Search NASA⌕ Search

Engineering topics

Truong, Thien N.

Publications and source records attributed to Truong, Thien N..

Investigation of Gallium–Boron Spin-On Codoping for poly-Si/SiO x Passivating Contacts

A doping technique for p-type poly-Si/SiOx passivating contacts using a spin-on method for different mixtures of Ga and B glass solutions is presented. Effects of solution mixing ratios on the contact performance (implied open circuit voltage iV oc , contact resistivity ..rho..c) are investigated. For all as-annealed samples at different drive-in temperatures, increasing the percentage of Ga in the solution shows a decrement in iV oc (from ~680 to ~610 mV) and increment in ..rho..c (from ~3 to ~800 mO cm 2 ). After a hydrogenation treatment by depositing a SiN x /AlO x stack followed by forming gas annealing, all samples show improved iVoc (~700 mV with Ga-B co-doped, and ~720 mV with all Ga). Interestingly, when co-doping Ga with B, even a small amount of B in the mixing solution shows negative effects on the surface passivation. Active and total dopant profiles obtained by electrical capacitance voltage and secondary-ion mass spectrometry measurements, respectively, reveal a relatively low percentage of electrically-active Ga and B in the poly-Si and Si layers. Overall, these results help understand the different features of the two dopants: a low ρ c with B, a good passivation with Ga, their degree of activation inside the poly-Si and Si layers, and the annealing effects.

14 SOLAR ENERGY↗

Morphology, microstructure, and doping behaviour: A comparison between different deposition methods for poly-Si/SiO x passivating contacts

In this work, we study how crystallographic structures, optoelectronic properties, and nanoscale surface morphologies of ex situ phosphorus-doped polycrystalline silicon (poly-Si)/SiO x passivating contacts, formed by different deposition methods (sputtering, plasma-enhanced chemical vapour deposition [PECVD], and low-pressure chemical vapour deposition [LPCVD]), are investigated and compared. Across all these deposition technologies, we noted the same trend: higher diffusion temperatures yield films that are more crystalline but that have rougher surface morphologies due to bigger surface crystal grains. Also, the recrystallization process of the as-deposited Si films starts from the SiO x interface, rather than from the film surface and bulk. However, there are some distinct differences among these technologies. First, the LPCVD method yields the lowest deposition rate, roughest surfaces, and smallest degree of crystallinity on finished poly-Si films. In contrast, the PECVD method has the highest deposition rate and smoothest surfaces for both as-deposited Si and annealed poly-Si films. Second, as-deposited sputtered and PECVD Si films contain only an amorphous phase, whereas as-deposited LPCVD films already has some crystalline phase. Third, the LPCVD phosphorus in-diffusion into the substrate depends strongly on the initial film thickness, whereas for the other two methods, it is weakly dependent on thickness. Finally, the passivation quality of every poly-Si film type has different responses to the film thickness and diffusion temperature, suggesting that the ex situ doping optimization should be performed independently.

14 SOLAR ENERGY↗

Deposition pressure dependent structural and optoelectronic properties of ex-situ boron-doped poly-Si/SiO x passivating contacts based on sputtered silicon

Among common methods to form polycrystalline silicon (poly-Si) films for passivating-contact solar cells, physical vapor deposition, in particular sputtering, is the safest one as it does not require any toxic gaseous precursors. One of the critical parameters to control the properties of sputtered silicon films is their deposition pressure. In this work, structural and optoelectronic characteristics of ex-situ boron-doped poly-Si/SiO x passivating contacts, formed from sputtered intrinsic amorphous silicon (a-Si) deposited at different pressures on top of SiO x /c-Si substrates and subjected to a high-temperature boron diffusion step, are investigated. The deposition rate and density of the as-deposited a-Si films increase with reducing pressure. Low-temperature photoluminescence spectra captured from the as-deposited samples at different pressures do not show typical emissions from hydrogenated a-Si. Meanwhile, their Fourier-transform infrared absorption spectra all show Si–H stretching modes, indicating that hydrogen had been initially incorporated into the chemical SiO x layers and eventually hydrogenated the a-Si/SiO x interfaces during the sputtering process. After the high-temperature boron-diffusion step, all hydrogen-related peaks disappear. Lower pressure films (1.5 and 2.5 mTorr) show more consistent improved performance after hydrogen treatments, compared to higher pressure films (4 and 5 mTorr). Overall, the resultant passivating contacts at 2.5 mTorr achieve a low single-side recombination current density Jo of ~9 fA/cm 2 , whereas their contact resistivity is still low at 15 mO cm 2 .

