Workshop on a future muon program at FNAL

The Snowmass report on rare processes and precision measurements recommended Mu2e-II and a next generation muon facility at Fermilab (Advanced Muon Facility) as priorities for the frontier. The Workshop on a future muon program at FNAL was held in March 2023 to discuss design studies for Mu2e-II, organizing efforts for the next generation muon facility, and identify synergies with other efforts (e.g., muon collider). Topics included high-power targetry, status of R&D for Mu2e-II, development of compressor rings, FFA and concepts for muon experiments (conversion, decays, muonium and other opportunities) at AMF. This document summarizes the workshop discussions with a focus on future R&D tasks needed to realize these concepts.

43 PARTICLE ACCELERATORS↗

Comparative analysis of the effects of tantalum doping and annealing on atomic layer deposited (Ta{sub 2}O{sub 5}){sub x}(Al{sub 2}O{sub 3}){sub 1−x} as potential gate dielectrics for GaN/Al{sub x}Ga{sub 1−x}N/GaN high electron mobility transistors

This paper describes a method to optimally combine wide band gap Al{sub 2}O{sub 3} with high dielectric constant (high-κ) Ta{sub 2}O{sub 5} for gate dielectric applications. (Ta{sub 2}O{sub 5}){sub x}(Al{sub 2}O{sub 3}){sub 1−x} thin films deposited by thermal atomic layer deposition (ALD) on GaN-capped Al{sub x}Ga{sub 1−x}N/GaN high electron mobility transistor (HEMT) structures have been studied as a function of the Ta{sub 2}O{sub 5} molar fraction. X-ray photoelectron spectroscopy shows that the bandgap of the oxide films linearly decreases from 6.5 eV for pure Al{sub 2}O{sub 3} to 4.6 eV for pure Ta{sub 2}O{sub 5}. The dielectric constant calculated from capacitance-voltage measurements also increases linearly from 7.8 for Al{sub 2}O{sub 3} up to 25.6 for Ta{sub 2}O{sub 5}. The effect of post-deposition annealing in N{sub 2} at 600 °C on the interfacial properties of undoped Al{sub 2}O{sub 3} and Ta-doped (Ta{sub 2}O{sub 5}){sub 0.12}(Al{sub 2}O{sub 3}){sub 0.88} films grown on GaN-HEMTs has been investigated. These conditions are analogous to the conditions used for source/drain contact formation in gate-first HEMT technology. A reduction of the Ga-O to Ga-N bond ratios at the oxide/HEMT interfaces is observed after annealing, which is attributed to a reduction of interstitial oxygen-related defects. As a result, the conduction band offsets (CBOs) of the Al{sub 2}O{sub 3}/GaN-HEMT and (Ta{sub 2}O{sub 5}){sub 0.16}(Al{sub 2}O{sub 3}){sub 0.84}/GaN-HEMT samples increased by ∼1.1 eV to 2.8 eV and 2.6 eV, respectively, which is advantageous for n-type HEMTs. The results demonstrate that ALD of Ta-doped Al{sub 2}O{sub 3} can be used to control the properties of the gate dielectric, allowing the κ-value to be increased, while still maintaining a sufficient CBO to the GaN-HEMT structure for low leakage currents.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Electron velocity of 6 × 10{sup 7 }cm/s at 300 K in stress engineered InAlN/GaN nano-channel high-electron-mobility transistors

