Search NASA⌕ Search

Engineering topics

Wang, Hsin

Publications and source records attributed to Wang, Hsin.

At least 163 records · Page 9

Thermoelectric Properties of Au- Containing Type-I Clathrates Ba8AuxGa16-3xGe30+2x

Type I clathrates, with compositions based on Ba8Ga16Ge30, are a class of promising thermoelectric materials due to their intrinsically low thermal conductivity. It has been demonstrated previously that the thermoelectric performance can be improved by transition metal substitution of the framework atoms. In this study, the effects of Au substitution for Ga/Ge on thermal and electrical transport properties of type I clathrate compounds have been investigated. Polycrystalline samples with a large range of Au content have been synthesized using conventional solid state techniques with the actual compositions of resulting materials approximately following Zintl-Klemm rules. The charge carrier type changes from electrons (n) to holes (p) as the Au content increases. The Seebeck coefficient (S) and power factor (S2/ where is the electrical resistivity) were improved by Au substitution and the resulting overall thermoelectric properties were enhanced by Au substitution with a thermoelectric figure of merit ZT ~ 0.63 at temperature T = 740 K for the composition Ba8Au5.47Ge39.96. The results presented herein show that Au-containing type I clathrates are promising p-type thermoelectric materials for high temperature applications.

Clathrates↗

Thermal Runaway Risk Evaluation of Li-Ion Cells Using a Pinch-Torsion Test

Internal short circuit (ISCr) can lead to failure of Li-ion cells and sometimes result in thermal runaway. Understanding the behavior of Li-ion cells in ISCr condition is thus critical to evaluate the safety of these energy storage devices. In the current work, a pinch-torsion test is developed to simulate ISCr in a controlled manner. It is demonstrated that the torsional component superimposed on compression loading can reduce the axial load required to induce ISCr with smaller short spot size. Using this pinch-torsion test, two commercial Li-ion pouch cells were tested under different state of charge (SOC). Based on the severity of the cell damage, a series of thermal runaway risk scores were used to rate the thermal stability of these cells. One of the cell types showed significantly increased hazard as the SOC increased while the other type exhibited relative uniform behavior among different SOC. Therefore this novel pinch-torsion test seems to be an attractive candidate for safety testing of Li-ion cells due to its abilities to consistently create small ISCr spots and to differentiate cell stability in a wide range of SOC.

internal short circuit↗

Li-Ion polymer cells thermal property changes as a function of cycle-life

The impact of elevated temperature chargeedischarge cycling on thermal conductivity (K-value) of Lithium Ion Polymer (LIP) cells of various chemistries from three different manufacturers was investigated. These included high voltage (Graphite/LiCoO2:3.0e4.35 V), wide voltage (Si:C/LiCoO2:2.7e4.35 V) and conventional (Graphite/LiCoO2:3.0e4.2 V) chemistries. Investigation results show limited variability within the in-plane and through-plane K-values for the fresh cells with graphite-based anodes from all three suppliers. After 500 cycles at 45 C, in-plane and through-plane K-values of the high voltage cells reduced less vs. those for the wide voltage cells. Such results suggest that high temperature cycling could have a greater impact on thermal properties of Si:C cells than on the LIP cells with graphite (Gr) anode cells we tested. This difference is due to the excess swelling of Si:C-anode based cells vs. Gr-anode cells during cycling, especially at elevated temperatures. Thermal modeling is used to evaluate the impact of K-value changes, due to cycles at 45 C, on the cells internal heat propagation under internal short circuit condition that leads to localized meltdown of the separator.

High voltage Li-Ion polymer cells↗

Failure analysis of pinch-torsion tests as a thermal runaway risk evaluation method of Li-Ion Cells

Recently a pinch-torsion test is developed for safety testing of Li-ion batteries (Ren et al., J. Power Source, 2013). It has been demonstrated that this test can generate small internal short-circuit spots in the separator in a controllable and repeatable manner. In the current research, the failure mechanism is examined by numerical simulations and comparisons to experimental observations. Finite element models are developed to evaluate the deformation of the separators under both pure pinch and pinch-torsion loading conditions. It is discovered that the addition of the torsion component significantly increased the maximum principal strain, which is believed to induce the internal short circuit. In addition, the applied load in the pinch-torsion test is significantly less than in the pure pinch test, thus dramatically improving the applicability of this method to ultra-thick batteries which otherwise require heavy load in excess of machine capability. It is further found that the separator failure is achieved in the early stage of torsion (within a few degree of rotation). Effect of coefficient of friction on the maximum principal strain is also examined.

