Search NASA⌕ Search

Engineering topics

Walker, Larry R

Publications and source records attributed to Walker, Larry R.

At least 19 records

Vacuum-tight sample transfer stage for a scanning electron microscopic study of stabilized lithium metal particles

To facilitate construction analysis, failure analysis, and research in lithium ion battery technology, a high quality methodology for battery disassembly is needed. This paper presents a methodology for battery disassembly that considers key factors based on the nature and purpose of post-disassembly analysis. The methodology involves upfront consideration of analysis paths that will be conducted on the exposed internal components to preserve the state (operational or failed) of the battery. The disassembly processes and exposures must not alter the battery materials once they are removed from their hermetically sealed containers. Because the process of battery disassembly can involve exposure to potentially hazardous compounds or lead to thermal run-away, a brief review concerning the safety hazards of disassembly is also given.

25 ENERGY STORAGE↗

Comparison of Short-Term Oxidation Behavior of Model and Commercial Chromia-Forming Ferritic Stainless Steels in Air with Water Vapor

A high-purity Fe-20Cr and commercial type 430 ferritic stainless steel were exposed at 700 and 800 C in dry air and air with 10% water vapor (wet air) and characterized by SEM, XRD, STEM, SIMS, and EPMA. The Fe-20Cr alloy formed a fast growing Fe-rich oxide scale at 700 C in wet air after 24 h exposure, but formed a thin chromia scale at 700 C in dry air and at 800 C in both dry air and wet air. In contrast, thin spinel + chromia base scales with a discontinuous silica subscale were formed on 430 stainless steel under all conditions studied. Extensive void formation was observed at the alloy-oxide interface for the Fe-20Cr in both dry and wet conditions, but not for the 430 stainless steel. The Fe-20Cr alloy was found to exhibit a greater relative extent of subsurface Cr depletion than the 430 stainless steel, despite the former's higher Cr content. Depletion of Cr in the Fe-20Cr after 24 h exposure was also greater at 700 C than 800 C. The relative differences in oxidation behavior are discussed in terms of the coarse alloy grain size of the high-purity Fe-20Cr material, and the effects of Mn, Si, and C on the oxide scale formed on the 430 stainless steel.

08 HYDROGEN↗

In-Situ Studies of Intercritically Austempered Ductile Iron Using Neutron Diffraction

Intercritically austempered ductile irons hold promise for applications requiring fatigue durability, excellent castability, low production energy requirements, reduced greenhouse gas emissions and excellent machinability. In the present study, four different ductile iron alloys, containing manganese and nickel as the primary austenite-stabilizing elements, were heat treated to obtain different quantities of austenite in the final microstructure. This paper reports the microstructures and phases present in these alloys. Further, lattice strains and diffraction elastic constants in various crystallographic directions and the transformation characteristics of the austenite as a function of applied stress were determined using in-situ loading with neutron diffraction at the second generation Neutron Residual Stress Facility (NRSF2) at the High Flux Isotope Reactor (HFIR) at Oak Ridge National Laboratory (ORNL).

36 MATERIALS SCIENCE↗

Material Compatibility with Isothermal Pb-Li

Eutectic Pb-Li is a leading candidate for current fusion blanket concepts as a coolant. However, there is very little data about the compatibility of most materials with Pb-Li above 500 C where the dissolution rate of many conventional alloys increases rapidly. Current work is beginning to assess Pb-Li compatibility from 500 to 800 C using isothermal capsule experiments. Aluminide coatings hold some promise in protecting conventional Fe-base alloys at 600-700 C. However, there is a significant initial Al loss that has not been clearly explained. Furthermore, the reaction product with coated materials is LiAlO{sub 2} rather than Al{sub 2}O{sub 3} at 600 and 700 C. Even when pre-oxidized to form {alpha}-Al{sub 2}O{sub 3}, an alumina layer on FeCrAl transformed to LiAlO{sub 2} at 700 and 800 C. At 500 C, the preformed oxide partially transformed from alumina and some Li was detected in the oxide layer.

