Near-surface modification of defective KTaO 3 by ionizing ion irradiation

The synergistic effect of nuclear (S n ) and electronic (S e ) energy loss observed in some ABO 3 perovskites has attracted considerable attention due to the real possibility to modify various near-surface properties, such as the electronic and optical properties, by patterning ion tracks in the defective near-surface regions. In this study, we show that low-energy ion-induced disordering in conjunction with ionizing ion irradiation (18 MeV Si, 21 MeV Ni and 91.6 MeV Xe) is a promising approach for tailoring ion tracks in the near-surface of defective KTaO 3 . Experimental characterization and computer simulations reveal that the size of these latent ion tracks increases with S e and level of pre-existing damage. These results further reveal that the threshold S e value (S e th ) for track creation increases with decreasing pre-damage level. The values of S e th increase from 5.02 keV nm -1 , for a pre-existing fractional disorder of 0.53 in KTaO 3 , to 10.81 keV nm -1 for pristine KTaO 3 . Above these thresholds, amorphous latent tracks are produced due local melting and rapid quenching. Below a disorder fraction of 0.08 and S e ≤ 6.68 keV nm -1 , the synergistic effect is not active, and damage accumulation is suppressed due to a competing ionization-induced damage annealing process. These results indicate that, depending on S e and the amount of pre-existing damage, highly ionizing ions can either enhance or suppress damage accumulation in KTaO 3 , thus providing a pathway to tailoring defects states. Comprehending the conflicting roles of highly ionizing ions in defective ABO 3 oxides is vital for understanding and predictive modeling of ion-solid interactions in complex oxides, as well as for achieving control over ion track size in the near-surface of defective KTaO 3 .

36 MATERIALS SCIENCE↗

Dislocation loop evolution and radiation hardening in nickel-based concentrated solid solution alloys

Effects of chemical composition, ion irradiation dose and temperature on unfaulting of irradiation induced Frank dislocation loops to perfect loops in two nickel based single-phase solid solution alloys, Ni–20Fe and NiFe–20Cr, have been studied. The fraction of Frank loops decreases with irradiation dose from 7.2 to 38.4 dpa at 500°C, but with more Frank loops remaining in the ternary alloy. However, perfect loops and dislocation networks become the dominant features of defects at 580°C in both alloys. The results indicate a thermally assisted loop unfaulting process that may be hindered by more sluggish defect motion in the alloy with more chemical components. Nano-indentation with both continuous stiffness method and single indentation method are used to measure radiation hardening. Loop unfaulting in both alloys irradiated at 580°C reduced radiation hardening while significant hardening is observed after irradiation at 500°C. The quasi-static single indentation method exhibits lower hardness results compared to continuous stiffness method, because dislocations induced from the cyclic loading in the latter method get relaxed and stabilized, resulting in higher resistance to the indenter.

36 MATERIALS SCIENCE↗

Local structure of Ni 80 X 20 (X: Cr, Mn, Pd) solid-solution alloys and its response to ion irradiation

In this work, the local structure of Ni 80 X 20 (X: Cr, Mn, Pd) solid-solution alloys was investigated with x-ray absorption and total scattering x-ray diffraction methods. Atomic pair distribution function (PDF) analysis indicated that the local lattice distortion is strongly relevant to the atomic size mismatch, and the local lattice distortion in Ni80Pd20 alloy is obviously larger than that in other solid-solution alloys. The bond length of different atomic pairs was derived from the fitting of extended x-ray absorption fine structure spectra. Quantitative analysis of the local bonding environment in Ni 80 Cr 20 during Ni ion irradiation suggested that Cr atoms tend to form clusters in Ni 80 Cr 20 with the increase of ion dose.