finite element analysis↗

Final Report - Recovery Act - Development and Application of Processing and Process Control for Nano-Composite Materials for Lithium Ion Batteries

Oak Ridge National Laboratory and A123 Systems, Inc. collaborated on this project to develop a better understanding, quality control procedures, and safety testing for A123 System s nanocomposite separator (NCS) technology which is a cell based patented technology and separator. NCS demonstrated excellent performance. x3450 prismatic cells were shown to survive >8000 cycles (1C/2C rate) at room temperature with greater than 80% capacity retention with only NCS present as an alternative to conventional polyolefin. However, for a successful commercialization, the coating conditions required to provide consistent and reliable product had not been optimized and QC techniques for being able to remove defective material before incorporation into a cell had not been developed. The work outlined in this report addresses these latter two points.

Nuclear Criticality Safety Program (NCSP)↗

The effect of structural vacancies on the thermoelectric properties of (Cu₂Te){sub 1–x}(Ga₂Te₃) x

We have studied the effects of structural vacancies on the thermoelectric properties of the ternary compounds (Cu₂Te) 1–x (Ga₂Te₃) x (x=0.5, 0.55, 0.571, 0.6, 0.625, 0.667 and 0.75), which are solid solutions found in the pseudo-binary phase diagram for Cu₂Te and Ga₂Te₃, and possesses tunable structural vacancy concentrations. This materials system is not suitable due to the cost and scarcity of the constituent elements, but the vacancy behavior is well understood and will provide a valuable test case for other systems more suitable from the standpoint of cost and abundance of raw materials, which also possesses these vacancy features, but whose structural characterization is lacking at this stage. We find that the nominally defect free phase CuGaTe₂ possess the highest ZT (ZT=S²T/ρκ, where S is the Seebeck coefficient and ρ is the electrical resistivity κ is the thermal conductivity and T is the absolute temperature) which approaches 1 at 840 K and seems to continuously increase above this temperature. This result is due to the unexpectedly low thermal conductivity found for this material at high temperature. The low thermal conductivity was caused by strong Umklapp (thermally resistive scattering processes involving three phonons) phonon scattering. We find that due to the coincidentally strong scattering of carriers by the structural defects that higher concentrations of these features lead to poor electrical transport properties and decreased ZT. - Graphical abstract: Thermal conductivity and zT as a function of temperature for a series of compounds of the type (Cu₂Te) 1–x (Ga₂Te₃)x (x=0.5, 0.55, 0.571, 0.6, 0.625, 0.667 and 0.75). Highlights: • All the samples show p-type semiconducting behavior in the temperature dependence of the Seebeck and Hall coefficients. • The increased carrier concentration and the introduction of vacancies diminish the carrier mobility and power factor. • The low temperature k decreases significantly as the Ga₂Te₃ content increases due to increasing point defects. • The highest ZT ~ 1.0 at 840 K among the samples in this study was found in CuGaTe₂, which contains no vacancies.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Thermal to Electrical Energy Conversion of Skutterudite-Based Thermoelectric Modules

The performance of thermoelectric (TE) materials has improved tremendously over the past decade. The intrinsic thermal and electrical properties of state-of-the-art TE materials demonstrate that the potential for widespread practical TE applications is very large and includes TE generators (TEGs) for automotive waste heat recovery. TE materials for automotive TEG applications must have good intrinsic performance, be thermomechanically compatible, and be chemically stable in the 400 K to 850 K temperature range. Both n-type and p-type varieties must be available at low cost, easily fabricated, and durable. They must also form robust junctions and develop good interfaces with other materials to permit efficient flows of electrical and thermal energy. Among the TE materials of interest for automotive waste heat recovery systems are the skutterudite compounds, which are the antimony-based transition-metal compounds RTE4Sb12, where R can be an alkali metal (e.g., Na, K), alkaline earth (e.g., Ba), or rare earth (e.g., La, Ce, Yb), and TE can be a transition metal (e.g., Co, Fe). We synthesized a considerable quantity of n-type and p-type skutterudites, fabricated TE modules, incorporated these modules into a prototype TEG, and tested the TEG on a production General Motors (GM) vehicle. We discuss our progress on skutterudite TE module fabrication and present module performance data for electrical power output under simulated operating conditions for automotive waste heat recovery systems. We also present preliminary durability results on our skutterudite modules.

