Search NASA⌕ Search

Engineering topics

Toops, Todd J

Publications and source records attributed to Toops, Todd J.

49 records · Page 3

Deactivation of Accelerated Engine-Aged and Field-Aged Fe-Zeolite SCR Catalysts

A single-cylinder diesel engine with an emissions control system - diesel oxidation catalyst (DOC), Fe-zeolite selective catalytic reduction (SCR) catalyst, and diesel particulate filter (DPF) - was used to perform accelerated thermal aging of the SCR catalyst. Cyclic aging is performed at SCR inlet temperatures of 650, 750 and 850 degrees C for up to 50 aging cycles. To assess the validity of the implemented accelerated thermal aging protocol, a field-aged SCR catalyst of similar formulation was also evaluated. The monoliths were cut into sections and evaluated for NO{sub x} performance in a bench-flow reactor. While the rear section of both the field-aged and the accelerated engine-aged SCR catalysts maintained high NO{sub x}conversion, 75-80% at 400 degrees C, the front section exhibited a drastic decrease to only 20-35% at 400 degrees C. This two-tiered deactivation was also observed for field-aged samples that were analyzed in this study. To understand the observed performance changes, thorough materials characterization was performed which revealed two primary degradation mechanisms. The first mechanism is a general Fe-zeolite deterioration which led to surface area losses, dealumination of the zeolite, and Fe{sub 2}O{sub 3} crystal growth. This degradation accelerated above 750 degrees C, and the effects were generally more severe in the front of the catalyst. The second deactivation mechanism is linked to trace levels of Pt that are suspected to be volatizing from the DOC and depositing on the front section of the SCR catalyst. Chemical evidence of this can be seen in the high levels of NH{sub 3} oxidation (80% conversion at 400 degrees C), which coincides with the decrease in performance.

33 ADVANCED PROPULSION SYSTEMS↗

Pre-Oxidized and Nitrided Stainless Steel Foil for Proton Exchange Membrane Fuel Cell Bipolar Plates: Part 2- Single-Cell Fuel Cell Evaluation of Stamped Plates

Thermal (gas) nitridation of stainless steel alloys can yield low interfacial contact resistance (ICR), electrically conductive and corrosion-resistant nitride containing surface layers (Cr{sub 2}N, CrN, TiN, V{sub 2}N, VN, etc.) of interest for fuel cells, batteries, and sensors. This paper presents results of proton exchange membrane (PEM) single-cell fuel cell studies of stamped and pre-oxidized/nitrided developmental Fe-20Cr-4V weight percent (wt.%) and commercial type 2205 stainless steel alloy foils. The single-cell fuel cell behavior of the stamped and pre-oxidized/nitrided material was compared to as-stamped (no surface treatment) 904L, 2205, and Fe-20Cr-4V stainless steel alloy foils and machined graphite of similar flow field design. The best fuel cell behavior among the alloys was exhibited by the pre-oxidized/nitrided Fe-20Cr-4V, which exhibited {approx}5-20% better peak power output than untreated Fe-20Cr-4V, 2205, and 904L metal stampings. Durability was assessed for pre-oxidized/nitrided Fe-20Cr-4V, 904L metal, and graphite plates by 1000+ h of cyclic single-cell fuel cell testing. All three materials showed good durability with no significant degradation in cell power output. Post-test analysis indicated no metal ion contamination of the membrane electrode assemblies (MEAs) occurred with the pre-oxidized and nitrided Fe-20Cr-4V or graphite plates, and only a minor amount of contamination with the 904L plates.

30 DIRECT ENERGY CONVERSION↗

A Study on a Prognosis Algorithm for PEMFC Lifetime Prediction based on Durability Tests

Of the fuel cells being studied, the proton exchange membrane fuel cell (PEMFC) is viewed as the most promising for transportation. Yet until today, the commercialization of the PEMFC has not been widespread in spite of its large expectation. Poor long term performances or durability, and high production and maintenance costs account for the main reasons. For the final commercialization of fuel cell in transportation field, the durability issue must be addressed, while the costs should be further brought down. In the meantime, health-monitoring and prognosis techniques are of great significance in ensuring the normal operation of the fuel cell and preventing or predicting its likely abrupt and catastrophic failure.

