flexural bearing mechanism has enabled the development of a self-sealing box for protecting air sensitive samples during transfer between glove boxes, micro-machining equipment, and microscopy equipment. The simplicity and self-actuating feature of this design makes it applicable to many devices that operate under vacuum conditions. The models used to design the flexural mechanism are presented in detail. Lastly, the device has been tested in a Zeiss Merlin GEMINI II scanning electron microscope with Li 3 PS 4 samples, showing effective isolation from air and corrosion prevention.
This study is the first quantitative analysis of mechanical reliability of all-solid state batteries. Mechanical degradation of the solid electrolyte (SE) is caused by intercalation-induced expansion of the electrode particles, within the constrains of a dense microstructure. A coupled electro-chemo-mechanical model was implemented to quantify the material properties that cause an SE to fracture. The treatment of microstructural details is essential to the understanding of stress-localization phenomena and fracture. A cohesive zone model is employed to simulate the evolution of damage. In the numerical tests, fracture is prevented when electrode-particle's expansion is lower than 7.5% (typical for most Li-intercalating compounds) and the solid-electrolyte's fracture energy higher than G c = 4 J m -2 . Perhaps counter-intuitively, the analyses show that compliant solid electrolytes (with Young's modulus in the order of E SE = 15 GPa) are more prone to micro-cracking. This result, captured by our non-linear kinematics model, contradicts the speculation that sulfide SEs are more suitable for the design of bulk-type batteries than oxide SEs. Mechanical degradation is linked to the battery power-density. Fracture in solid Li-ion conductors represents a barrier for Li transport, and accelerates the decay of rate performance.
Here, Young's modulus, hardness, and fracture toughness are measured by instrumented nanoindentation for an amorphous Li 2 S–P 2 S 5 Li-ion solid electrolyte. Although low elastic modulus suggests accommodation of significant chemomechanical strain, low fracture toughness can facilitate brittle crack formation in such materials.
Since the gravimetric lithiation capacity of silicon is roughly ten times that of graphite, while their mass densities are comparable, for the same particle size the current density required to cycle a silicon electrode at a given C-rate is about ten times greater than that of graphite. Depending on the magnitude of the corresponding Butler-Volmer exchange current density, j o , such high current densities may cause the charge transfer kinetics at the silicon-electrolyte interface to become rate limiting. Previously reported values of j o for Si differ by about 10 orders of magnitude. Here we report j o measurements using electrochemical impedance spectroscopy (EIS) for single crystal electronically conductive silicon wafers with well-defined (100) and (111) orientations and active surface areas. The electrochemical cycling regime was designed to avoid artifacts due to stress-induced surface cracking of Si upon lithiation. The exchange current density of the silicon-electrolyte interface is found to be 0.1 ± 0.01 mA/cm 2 when using electrolyte consisting of 1 M LiPF 6 in EC/DMC (1/1 by wt) + FEC (10 wt%) + VC (2 wt%). Furthermore, these results are then used to illustrate the dependence of kinetic overpotential on particle size and C-rate for silicon compared to lower volumetric capacity compounds such as graphite.