module↗

Transport Properties of Bulk Thermoelectrics An International Round-Robin Study, Part I: Seebeck Coefficient and Electrical Resistivity

Recent research and development of high temperature thermoelectric materials has demonstrated great potential of converting automobile exhaust heat directly into electricity. Thermoelectrics based on classic bismuth telluride have also started to impact the automotive industry by enhancing air conditioning efficiency and integrated cabin climate control. In addition to engineering challenges of making reliable and efficient devices to withstand thermal and mechanical cycling, the remaining issues in thermoelectric power generation and refrigeration are mostly materials related. The figure-of-merit, ZT, still needs to improve from the current value of 1.0 - 1.5 to above 2 to be competitive to other alternative technologies. In the meantime, the thermoelectric community could greatly benefit from the development of international test standards, improved test methods and better characterization tools. Internationally, thermoelectrics have been recognized by many countries as an important area for improving energy efficiency. The International Energy Agency (IEA) group under the implementing agreement for Advanced Materials for Transportation (AMT) identified thermoelectric materials as an important area in 2009. This paper is Part I of the international round-robin testing of transport properties of bulk thermoelectrics. The main focuses in Part I are on two electronic transport properties: Seebeck coefficient and electrical resistivity.

thermoelectrics↗

An International Round-Robin Study, Part II: Thermal Diffusivity, Specific Heat and Thermal Conductivity

For bulk thermoelectrics, figure-of-merit, ZT, still needs to improve from the current value of 1.0 - 1.5 to above 2 to be competitive to other alternative technologies. In recent years, the most significant improvements in ZT were mainly due to successful reduction of thermal conductivity. However, thermal conductivity cannot be measured directly at high temperatures. The combined measurements of thermal diffusivity and specific heat and density are required. It has been shown that thermal conductivity is the property with the greatest uncertainty and has a direct influence on the accuracy of the figure of merit. The International Energy Agency (IEA) group under the implementing agreement for Advanced Materials for Transportation (AMT) has conducted two international round-robins since 2009. This paper is Part II of the international round-robin testing of transport properties of bulk bismuth telluride. The main focuses in Part II are on thermal diffusivity, specific heat and thermal conductivity.

specific heat↗

Thermal Conductivity of Wood-Derived Graphite and Copper-Graphite

The thermal conductivity of wood-derived graphite and graphite/copper composites was studied both experimentally and using finite element analysis. The unique, naturally-derived, anisotropic porosity inherent to wood-derived carbon makes standard porosity-based approximations for thermal conductivity poor estimators. For this reason, a finite element technique which uses sample microstructure as model input was utilized to determine the conductivity of the carbon phase independent of porosity. Similar modeling techniques were also applied to carbon/copper composite microstructures and predicted conductivities were compared to those determined via experiment.

B. Porosity↗

Synthesis, Crystal Structure, and High Temperature Transport Properties of p-type Cu2Zn1-xFexSnSe4

Iron substituted Cu2Zn1-xFexSnSe4 stannites were synthesized by reaction of the constituent elements and subsequent solid state annealing, followed by densification by hot-pressing. The compositions for each specimen were confirmed with a combination of Rietveld refinement and elemental analysis. Refinement results indicated that only the 2a site was occupied by Zn and Fe. Their high temperature transport properties were measured from 300 to 800 K. The electrical resistivity and thermal conductivity decrease with increasing Fe content. For the lower Fe content specimens with x = 0.2 and 0.4, the electrical properties are strongly temperature dependent, unlike that of the higher Fe content specimens (x = 0.6 and 0.8). A maximum ZT value of 0.46 was obtained at 800 K for Cu2Zn0.4Fe0.6SnSe4.

p-type↗