36 MATERIALS SCIENCE↗

Cladding Alloys for Fluoride Salt Compatibility

This report provides an overview of several candidate technologies for cladding nickel-based corrosion protection layers onto high-temperature structural alloys. The report also provides a brief overview of the welding and weld performance issues associated with joining nickel-clad nickel-based alloys. From the available techniques, two cladding technologies were selected for initial evaluation. The first technique is a line-of-sight method that would be useful for cladding large structures such as vessel interiors or large piping. The line-of-sight method is a laser-based surface cladding technique in which a high-purity nickel powder mixed into a polymer binder is first sprayed onto the surface, baked, and then rapidly melted using a high-power laser. The second technique is a vapor phase technique based on the nickel-carbonyl process that is suitable for cladding inaccessible surfaces such as the interior surfaces of heat exchangers. An initial evaluation for performed on the quality of nickel claddings processed using the two selected cladding techniques.

alloys↗

Increasing the Upper Temperature Oxidation Limit of Alumina Forming Austenitic Stainless Steels in Air with Water Vapor

A family of alumina-forming austenitic (AFA) stainless steels is under development for use in aggressive oxidizing conditions from {approx}600-900 C. These alloys exhibit promising mechanical properties but oxidation resistance in air with water vapor environments is currently limited to {approx}800 C due to a transition from external protective alumina scale formation to internal oxidation of aluminum with increasing temperature. The oxidation behavior of a series of AFA alloys was systematically studied as a function of Cr, Si, Al, C, and B additions in an effort to provide a basis to increase the upper-temperature oxidation limit. Oxidation exposures were conducted in air with 10% water vapor environments from 800-1000 C, with post oxidation characterization of the 900 C exposed samples by electron probe microanalysis (EPMA), scanning and transmission electron microscopy, and photo-stimulated luminescence spectroscopy (PSLS). Increased levels of Al, C, and B additions were found to increase the upper-temperature oxidation limit in air with water vapor to between 950 and 1000 C. These findings are discussed in terms of alloy microstructure and possible gettering of hydrogen from water vapor at second phase carbide and boride precipitates.

08 HYDROGEN↗

The Effect of Thermomechanical Processing on the Tensile, Fatigue, and Creep Behavior of Magnesium Alloy AM60

Tensile, fatigue, fracture toughness, and creep experiments were performed on a commercially available magnesium-aluminum alloy (AM60) after three processing treatments: (1) as-THIXOMOLDED (as-molded), (2) THIXOMOLDED then thermomechanically processed (TTMP), and (3) THIXOMOLDED then TTMP then annealed (annealed). The TTMP procedure resulted in a significantly reduced grain size and a tensile yield strength greater than twice that of the as-molded material without a debit in elongation to failure ({epsilon}{sub f}). The as-molded material exhibited the lowest strength, while the annealed material exhibited an intermediate strength but the highest {epsilon}{sub f} (>1 pct). The TTMP and annealed materials exhibited fracture toughness values almost twice that of the as-molded material. The as-molded material exhibited the lowest fatigue threshold values and the lowest fatigue resistance. The annealed material exhibited the greatest fatigue resistance, and this was suggested to be related to its balance of tensile strength and ductility. The fatigue lives of each material were similar at both room temperature (RT) and 423 K (150 C). The tensile-creep behavior was evaluated for applied stresses ranging between 20 and 75 MPa and temperatures between 373 and 473 K (100 and 200 C). During both the fatigue and creep experiments, cracking preferentially occurred at grain boundaries. Overall, the results indicate that thermomechanical processing of AM60 dramatically improves the tensile, fracture toughness, and fatigue behavior, making this alloy attractive for structural applications. The reduced creep resistance after thermomechanical processing offers an opportunity for further research and development.

