Fracture mode, microstructure and temperature-dependent elastic moduli for thermoelectric composites of PbTe–PbS with SiC nanoparticle additions
Explore the source record for details and available documents.
Engineering topics
Publications and source records attributed to Trejo, Rosa M.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
The feasibility of adding glass or inorganic binder to conventional SOFC cathode contact materials (CCM) in order to improve bonding to adjacent materials in the cell stack is assessed. Two glasses (SEM-COM SCZ-8 and Schott GM31107) and one inorganic binder (Aremco 644A) are mixed with LSM particles to produce composite CCM pastes. These are used to bond Mn1.5Co1.5O4-coated stainless steel mesh current collectors to anode-supported button cells. The cells are operated at 800 C for about 1000 h. The cell with SCZ-8 addition to the CCM displays quite stable operation (3.9%/1000 h degradation), whereas the other additives lead to somewhat higher degradation rate. Bonding of the CCM to coated stainless steel coupons is also assessed. Interfacial fracture toughness is determined using a four-point bend test. The fracture toughness for LSM Schott glass (12.3 N mm 1), LSM SCZ-8 glass (6.8 N mm 1) and LSM 644A binder (5.4 N mm 1) are significantly improved relative to pure LSM (1.7 N mm 1). Indeed, addition of binder or glass is found to improve bonding of the CCM layer without sacrificing cell performance.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Fine holes in metal alloys are employed for many important technological purposes, including cooling and the precise atomization of liquids. For example, they play an important role in the metering and delivery of fuel to the combustion chambers in energy-efficient, low-emissions diesel engines. Electro-discharge machining (EDM) is one process employed to produce such holes. Since the hole shape and bore morphology can affect fluid flow, and holes also represent structural discontinuities in the tips of the spray nozzles, it is important to understand the microstructures adjacent to these holes, the features of the hole walls, and the nanomechanical properties of the material that was in some manner altered by the EDM hole-making process. Several techniques were used to characterize the structure and properties of spray-holes in a commercial injector nozzle. These include scanning electron microscopy, cross-sectioning and metallographic etching, bore surface roughness measurements by optical interferometry, scanning electron microscopy, and transmission electron microscopy of recast EDM layers extracted with the help of a focused ion beam.
Explore the source record for details and available documents.
Explore the source record for details and available documents.
Thermomechanical characterization is important to material evaluation and device design in the development of thermoelectric technology. In this study, we utilize the resonant ultrasound spectroscopy (RUS) technique to examine the elastic behavior of a cast LAST (Pb Sb Ag Te) material with a composition of Ag0.86Pb19Sb1.0Te20 between room temperature and 823 K. The temperature-dependent Young s modulus exhibits a monotonically decreasing trend with increasing temperature. However, an abnormal slope change in the Young s modulus temperature curve around 500 K is observed. In addition, hysteresis between heating and cooling data in the temperature range of 450 550 K is observed, which appears to be dependent on the heating/cooling rate during the RUS experiments such that the hysteresis disappears when the heating/cooling rate was decreased from 5 to 2 K min 1. In this study we propose an order disorder transition model for the anomalous temperature-dependent Young s modulus behavior observed in this study.
Explore the source record for details and available documents.
High energy ion beam surface treatments were applied to a selected group of polymers. Of the six materials in the present study, four were thermoplastics (polycarbonate, polyethylene, polyethylene terephthalate, and polystyrene) and two were thermosets (epoxy and polyimide). The particular epoxy evaluated in this work is one of the resins used in formulating fiber reinforced composites for military helicopter blades. Measures of mechanical properties of the near surface regions were obtained by nanoindentation hardness and pin on disk wear. Attempts were also made to measure erosion resistance by particle impact. All materials were hardness tested. Pristine materials were very soft, having values in the range of approximately 0.1 to 0.5 GPa. Ion beam treatment increased hardness by up to 50 times compared to untreated materials. For reference, all materials were hardened to values higher than those typical of stainless steels. Wear tests were carried out on three of the materials, PET, PI and epoxy. On the ion beam treated epoxy no wear could be detected, whereas the untreated material showed significant wear.
The residual stresses in manganese cobaltite, i.e., Mn1.5Co1.5O4, coatings applied onto alloys 441 and Crofer 22 APU were determined by X-Ray Diffraction. The residual stresses were found to be tensile at 800 C for both systems. The residual stress for spinel-coated AL441 relaxed with time and reached a value of 0.16 0.02 GPa after 300 minutes. The stress relaxation process was slower for spinel-coated Crofer and reached a value of 0.23 0.01 GPa after 500 minutes. Four-point bend SENB testing technique was used to evaluate the toughness of the interfaces between LSM10, i.e., (La0.9Sr0.1)0.98MnO3+δ, and spinel-coated AL441 and Crofer. Sandwich test specimens were prepared by sintering the LSM10 layer at 900 C for four hours in air or under PO2 cyclic conditions. The strain energy release rate was found to be 1.52 0.11 J/m2 for regular sintering and 1.47 0.15 J/m2 for sintering with cyclic PO2 treatment. This difference was found to be statistically insignificant.