A stress engineered three dimensional (3D) Triple T-gate (TT-gate) on lattice matched In{sub 0.17}Al{sub 0.83}N/GaN nano-channel (NC) Fin-High-Electron-Mobility Transistor (Fin-HEMT) with significantly enhanced device performance was achieved that is promising for high-speed device applications. The Fin-HEMT with 200-nm effective fin-width (W{sub eff}) exhibited a very high I{sub Dmax} of 3940 mA/mm and a highest g{sub m} of 1417 mS/mm. This dramatic increase of I{sub D} and g{sub m} in the 3D TT-gate In{sub 0.17}Al{sub 0.83}N/GaN NC Fin-HEMT translated to an extracted highest electron velocity (v{sub e}) of 6.0 × 10{sup 7 }cm/s, which is ∼1.89× higher than that of the conventional In{sub 0.17}Al{sub 0.83}N/GaN HEMT (3.17 × 10{sup 7 }cm/s). The v{sub e} in the conventional III-nitride transistors are typically limited by highly efficient optical-phonon emission. However, the unusually high v{sub e} at 300 K in the 3D TT-gate In{sub 0.17}Al{sub 0.83}N/GaN NC Fin-HEMT is attributed to the increase of in-plane tensile stress component by SiN passivation in the formed NC which is also verified by micro-photoluminescence (0.47 ± 0.02 GPa) and micro-Raman spectroscopy (0.39 ± 0.12 GPa) measurements. The ability to reach the v{sub e} = 6 × 10{sup 7 }cm/s at 300 K by a stress engineered 3D TT-gate lattice-matched In{sub 0.17}Al{sub 0.83}N/GaN NC Fin-HEMTs shows they are promising for next-generation ultra-scaled high-speed device applications.

36 MATERIALS SCIENCE↗

Durable ultrathin silicon nitride/carbon bilayer overcoats for magnetic heads: The role of enhanced interfacial bonding

Pole tip recession (PTR) is one of the major issues faced in magnetic tape storage technology, which causes an increase in the magnetic spacing and hence signal loss during data readback. Despite efforts to reduce the magnetic spacing, PTR, and surface wear on the heads by using protective overcoats, most of them either employ complex fabrication processes and approaches do not provide adequate protection to the head or are too thick (∼10–20 nm), especially for future high density tape storage. In this work, we discuss an approach to reduce the PTR and surface wear at the head by developing an ultrathin ∼7 nm bilayer overcoat of silicon/silicon nitride (Si/SiN{sub x}) and carbon (C), which is totally fabricated by a cost-effective and industrial-friendly magnetron sputtering process. When compared with a monolithic C overcoat of similar thickness, the electrically insulating Si/SiN{sub x}/C bilayer overcoat was found to provide better wear protection for commercial tape heads, as demonstrated by Auger electron spectroscopic analyses after wear tests with commercial tape media. Although the microstructures of carbon in the monolithic and bilayer overcoats were similar, the improved wear durability of the bilayer overcoat was attributed to the creation of extensive interfacial bonding of Si and N with the C overcoat and the alumina-titanium carbide composite head substrate, as predicted by time-of-flight secondary ion mass spectrometry and confirmed by in-depth X-ray photoelectron spectroscopy analyses. This study highlights the pivotal role of enhanced interfaces and interfacial bonding in developing ultrathin yet wear-durable overcoats for tape heads.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Effect of Gd dopant concentration on the defect engineering in ceria nanostructures

Graphical abstract: Display Omitted Highlights: ► Investigates the ionic conductivity of defect engineered Gd doped nano scale ceria. ► Reveals that there exists an optimum concentration of dopant to engineer ceria with large O{sub 2} vacancies. ► For the first time the Nanosponge morphology observed in the Gd doped nanoceria. ► It is observed that 5% of Gd in ceria is optimum to induce appropriate amount of defects. ► Thereby an enhanced ionic conductivity is achieved in 5% Gd doped ceria. -- Abstract: In this study, the fabrication and characterization of pure and gadolinium (Gd) doped ceria nanostructures (Ce{sub 1−x}Gd{sub x}O{sub 2−δ} where x = 0.05, 0.1 and 0.2) are investigated. The origin of defect formation has been systematically investigated by XRD and UV-Visible Raman. All the fabricated ceria are found to be “Nanosponge” morphology which is observed by using FESEM technique. The charge transfer of O{sup 2−} ions and Ce{sup 3+}/Ce{sup 4+} in the ceria host due to these defect structures are studied by UV–DRS. Impedance analysis is showed an enhanced ionic conductivity for 5% Gd doped ceria compared to other concentration of Gd, revealing that the dopant concentration is a critical parameter in engineering a large number of vacancy defects in ceria nanostructures.