36 MATERIALS SCIENCE↗

An in situ SEM experimental study of the thermal stability of a LAST thermoelectric material

Thermal stability is a key factor affecting the deployment of thermoelectric (TE) materials in the application of power generation. LAST (Lead-Antimony-Silver-Tellurium) is an emerging material with promising TE properties. The current study focused on the thermal stability of a LAST composition Ag0.86Pb19SbTe20 fabricated from a cast ingot. Using a customized heating stage, the morphology of LAST particles was studied via scanning electron microscopy (SEM) in situ, between room temperature and 575oC. The LAST material included in this study was stable below 550oC. The inclusion phase, which was antimony-rich, has a lower thermal stability than the PbTe-rich matrix. The SEM finding was also consistent with a thermogravimetrtic analysis.

36 MATERIALS SCIENCE↗

Early Experiments with a New In Situ SEM Heating Technology

A new heating technology (Protochips, Inc.) has recently been introduced for in situ electron microscopy studies, including both TEM and SEM applications. Aduro{trademark} heater devices, fabricated using MEMS-based processing, offer numerous advantages for in situ SEM applications over those using a miniaturized furnace. The device supports a sample on a thin ceramic membrane that is directly heated by passing a current of a few mA, thereby also heating the sample. The entire heated area of the device is only 500um x 500um, so it is operated without circulating cooling water. The extremely small heated zone enables a rapid temperature response (10{sup 6} C/s) for both heating and cooling, and it emits a far lower signal of photons and thermal electrons than a typical furnace-type heating device. This allows heating to temperatures in excess of 1000 C without totally degrading the secondary electron signal. The purpose of the present work is to characterize the factors that influence the image quality and resolution of the SEM during heating. We are interested in understanding relative changes of signal-to-noise levels and contrast in secondary electron (SE) and backscattered electron (BSE) images as a function of increasing the heating temperature. We have also assessed the capability for performing energy dispersive X-ray spectroscopy (EDS) during heating experiments. The in situ holder and the structure of a standard heater chip used in this study are shown in Fig. 1. The chip has an array of 5 {micro}m holes in the electrically conductive heater membrane, separated by electrode 'fingers' in this case. A C-flat{trademark} holey carbon film is overlaid on top of the heater membrane. The heating experiments were conducted in a Hitachi S3400 VP-SEM, operated at 15kV and equipped with an EDAX Si(Li) detector. Fig. 2 shows an Ir-doped FeSi particle situated near the edge of the hole in the membrane, imaged with secondary electrons through an Everhart-Thornley (ET) detector in the specimen chamber, at (2a) RT and at (2b) 1200 C, respectively. The image contrast of the low-Z region of the particle was characterized by an intensity profile across the edge of the holey carbon film against the hole (vacuum). Indicated by Line No.1, the contrast difference was 48% at RT, which dropped to 22% at 1200 C. However, the contrast difference of the medium-Z particle against the low-Z support was well above 30% at 1200 C (Line No.2). Heating had a more adverse effect on the contrast of BSE micrographs, likely caused by the direct detection of photons by solid-state BSE detector. The upper limit for acquiring a BSE micrograph of the low-Z material was about 850 C as the contrast was completely washed out by 900 C. EDS analyses carried out during heating showed effects primarily for the collection of low-energy X-rays (<1.2 keV) below a temperature of 600 C: the background counts increased with temperature, thus reduced the signal-to-noise ratio. The upper limit for EDS analysis during heating was about 700 C. The decrease in the signal-to-noise ratio for electron detection and EDS spectrum acquisition is mainly due to the emission of thermal electrons and photons at elevated temperatures. The emitted photons are not position sensitive, thus they uniformly raise the background level of a grayscale BSE image (photons do not affect the signal of the ET detector). However, thermal electrons in the range of {approx}0.1eV are collected by the ET detector, and thereby reduce contrast in the image. It is impressive that even at the highest temperature achievable by the Aduro device (1200 C), acceptable contrast in SE images is achieved. This is because of the extremely small emitting area of the heater membrane. One solution for improving the contrast of an SE micrograph is to suppress the thermal electrons by a small local positive bias. There are two approaches: (1) manipulating the positive bias of the ET detector or (2) using an energy filter to reduce or remove the thermal electrons. A combined Monte Carlo simulation and experimental study is underway to determine the optimal parameters for minimal detection of thermal electrons. We expect the findings from this study will allow for the optimization of the image contrast.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Wear Analysis of Wind Turbine Gearbox Bearings