30 DIRECT ENERGY CONVERSION↗

Nitrided Metallic Bipolar Plates

Effort devoted to scale up and demonstration of thin stamped metallic bipolar plates. Overall goal is to demonstrate potential for metallic bipolar plates to meet 5000 h automotive durability goal at a cost of less than $5/kW.

08 HYDROGEN↗

Effect of Ceria on the Sulfation and Desulfation Characteristics of a Model Lean NOx Trap Catalyst

The effect of ceria addition on the sulfation and desulfation characteristics of a model Ba-based lean NO{sub x} trap (LNT) catalyst was studied. According to DRIFTS and NO{sub x} storage capacity measurements, ceria is able to store sulfur during catalyst exposure to SO{sub 2}, thereby helping to limit sulfation of the main (Ba) NO{sub x} storage phase and maintain NO{sub x} storage capacity. Temperature programmed desulfation experiments revealed that desulfation of a model ceria-containing catalyst occurred in two stages, corresponding to sulfur elimination from the ceria phase at {approx}450 C, followed by sulfur loss from the Ba phase at {approx}650 C. Significantly, the ceria-containing catalyst displayed relatively lower sulfur evolution from the Ba phase than its non-ceria analog, confirming that the presence of ceria lessened the degree of sulfur accumulation on the Ba phase.

54 ENVIRONMENTAL SCIENCES↗

NOx storage and reduction in model lean NOx trap catalysts studied by in situ DRIFTS

NO{sub x} storage and reduction on a model Pt/BaO/Al{sub 2}O{sub 3} catalyst was studied by means of in situ DRIFTS measurements. To examine the effect of ceria addition, experiments were also conducted using Pt/BaO/Al{sub 2}O{sub 3} to which Pt/CeO{sub 2} was added as a physical mixture in a 74:26 weight ratio. For the former catalyst, DRIFT spectra acquired during NO/O{sub 2} and NO{sub 2}/O{sub 2} storage indicated the formation of nitrite at 200 C during the initial stages of adsorption, while increasing the adsorption temperature appeared to facilitate the oxidation of nitrite to nitrate. The ceria-containing catalyst afforded similar DRIFT spectra under these conditions, although the presence of cerium nitrates was observed at 200 and 300 C, consistent with NO{sub x} storage on the ceria phase. DRIFT spectra acquired during NO{sub x} reduction in CO and CO/H{sub 2} showed that Ba nitrate species remained on the surface of both catalysts at 450 C, whereas the use of H{sub 2}-only resulted in complete removal of stored NO{sub x}. The observation of Ba carbonates when CO was present suggests that the inferior reduction efficiency of CO may arise from the formation of a crust of BaCO{sub 3} on the Ba phase, which inhibits further NO{sub x} reduction. DRIFT spectra acquired during lean-rich cycling (6.5 min lean, 1.0 min rich) with CO/H{sub 2} as the rich phase reductants revealed that a significant concentration of nitrates remained on the catalysts at the end of the rich phase. This implies that a large fraction of nitrate is not decomposed during cycling and thus cannot participate in NO{sub x} abatement through storage and regeneration.

33 ADVANCED PROPULSION SYSTEMS↗

Nondestructive X-ray Inspection of Thermal Damage, Soot and Ash Distributions in Diesel Particulate Filters

We describe novel results of ongoing research at 3DX-RAY Ltd and Oak Ridge National Laboratory using new, commercially available, nondestructive x-ray techniques to make engineering measurements of diesel particulate filters (DPF). Nondestructive x-ray imaging and data-analysis techniques were developed to detect and visualize the small density changes corresponding to the addition of substances such as soot and ash to DPF monoliths. The usefulness of this technique was explored through the analysis of field-aged samples, accelerated-aged samples, and the synthetic addition of ash and soot to clean DPF samples. We demonstrate the ability to visualize and measure flaws in substrates and quantify the distribution of ash and soot within the DPF. We also show that the technology is sensitive enough for evaluations of soot and ash distribution and thermal damage without removing the DPF from its metal casing.