36 MATERIALS SCIENCE↗

Irradiation effects of medium-entropy alloy NiCoCr with and without pre-indentation

Medium entropy alloy NiCoCr draws great attention due to its excellent strength-ductility trade-off mechanical behavior. Its irradiation behavior at elevated temperatures has been investigated using ion beam irradiation in a temperature range of 420–580°C and transmission electron microscopy. Irradiation induced stacking fault tetrahedra were only observed at 420°C. With increasing irradiation temperature, all stacking fault tetrahedra vanished, while the size of voids and dislocation loops increased significantly. Nanoindentation-induced structural complexities, including dislocations, stacking faults and twins helped to reduce void swelling. However, at the elevated temperatures, NiCoCr is still much more susceptible to void swelling compared to high entropy alloys such as NiCoFeCrMn and NiCoFeCrPd.

36 MATERIALS SCIENCE↗

Multi-axial and multi-energy channeling study of disorder evolution in ion-irradiated nickel

In this study, to better understand defect structure and the evolution of irradiation-induced damage in single crystal Ni, in situ Rutherford backscattering spectroscopy in channeling geometry (RBS/C) is performed along the <100>, <110>, and <211> axes with different probing beam energies. The RBS/C data reveal that damage evolution occurs in three steps. The first step at low doses (up to 0.2 dpa), characterized by a linear increase with dose, is related to the formation of point defects and small clusters. The second step in the intermediate dose range (0.2–1.0 dpa) shows a sublinear increase in disorder to saturation. This sublinear increase is due to the growth of defect clusters resulting from the interaction of irradiation-induced defects with already existing damage from previous ion impacts. The third step at high doses (1.0–32.4 dpa) exhibits a surprising decrease in the disorder level, which may be attributed to defect evolution from black spot defects to large dislocation loops that leads to strain relaxation. In addition, the damage extends much deeper than the predicted depths and is attributed to long-range defect migration effects confirmed by transmission electron microscopy (TEM) observations. Although similar damage evolution trends have been observed along all channeling directions, the disorder accumulation is largest along the <100> and <211> axes than observed along <110> axis. This “preferential” disordering process along <100> and <211> suggests that more defects are shielded by the <110> atomic rows than the two other axes. Finally, the co-existence of both uncorrelated displaced lattice atoms and dislocation loops in Ni irradiated at 1 ion/nm 2 is revealed by the energy-dependent RBS/C studies along all three axes. In contrast, dislocation loops and stacking fault tetrahedral are simultaneously present in the crystal structure of Ni irradiated at 100 ions/nm 2 that is consistent with previous molecular dynamics simulations and TEM observations.

36 MATERIALS SCIENCE↗

Temperature-dependent defect accumulation and evolution in Ni-irradiated NiFe concentrated solid-solution alloy

Temperature significantly affects defect migration and evolution in irradiated materials. However, the effects of temperature on defect evolution in concentrated solid-solution alloys (CSAs), including high entropy alloys, are not well understood, despite their potential as structural materials in advanced nuclear reactors. As an important model system of these CSAs, equiatomic Ni 50 Fe 50 (NiFe) was selected to understand the effects of temperature on defect evolution during irradiation and subsequent thermal annealing. Specifically, defect accumulation and evolution in NiFe alloy under Ni-ion irradiation at 150, 300, and 500 K were studied, and the irradiated specimens were subsequently annealed at higher temperatures. Rutherford backscattering spectrometry along the <100> channeling direction was employed to study damage accumulation and evolution before and after each irradiation and annealing experiment. Here we show that more defects survive and accumulate at 150 K, but more importantly defects can migrate to deeper depths at this low irradiation temperature. Irradiation-induced damage at 150 and 300 K does not recover substantially after post-irradiation annealing at 500 K, but dramatic recovery is observed after post-irradiation annealing at 700 K, indicating an onset temperature of defect recovery between 500 and 700 K. Here, the migration of irradiation-induced defects upon annealing is closely related to the mobility and stress state arising from the surviving defects. With the consideration of five stages of defect recovery in conventional dilute alloys, the underlying mechanisms for temperature-dependent defect accumulation and evolution in NiFe CSA are discussed.