The objective of this effort was to investigate and characterize the nature of surface damage and wear to wind turbine gearbox bearings returned from service in the field. Bearings were supplied for examination by S. Butterfield and J. Johnson of the National Wind Technology Center (NREL), Boulder, Colorado. Studies consisted of visual examination, optical and electron microscopy, dimensional measurements of wear-induced macro-scale and micro-scale features, measurements of macro- and micro-scale hardness, 3D imaging of surface damage, studies of elemental distributions on fracture surfaces, and examinations of polished cross-sections of surfaces under various etched and non-etched conditions.

14 SOLAR ENERGY↗

Sulfidation-Oxidation Behavior of FeCrAl and TiCrAl and the Third-Element Effect

Short-term sulfidation-oxidation exposures were conducted under high pS2 and low pO2 conditions for TiCrAl and FeCrAl alloys at 600 and 800 C. Low mass gains and submicron Al-rich oxide scales were formed on the TiCrAl, while high mass gains and FeS-based scale formation were observed for FeCrAl. Based on the good behavior of the TiCrAl, third-element effect additions of Cr are not inherently detrimental under sulfidation-oxidation conditions. Rather, differences in the mechanistic action of the third-element addition of Cr between FeCrAl and TiCrAl alloys and its relevance to low oxygen potential sulfidation-oxidation environments were the key factors in determining whether or not a protective alumina scale was established. For FeCrAl, no internal oxidation of Al was observed, which suggested that effects related to secondary gettering were not sufficient to yield protective Al2O3 formation in these environments. Rather, it was proposed that additional third-element effect benefits of Cr based on the existence of solid solutions among Al, Cr, and Fe oxides to mitigate rapid transient Fe-oxide formation were rendered ineffective because FeS formation was thermodynamically favored over Fe-oxide in the environment. In the case of TiCrAl, the stability of Ti-oxide in the sulfidation-oxidation environment and the non-classical third-element effects of Cr on promoting protective Al2O3 scale led to good corrosion resistance.

36 MATERIALS SCIENCE↗

Nature and spatial distribution of sulfur species in a sulfated barium-based commercial lean NOx trap catalyst

We report observations of the nature and spatial distribution of sulfur species on a sulfated Ba-based commercial lean NO{sub x} trap (LNT) catalyst. The monolithic catalyst was sulfated in a bench flow reactor during 60/4-s NO{sub x} storage/reduction cycling to achieve a total sulfur loading of 3.4 g L{sup -1} of catalyst. Washcoat composition, structure and sulfur distribution were analyzed with electron probe microanalysis, X-ray diffraction, Raman spectroscopy, X-ray photoelectron spectroscopy, and temperature-programmed reduction. The most significant washcoat elements of catalytic relevance were Pt, Pd, Rh, Ba, Ce, Zr, Mg, Al, and these were present mainly in four distinct domains; Mg/Al mixed oxide with Pt, Ce; Al oxide with Rh, Pd; Ce/Zr mixed oxide with Pt, Pd, Ba (high Ba content); Ce/Zr mixed oxide with Pt, Pd, Ba (lower Ba content). Sulfur was present in the form of sulfates that decreased in concentration along the LNT axis from front to back. Barium showed the highest sulfur affinity leading to a plug-like axial progression of its sulfation. The sulfation of AI, Mg/Al, and Ce/Zr oxides was less vigorous with a more axially dispersed and less penetrating front.