33 ADVANCED PROPULSION SYSTEMS↗

The Role of Phosphorus and Soot on the Deactivation of Diesel Oxidation Catalysts

The deactivation of diesel oxidation catalysts (DOCs) by soot contamination and lube-oil derived phosphorus poisoning is investigated. Pt/CeO2/-Al2O3 DOCs aged using three different protocols developed by the authors and six high mileage field-returned DOCs of similar formulation are evaluated for THC and CO oxidation performance using a bench-flow reactor. Collectively, these catalysts exhibit a variety of phosphorus and soot morphologies contributing to performance deactivation. To isolate and examine the contribution of each deactivation mechanism, performance evaluations are carried out for each DOC ''as received'' and after removal of surface carbon in a high-temperature oxidizing environment. In such a manner the deactivation contribution of soot contamination is de-convoluted from that of phosphorus poisoning. It will be shown that this is accomplished while preserving phosphorus (and to a lesser degree sulfur, calcium and zinc) chemistries and concentrations within the washcoat. Washcoat contaminant information and materials changes are characterized using electron-probe microanalysis (EPMA), X-ray diffraction (XRD), scanning electron microscopy and energy dispersive spectroscopy (SEM-EDS), BET surface area, oxygen storage capacity (OSC), X-ray fluorescence (XRF) and inductively coupled plasma (ICP) analysis, from which the relative severity of each mechanism can be quantified. Results show that soot contamination from diesel exhaust severely degrades THC and CO oxidation performance by acting as a catalyst surface diffusion barrier. This results in a considerable increase of light-off temperatures. In contrast, phosphorus poisoning, which is considered a significant deactivation mechanism in three-way catalysts, is shown to have minimal effect on DOC oxidation performance for the conditions studied here. Material changes include the formation of both Ce(III-IV) and aluminum phosphates which do not significantly hinder the THC and CO oxidation in lean exhaust. In addition, thermal aging and sulfur poisoning are shown to produce minimal contributions to the overall deactivation. Consequently, performance of aged DOCs after soot removal is observed to be comparable to that of a fresh catalyst under our testing conditions.

33 ADVANCED PROPULSION SYSTEMS↗

Impact of Biofuel Blending on Diesel Soot Oxidation: Implications for Aftertreatment

Control strategies for diesel particulate filters (DPFs) remain one of the most important aspects of aftertreatment research and understanding the soot oxidation mechanism is key to controlling regeneration. Currently, most DPF models contain simple, first order heterogeneous reactions oxidation models with empirically fit parameters. This work improves the understanding of fundamental oxidation kinetics necessary to advance the capabilities of predictive modeling, by leading to better control over regeneration of the device. This study investigated the effects of blending soybean-derived biodiesel fuel on diesel particulate emissions under conventional combustion from a 1.7L direct injection, common rail diesel engine. Five biofuel blend levels were investigated and compared to conventional certification diesel for the nanostructure, surface chemistry and major constituents of the soluble organic fraction (SOF) of diesel particulate matter (PM), and the relationship between these properties and the particulate oxidation kinetics.

33 ADVANCED PROPULSION SYSTEMS↗

Effects of Rapid High Temperature Cyclic Aging on a Fully-Formulated Lean NOx Trap Catalyst

In this study, high-temperature deactivation of a fully-formulated lean NOx trap (LNT) is investigated with an accelerated aging protocol where accelerated aging is accomplished by rapid temperature cycling and by higher temperatures. Thermal aging is carried out in a bench-flow reactor at nominal temperatures of 700, 800, 900, and 1000 C using an aging cycle consisting of a 130s lean-phase and a 50s rich-phase. After a prescribed number of lean/rich aging cycles, the NOx conversion of the aged LNT is evaluated at 200, 300, and 400 C. The NOx performance is obtained at a GHSV of 30,000 h-1 using an evaluation cycle consisting of a 60s lean-phase and 5s rich-phase. The effects of aging on the LNT washcoat are determined with EPMA, XRD, STEM/EDS, and BET. Aging at 700 and 800 C has a minimal effect on LNT performance and material properties. However, at aging temperatures of 900 and 1000 C reduction in surface area and sintering of PGM particles are observed and result in a drastic reduction in NOx conversion. Additionally, after aging at 900 C and 1000 C the NOx storage medium, BaCO3, is no longer visible in the XRD patterns, even though a Ba-phase identified by EPMA still exists in all aged samples. BaAl2O4 is not identified at any aging temperatures; possibly due to stabilization effects provided by washcoat additives present in this particular LNT.

33 ADVANCED PROPULSION SYSTEMS↗