14 SOLAR ENERGY↗

Emission Control from Transition Metal Dichalcogenide Monolayers by Aggregation-Induced Molecular Rotors

Organic–inorganic (O–I) heterostructures, consisting of atomically thin inorganic semiconductors and organic molecules, present synergistic and enhanced optoelectronic properties with a high tunability. Here, we develop a class of air-stable vertical O–I heterostructures comprising a monolayer of transition-metal dichalcogenides (TMDs), including WS 2 , WSe 2 , and MoSe 2 , on top of tetraphenylethylene (TPE) core-based aggregation-induced emission (AIE) molecular rotors. The created O–I heterostructures yields a photoluminescence (PL) enhancement of up to ~950%, ~500%, and ~330% in the top monolayer WS 2 , MoSe 2 , and WSe 2 as compared to PL in their pristine monolayers, respectively. The strong PL enhancement is mainly attributed to the efficient photogenerated carrier process in the AIE luminogens (courtesy of their restricted intermolecular motions in the solid state) and the charge-transfer process in the created type I O–I heterostructures. Moreover, we observe an improvement in photovoltaic properties of the TMDs in the heterostructures including the quasi-Fermi level splitting, minority carrier lifetime, and light absorption. Overall, this work presents an inspiring example of combining stable, highly luminescent AIE-based molecules, with rich photochemistry and versatile applications, with atomically thin inorganic semiconductors for multifunctional and efficient optoelectronic devices.

14 SOLAR ENERGY↗

Hydrogen-Assisted Defect Engineering of Doped Poly-Si Films for Passivating Contact Solar Cells

Hydrogen-assisted defect engineering, via a hydrogenated silicon nitride (SiN x :H) capping layer, on doped polycrystalline silicon (poly-Si) passivating-contact structures, is explored using complementary techniques. The hydrogen treatment universally improves the passivation quality of poly-Si/SiO x stacks on all samples investigated. Meanwhile, their contact resistivity remains very low at ~6 m$\Omega$cm 2 . Moreover, the nature of charge carrier recombination within the poly-Si films is also investigated by means of photoluminescence. On planar c-Si substrates, the poly-Si films emit two broad photoluminescence peaks ~850-1050 nm and ~1300-1500 nm. The former is the characteristic peak of the hydrogenated amorphous Si (a-Si:H) phase and only appears after the treatment, demonstrating that i) a significant amount of hydrogen has been driven into the poly-Si film and ii) an amorphous phase is present within it. The second peak originates from sub-bandgap radiative defects inside the poly-Si films and increases after the treatment, suggesting a suppression of their non-radiative recombination channels. For films deposited on textured c-Si substrates, there is a disrupted oxide boundary, preventing a build-up of excess carriers inside the films and leading to quenching of the film luminescence.

36 MATERIALS SCIENCE↗

Hydrogenation Mechanisms of Poly-Si/SiO x Passivating Contacts by Different Capping Layers

Herein, posttreatment techniques of phosphorus-doped poly-Si/SiO x passivating contacts, including forming gas annealing (FGA), atomic layer deposition (ALD) of hydrogenated aluminum oxide (AlO x :H), and plasma-enhanced chemical vapor deposition (PECVD) of hydrogenated silicon nitride (SiN x :H), are investigated and compared in terms of their application to silicon solar cells. A simple FGA posttreatment produces a significant increase in the implied open circuit voltage (iV oc ) and the effective minority-carrier lifetime (teff) of high-resistivity crystalline Si (c-Si) samples, whereas low-resistivity samples show a minimal change. Treatment by means of AlO x :H and/or SiN x :H followed by postdeposition FGA results in a universal increase in t eff and iV oc for all substrate resistivities (as high as 12.5 ms and 728 mV for 100 Ω cm and 5.4 ms and 727 mV for 2 Ω cm n-type c-Si substrates). In addition, both the FGA and AlO x :H + FGA techniques can inject sufficient hydrogen into the samples to passivate defects at the SiO x /c-Si and poly-Si/SiO x interfaces. However, this hydrogen concentration is insufficient to neutralize both the nonradiative defects inside the poly-Si films and dangling bonds associated with the amorphous Si phase present in them. The hydrogen injected by the SiN x :H + FGA technique can passivate both the interfaces and the defects and dangling bonds within the poly-Si film. These results are confirmed by low-temperature photoluminescence spectroscopy, Fourier transform infrared spectroscopy, and dynamic secondary-ion mass spectrometry measurements.

14 SOLAR ENERGY↗

Sub-Bandgap Luminescence from Doped Polycrystalline and Amorphous Silicon Films and Its Application to Understanding Passivating-Contact Solar Cells

We report luminescence phenomena from doped polycrystalline silicon (poly-Si) films and their applications to study carrier transport properties in passivating-contact solar cells. Low-temperature luminescence spectra emitted from doped poly-Si layers are found to be very broad and stretched from the crystalline silicon (c-Si) luminescence peak to significantly lower energies. This suggests that these layers contain radiative defect levels whose energies are continuously distributed from the band edges to deep levels in the poly-Si bandgap. Moreover, photoinduced carriers inside poly-Si layers are found to be completely blocked by an ultrathin SiOx interlayer (~1.3 nm). This demonstrates that there is no free-carrier coupling from poly-Si layers in practical passivating-contact solar cells. Finally, we demonstrate that the same principle can be applied to study carrier transport properties in hydrogenated amorphous silicon films.

14 SOLAR ENERGY↗