02 PETROLEUM↗

Comparison of Three Primary Surface Recuperator Alloys

Extensive work performed by Capstone Turbine Corporation, Oak Ridge National Laboratory, and various others has shown that the traditional primary surface recuperator alloy, type 347 stainless steel, is unsuitable for applications above 650 C ({approx}1200 F). Numerous studies have shown that the presence of water vapor greatly accelerates the oxidation rate of type 347 stainless steel at temperatures above 650 C ({approx}1200 F). Water vapor is present as a product of combustion in the microturbine exhaust, making it necessary to find replacement alloys for type 347 stainless steel that will meet the long life requirements of microturbine primary surface recuperators. It has been well established over the past few years that alloys with higher chromium and nickel contents than type 347 stainless steel have much greater oxidation resistance in the microturbine environment. One such alloy that has replaced type 347 stainless steel in primary surface recuperators is Haynes Alloy HR-120 (Haynes and HR-120 are trademarks of Haynes International, Inc.), a solid-solution-strengthened alloy with nominally 33 wt % Fe, 37 wt % Ni and 25 wt % Cr. Unfortunately, while HR-120 is significantly more oxidation resistant in the microturbine environment, it is also a much more expensive alloy. In the interest of cost reduction, other candidate primary surface recuperator alloys are being investigated as possible alternatives to type 347 stainless steel. An initial rainbow recuperator test has been performed at Capstone to compare the oxidation resistance of type 347 stainless steel, HR-120, and the Allegheny Ludlum austenitic alloy AL 20-25+Nb (AL 20-25+Nb is a trademark of ATI Properties, Inc. and is licensed to Allegheny Ludlum Corporation). Evaluation of surface oxide scale formation and associated alloy depletion and other compositional changes has been carried out at Oak Ridge National Laboratory. The results of this initial rainbow test will be presented and discussed in this paper.

36 MATERIALS SCIENCE↗

Composition, Microstructure, and Water Vapor Effects on Internal/External Oxidation of Alumina-Forming Austenitic (AFA) Stainless Steels

A family of creep-resistant austenitic stainless steels based on alumina (Al2O3) scale formation for superior high-temperature oxidation resistance was recently identified. Results of long-term cyclic oxidation studies (100 h cycles and total exposure duration for up to 7500 h) from 650-800 aC in air and/or air with 10% water vapor for a series of 2.5, 3, and 4 wt.% Al AFA compositions, with varying levels of Nb and Ni additions, are presented. Water vapor was observed to enhance subscale Al consumption in the AFA alloys relative to dry air exposure, presumably via enhanced alumina scale cracking and reformation. Water vapor also increased the tendency for internal oxidation. Increased levels of Nb additions were found to significantly improve oxidation resistance, as were reactive element additions of Hf and Y. Computational thermodynamic calculations of the austenitic matrix phase composition and the volume fraction of MC, B2-NiAl, and Fe2Nb base Laves phase precipitates were used to guide interpretation of oxidation behavior alloy composition trends in terms of two-phase oxidation theory, reservoir effect, and the third-element effect of Cr. The implications of these findings for the upper-temperature service limit for this new class of alloys and the potential for AFA alloy modification for increased service temperatures are discussed.

36 MATERIALS SCIENCE↗

Probing microscopic variations of superconductivity on the surface of Ba(Fe1-xCox)2As2 single crystals

The spatially resolved electrical transport properties have been studied on the surface of optimally-doped superconducting Ba(Fe1-xCox)2As2 single crystal by using a four-probe scanning tunneling microscopy. While some non-uniform contrast appears near the edge of the cleaved crystal, the scanning electron microscopy (SEM) reveals mostly uniform contrast. For the regions that showed uniform SEM contrast, a sharp superconducting transition at TC = 22.1 K has been observed with a transition width TC = 0.2 K. In the non-uniform contrast region, TC is found to vary between 19.6 and 22.2 K with TC from 0.3 to 3.2 K. The wavelength dispersive x-ray spectroscopy reveals that Co concentration remains 7.72% in the uniform region, but changes between 7.38% and 7.62% in the non-uniform region. Thus the variations of superconductivity are associated with local compositional change.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