36 MATERIALS SCIENCE↗

Channeling analysis in studying ion irradiation damage in materials containing various types of defects

We present that ion channeling is a powerful quantitative technique for studying ion-irradiation induced defect evolution in single crystalline materials. An iterative procedure to determine dechanneling yields has been developed for decades, serving as a major method for analyzing experimental channeling data. The applicability of such procedure is, however, generally limited to the crystalline damage with only point defects and local amorphous domains. For the other cases, such as irradiated metals, the assumption of direct-backscattering free has usually been made. In the present study, Ni, TiAl, MgO, and SrTiO 3 single crystals are selected as four model materials, representing metals, intermetallic alloys, and ceramic compounds with different defect evolution processes under irradiation, to investigate the fidelity of applying dechanneling analysis on various types of defects. The pure dechanneling assumption is shown oversimplified in Ni irradiated with low fluence self-ions and may result in error on the derived damage profile. Moreover, the iterative procedure of dechanneling analysis is shown valid for more general situations than the randomly distributed atoms, including those not exhibiting a peak in channeling spectra. The disappearance of damage peak in channeling spectra is attributed to the combined effects of small (but non-zero) scattering factor, long-range damage effects, and non-ignorable damage level in pristine crystals. Furthermore, the ratio of direct backscattering to dechanneling areas provides information on defect configurations in the materials containing a well-defined damage peak in channeling spectra. Finally, the contribution from dechanneling sources increases from SrTiO 3 , TiAl, to MgO, according to the derived scattering and dechanneling factors.

36 MATERIALS SCIENCE↗

Interstitial migration behavior and defect evolution in ion irradiated pure nickel and Ni-xFe binary alloys

Transition from long-range one-dimensional to short-range three-dimensional migration modes of interstitial defect clusters greatly reduces the damage accumulation in single-phase concentrated solid solution alloys under ion irradiation. A synergetic investigation with experimental, computational and modeling approaches revealed that both the resistance to void swelling and the delay in dislocation evolution in Ni-Fe alloys increased with iron concentration. This was attributed to the gradually increased sluggishness of defect migration, which enhances interstitial and vacancy recombination. Transition from long-range one-dimensional defect motion in pure nickel to short-range three-dimensional motion in concentrated Ni-Fe alloys is continuum, not abrupt, and within an iron concentration range up to 20%. Lastly, the gradual transition process can be quantitatively characterized by the mean free path of the interstitial defect clusters.

36 MATERIALS SCIENCE↗

Influence of irradiation temperature on void swelling in NiCoFeCrMn and NiCoFeCrPd

Here, using ion irradiation and transmission electron microscopy, temperature dependent void swelling and dislocation loop evolution in equiatomic NiCoFeCrMn and NiCoFeCrPd high entropy alloys were investigated. Voids were observed in all tested conditions. An order higher of swelling was observed in both HEAs as temperature increased from 420 to 580 °C. Alloying with Pd was found to have a stronger suppression effect on void and dislocation loop growth than alloying with Mn. Possible contributions to the swelling resistance were explored, including localized lattice distortion and higher defect migration barrier in NiCoFeCrPd. Additionally, no phase decomposition was observed in either alloy.

36 MATERIALS SCIENCE↗

Enhanced void swelling in NiCoFeCrPd high-entropy alloy by indentation-induced dislocations

The role of dislocations on ion irradiation-induced void formation is studied in a high-entropy alloy (HEA) NiCoFeCrPd. Despite previous observations that show high-entropy alloys are swelling resistant due to a high defect recombination rate, the swelling is enhanced with increasing density of pre-existing dislocations at low strain levels that shortened transient duration before the onset of void swelling. Under certain irradiation conditions, a high density of dislocations may carry the material closer to the sink-dominated regime. Finally, compared to another HEA NiCoFeCrMn, NiCoFeCrPd has a smaller loop size and higher loop density due to the stronger lattice distortion.

