Search NASA⌕ Search

Engineering topics

Tornheim, Adam

Publications and source records attributed to Tornheim, Adam.

Evaluation of Cathode Materials with Lithium-Metal Anodes: Baseline Performance and Protocol Standardization of Coin Cells

The collaborative evaluation of electrode materials across multiple research entities requires standardized electrochemical testing protocols to produce reliable, one-to-one comparisons between different systems of interest. Similar to the work done by Long et al. on protocol standardization for coin-cell testing with graphite anodes [J. Electrochem. Soc., 163, A2999, (2016)], here we introduce two standardized testing protocols designed to quickly evaluate important electrochemical properties of cathode materials using lithium-metal anodes. The two protocols measure kinetic and thermodynamic capacity losses, rate- and voltage-dependent cycling capacities, instabilities at high voltage and high cycling rate, and overpotentials at various states of charge. We then apply these protocols to four commercially available cathode materials to establish benchmark performance metrics that can be used to screen and evaluate new cathode materials.

25 ENERGY STORAGE↗

The influence of temperature on area-specific impedance and capacity of Li-ion cells with nickel-containing positive electrodes

The temperature-dependent behaviors of five nickel-containing positive electrodes (NCA, NMC811, NMC622, NMC532, and NMC111) in lithium-ion batteries are investigated using an electrochemical protocol involving rate studies, mild aging (~100 cycles), and hybrid pulse power characterization (HPPC). Tests are conducted using coin-cells with graphite negative electrodes at -20 °C, 0 °C, 20 °C, and 40 °C. Three techniques are compared for determining the area-specific impedance (ASI): i) fits to the rate study average voltages, ii) fitting to the entire voltage curves using a regularization scheme, and iii) HPPC. When fit to an Arrhenius-type equation, all methods yield similar apparent activation energies (±2 kJ/mol) for the impedance, which range from -20 to -31 kJ/mol for the electrodes. Impedance growth increases with temperature but remains at less than 0.2% per cycle for most electrodes and temperatures. NCA and NMC811 are the exceptions, which yield 0.5% and 1.5% increases in ASI per cycle, respectively, at 40 °C. For cells with the same electrodes, the capacities are similar at 20 and 40 °C but reduce at lower temperatures, with up to a 52% reduction at -20 °C and 2C. The fade in energy of the cells during C/3 cycling is attributed to decreasing capacity as opposed to increasing ASI.

25 ENERGY STORAGE↗

Concealed Cathode Degradation in Lithium-Ion Cells with a Ni-Rich Oxide

Difficulties with sourcing cobalt and the interest in increasing cell energy have motivated the development of Ni-rich oxide materials for lithium-ion battery cathodes. Despite the intense research on the topic, there is limited information available on the long-term performance of novel cathode formulations. Here, we evaluate the stability of LiNi 0.9 Mn 0.05 Co 0.05 O 2 in full-cells tested for over five months, assessing how cycling, voltage and electrolyte additives impact cathode aging. We use differential voltage analysis to extract insights about the cathode from the full-cell data and identify the isolation of cathode particles in the delithiated (charged) state as a relevant mode of aging. Importantly, this particular mechanism of cathode aging does not cause immediate cell capacity fade, causing the simple analysis of cell capacity retention to overestimate the cathode stability under the investigated conditions. So, our observations serve as cautionary tale indicating that careful analysis of data from extended testing may be required for assessing the performance of Ni-rich cathodes and for evaluating how these materials are affected by electrolyte additives.

25 ENERGY STORAGE↗

What do Coulombic Efficiency and Capacity Retention Truly Measure? A Deep Dive into Cyclable Lithium Inventory, Limitation Type, and Redox Side Reactions

Here, the battery performance metrics of Coulombic efficiency (CE) and capacity retention (CR) are derived in terms of cycling current and side-reaction currents at each electrode. A cyclable lithium inventory (CLI) framework is developed to explain the fundamental differences between inventory-limited and site-limited cells. The otherwise unmeasurable oxidation and reduction side-reaction currents are expressed in terms of cycling current, CE, and CR for both limitation types. Important conclusions regarding cyclable lithium inventory, limitation type, and the interpretation of CE and CR are discussed. From the framework, CE depends on either the oxidation side-reaction current or the reduction side-reaction current, but not both. CE and CR depend on cell limitation type and are increased by faster cycling. Experiments are presented to support the framework and demonstrate that cells can transition between limitation types. These conclusions are presented in terms of lithium-ion batteries, but this framework may be extended to describe other battery systems.

25 ENERGY STORAGE↗