Search NASA⌕ Search

Engineering topics

Vianco, Paul T.

Publications and source records attributed to Vianco, Paul T..

At least 19 records

Evaluating MetGlasTM Solderability with Tin-Silver-Copper and Tin-Silver-Bismuth Solder Alloys

The solderability of MetGlas TM (subsidiary of Hitachi Metals, America Ltd) 2826 MB, a rapidly solidified metallic foil, was evaluated by the meniscus height/wetting force method for tin-silver-copper (SnAgCu) and tin-silver-bismuth (SnAgBi) solders to understand the effects of the extreme non-equilibrium condition of the MetglasTM surface on solderability performance. Of the variables studied here (solder temperature, heat treatment, and solder composition), solder composition had the largest impact on contact angle. Flux and foil composition remained constant throughout; but, these factors would also be predicted to significantly affect solderability. A greater understanding of the manner whereby non-equilibrium cooling affects solderability of these foils will broaden the application of soldering technology of structures fabricated by rapid cooling process (i.e. additively manufactured coatings and parts). Developing a robust database for Pb-free solderability behavior is also necessary, as industry transitions from tin-lead (SnPb) to lead free (Pb-free) solders.

36 MATERIALS SCIENCE↗

A Review of Interface Microstructures in Electronic Packaging Applications: Soldering Technology

Here, this report examines the role of interfaces in electronic packaging applications with the focus placed on soldering technology. Materials and processes are described with respect to their roles on the performance and reliability of associated interfaces. The discussion will also include interface microstructures created by coatings and finishes that are frequently used in packaging applications. Numerous examples are cited to illustrate the importance of interfaces in physical and mechanical metallurgy as well as the engineering function of interconnections. Regardless of the specific application, interfaces are non-equilibrium structures , which has important ramifications for the long-term reliability of electronic packaging.

42 ENGINEERING↗

Interface Reactions Responsible for Run-out in Active Brazing: Part 2

This Part 2 study examined the microstructural characteristics of braze joints made between two KOVar TM base materials using the filler metals, Ag-xAl, having x = 0, 2, 5, and 10 wt.% Al additions. Brazing processes had temperatures of 965°C (1769°F) and 995°C and brazing times of 5 and 20 min. All brazing was performed under high vacuum.

36 MATERIALS SCIENCE↗

Gold-Tin Solder Wetting Behavior for Package Lid Seals

This study examined the cause of nonwetted regions of the gold (Au) finish on iron-nickel (Fe–Ni) alloy lids that seal ceramic packages using the 80Au-20Sn solder (wt %, abbreviated Au–Sn) and their impact on the final lid-to-ceramic frame solder joint. The Auger electron spectroscopy (AES) surface and depth profile techniques identified surface and through-thickness contaminants in the Au metallization layer. In one case, the AES analysis identified background levels of carbon (C) contamination on the surface; however, the depth profile detected Fe and Ni contaminants that originated from the plating process. The Fe and Ni could impede the completion of wetting and spreading to the edge of the Au metallization. The Au layer of lids not exposed to a Au–Sn solder reflow step had significant surface and through-thickness C contamination. Inorganic contaminants were absent. Subsequent simulated reflow processes removed the C contamination from the Au layer without driving Ni diffusion from the underlying solderable layer. Finally, an Au metallization having negligible C contamination developed elevated C levels after exposure to a simulated reflow process due to C contamination diffusing into it from the underlying Ni layer. However, the second reflow step removed that contamination from the Au layer, thereby allowing the metallization to support the formation of lid-to-ceramic frame Au–Sn joints without risk to their mechanical strength or hermeticity.

36 MATERIALS SCIENCE↗

Grain Boundary Diffusion Characterized by KPFM

Materials aging is a high-consequence failure mode in electronic systems. Such mechanisms can degrade the electrical properties of connectors, relays, wire bonds, and other interconnections. Lost performance will impact, not only that of the device, but also the function and reliability of next-level assemblies and the weapons system as a whole. The detections of changes to materials surfaces at the nanometer-scale resolution, provides a means to identify aging processes at their early stages before they manifest into latent failures that affect system-level performance and reliability. Diffusion will be studied on thin films that undergo accelerated aging using the nanometer scale characterization technique of Frequency Modulated Kelvin Probe Force Microscopy (FM-KPFM). The KPFM provides a relatively easy, non-destructive methodology that does not require high-vacuum facilities to obtain nanometer spatial resolution of surface chemistry changes. The KPFM method can provide the means to measure surface, and near-surface, elemental concentrations that allow the determination of diffusion rate kinetics. These attributes will be illustrated by assessing diffusion in a thin film couple. Validation data will obtained from traditional techniques: (a) Auger electron spectroscopy (AES), x-ray fluorescence (XRF), and xray photoelectron spectroscopy (XPS).

36 MATERIALS SCIENCE↗

Grain Boundary Diffusion Characterized by KPFM

Materials aging is a high-consequence failure mode in electronic systems. Such mechanisms can degrade the electrical properties of connectors, relays, wire bonds, and other interconnections. Lost performance will impact, not only that of the device, but also the function and reliability of next-level assemblies and the weapons system as a whole. The detections of changes to materials surfaces at the nanometer-scale resolution, provides a means to identify aging processes at their early stages before they manifest into latent failures that affect system-level performance and reliability. Diffusion will be studied on thin films that undergo accelerated aging using the nanometer scale characterization technique of Frequency Modulated Kelvin Probe Force Microscopy (FM-KPFM). The KPFM provides a relatively easy, non-destructive methodology that does not require high-vacuum facilities to obtain nanometer spatial resolution of surface chemistry changes. The KPFM method can provide the means to measure surface, and near-surface, elemental concentrations that allow the determination of diffusion rate kinetics. These attributes will be illustrated by assessing diffusion in a thin film couple. Validation data will obtained from traditional techniques: (a) Auger electron spectroscopy (AES), x-ray fluorescence (XRF), and xray photoelectron spectroscopy (XPS).

36 MATERIALS SCIENCE↗