36 MATERIALS SCIENCE↗

Effect of alloying elements on defect evolution in Ni-20X binary alloys

The effect of alloying elements on radiation-induced microstructural evolution in Ni and Ni-20X (X = Fe, Cr, Mn and Pd) binary alloys was investigated using ion irradiation and cross-sectional transmission electron microscopy. The three-dimensional migration mode is identified to be the dominating migration mechanism for interstitial clusters in these binary alloys, contrary to the one-dimensional mode that dominates in the well-studied dilute alloys. The results reveal that: (1) the average size of defect clusters decreases as the solute atomic volume size factor increases. Smaller void size in Ni-20Cr is attributed to faster vacancy mobility in the near surface region, and weaker vacancy binding energy beyond the irradiation peak than Ni-20Fe. The smaller voids observed in Ni-20Mn and Ni-20Pd beyond the damage peak are due to the stronger Mn/Pd-vacancy binding effect of largely oversized solute atoms. (2) Oversized solutes can act as strong trapping sites for interstitials. The larger the solute atomic volume factor, the stronger the trapping force. This leads to a more significantly sluggish interstitial migration and smaller dislocation loop size. The average dislocation loop size in Ni-20Fe was four times larger than Ni-20Pd (atomic volume factor being 10.6% and 41.3%) but an order of magnitude lower in density. The smaller dislocation loop size in Ni-20Cr is attributed to stronger interstitial binding of Cr-Ni. In conclusion, overall, the alloying effect on defects is more significant in concentrated binary alloys than in dilute binary alloys, due to the concentration difference of alloying atoms and the interstitial dominant migration mechanisms in the main irradiated region.

36 MATERIALS SCIENCE↗

Revealing ionization-induced dynamic recovery in ion-irradiated SrTiO 3

The lack of fundamental understanding on the coupled effects of energy deposition to electrons and atomic nuclei on defect processes and irradiation response poses a significant roadblock for the design and control of material properties. In this work, SrTiO 3 has been irradiated with various ion species over a wide range of ion fluences at room temperature with a goal to deposit different amounts of energy to target electrons and atomic nuclei by varying the ratio of electronic to nuclear energy loss. Here, the results unambiguously show a dramatic difference in behavior of SrTiO 3 irradiated with light ions (Ne, O) compared to heavy ions (Ar). While the damage accumulation and amorphization under Ar ion irradiation are consistent with previous observations and existing models, the damage accumulation under Ne irradiation reveals a quasi-saturation state at a fractional disorder of 0.54 at the damage peak for an ion fluence corresponding to a dose of 0.5 dpa; this is followed by further increases in disorder with increasing ion fluence. In the case of O ion irradiation, the damage accumulation at the damage peak closely follows that for Ne ion irradiation up to a fluence corresponding to a dose of 0.5 dpa, where a quasi-saturation of fractional disorder level occurs at about 0.48; however, in this case, the disorder at the damage peak decreases slightly with further increases in fluence. This behavior is associated with changes in kinetics due to irradiation-enhanced diffusional processes that are dependent on electronic energy loss and the ratio of electronic to nuclear energy dissipation. Lastly, these findings are critical for advancing the fundamental understanding of ion-solid interactions and for a large number of applications in oxide electronics where SrTiO 3 is a foundational material.

36 MATERIALS SCIENCE↗

Effects of chemical alternation on damage accumulation in concentrated solid-solution alloys

Single-phase concentrated solid-solution alloys (SP-CSAs) have recently gained unprecedented attention due to their promising properties. To understand effects of alloying elements on irradiation-induced defect production, recombination and evolution, an integrated study of ion irradiation, ion beam analysis and atomistic simulations are carried out on a unique set of model crystals with increasing chemical complexity, from pure Ni to Ni 80 Fe 20 , Ni 50 Fe 50 , and Ni 80 Cr 20 binaries, and to a more complex Ni 40 Fe 40 Cr 20 alloy. Both experimental and simulation results suggest that the binary and ternary alloys exhibit higher radiation resistance than elemental Ni. The modeling work predicts that Ni 40 Fe 40 Cr 20 has the best radiation tolerance, with the number of surviving Frenkel pairs being factors of 2.0 and 1.4 lower than pure Ni and the 80:20 binary alloys, respectively. While the reduced defect mobility in SP-CSAs is identified as a general mechanism leading to slower growth of large defect clusters, the effect of specific alloying elements on suppression of damage accumulation is clearly demonstrated. This work suggests that concentrated solid-solution provides an effective way to enhance radiation tolerance by creating elemental alternation at the atomic level. The demonstrated chemical effects on defect dynamics may inspire new design principles of radiation-tolerant structural alloys for advanced energy systems.

36 MATERIALS SCIENCE↗

Irradiation-induced damage evolution in concentrated Ni-based alloys

Understanding the effects of chemical complexity from the number, type and concentration of alloying elements in single-phase concentred solid-solution alloys (SP-CSAs) on defect dynamics and microstructure evolution is pivotal for developing next-generation radiation-tolerant structural alloys. A specially chosen set of SP-CSAs with different chemical complexity (Ni 80 Fe 20 , Ni 80 Cr 20 and Ni 40 Fe 40 Cr 20 ) are investigated using 1.5 MeV Mn ions over a wide fluence range, from 2 × 10 13 to 1 × 10 16 ions cm –2 at room temperature. Based on an integrated study of Rutherford backscattering spectroscopy in channeling geometry and molecular dynamics simulations, the results demonstrate that Ni 40 Fe 40 Cr 20 is more radiation tolerant than Ni 80 Fe 20 , Ni 80 Cr 20 and elemental Ni in the low fluence regime. While chemical complexity of this set of SP-CSAs is clearly demonstrated to affect defect evolution through suppressed defect production and enhanced recombination at early stages, the effect of the mixed ferro- and anti-ferromagnetic interactions is not the only controlling factor responsible for the improved radiation performance. As a result, the observed strong alloying effect on defect evolution is attributed to the altered defect migration mobilities of defect clusters in these alloys, an intrinsic characteristic of the complex energy landscapes in CSAs.

36 MATERIALS SCIENCE↗

Suppression of vacancy cluster growth in concentrated solid solution alloys

Large vacancy clusters, such as stacking-fault tetrahedra, are detrimental vacancy-type defects in ion-irradiated structural alloys. Suppression of vacancy cluster formation and growth is highly desirable to improve the irradiation tolerance of these materials. In this paper, we demonstrate that vacancy cluster growth can be inhibited in concentrated solid solution alloys by modifying cluster migration pathways and diffusion kinetics. The alloying effects of Fe and Cr on the migration of vacancy clusters in Ni concentrated alloys are investigated by molecular dynamics simulations and ion irradiation experiment. While the diffusion coefficients of small vacancy clusters in Ni-based binary and ternary solid solution alloys are higher than in pure Ni, they become lower for large clusters. This observation suggests that large clusters can easily migrate and grow to very large sizes in pure Ni. In contrast, cluster growth is suppressed in solid solution alloys owing to the limited mobility of large vacancy clusters. Finally, the differences in cluster sizes and mobilities in Ni and in solid solution alloys are consistent with the results from ion irradiation experiments.

36 MATERIALS SCIENCE↗

Simulation of Rutherford backscattering spectrometry from arbitrary atom structures

Rutherford backscattering spectrometry in a channeling direction (RBS/C) is a powerful tool for analysis of the fraction of atoms displaced from their lattice positions. However, it is in many cases not straightforward to analyze what is the actual defect structure underlying the RBS/C signal. To reveal insights of RBS/C signals from arbitrarily complex defective atomic structures, we develop in this paper a method for simulating the RBS/C spectrum from a set of arbitrary read-in atom coordinates (obtained, e.g., from molecular dynamics simulations). We apply the developed method to simulate the RBS/C signals from Ni crystal structures containing randomly displaced atoms, Frenkel point defects, and extended defects, respectively. The RBS/C simulations show that, even for the same number of atoms in defects, the RBS/C signal is much stronger for the extended defects. Finally, comparison with experimental results shows that the disorder profile obtained from RBS/C signals in ion-irradiated Ni is due to a small fraction of extended defects rather than a large number of individual random atoms.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