Search NASA⌕ Search

Engineering topics

Weatherup, Robert S.

Publications and source records attributed to Weatherup, Robert S..

Chemical state of nickel nanoparticles during the oxygen evolution reaction in a carbonate-bicarbonate buffer solution

The chemical state of nickel anodes during the oxygen evolution reaction can impact their electrocatalytic performance. Here, X-ray photoelectron and absorption spectroscopies reveal the chemical state of nickel nanoparticles under oxygen evolution reaction conditions in amildly alkaline carbonate-bicarbonate buffer solution. Ni 2+ and Ni 3+ species are observed at the reaction onset potential with a 7:4 ratio, with no remaining metallic nickel. These species include NiO, which increasingly converts to other Ni 2+ and Ni 3+ species once the potential is increased above the onset potential. Conversely, when a 20-nm-thick nickel film is used instead of nickel nanoparticles, a significant amount of metallic nickel remains in the inner layers. Nickel nanoparticles also undergo significant morphological and structural changes during the reaction, as evidenced by ex situ transmission electron microscopy. Amorphization of the nanoparticles is attributed to significant H 2 O incorporation, with the oxygen intensity increasing both in operando and ex situ measurements.

36 MATERIALS SCIENCE↗

Electronic interactions and stability issues at the copper-graphene interface in air and in alkaline solution under electrochemical control

A micro-electrochemical cell is sealed with a polymer-free single-layer graphene (SLG) membrane to monitor the stability of Cu nanoparticles (NPs) attached to SLG, as well as the interfacial electronic interactions between Cu NPs and SLG both in air and in a mildly alkaline aqueous solution under electrochemical control. A combination of techniques, including in-situ Kelvin probe force microscopy (KPFM) and ex-situ electron microscopy, are applied. When Cu NPs are metallic at cathodic potentials, there is a relatively bias-independent offset in the SLG work function due to charge transfer at the Cu-SLG contact. When Cu NPs are oxidized at anodic potentials, on the other hand, the work function of SLG also depends on the applied bias in a quasi-linear fashion due to electrochemical gating, in addition to charge transfer at the CuOx-SLG contact. Furthermore, Cu NPs were found to oxidize and detach from SLG when kept under anodic potentials for a few hours, whereas they remain adhered to SLG at cathodic potentials. This is attributed to water intercalation at the CuO-SLG interface associated with the enhanced hydrophilicity of positively polarized graphene, as supported by the absence of Cu detachment following oxidation by galvanic corrosion in air.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electrolyte Reactivity at the Charged Ni-Rich Cathode Interface and Degradation in Li-Ion Batteries

The chemical and electrochemical reactions at the positive electrode–electrolyte interface in Li-ion batteries are hugely influential on cycle life and safety. Ni-rich layered transition metal oxides exhibit higher interfacial reactivity than their lower Ni-content analogues, reacting via mechanisms that are poorly understood. Here, we study the pivotal role of the electrolyte solvent, specifically cyclic ethylene carbonate (EC) and linear ethyl methyl carbonate (EMC), in determining the interfacial reactivity at charged LiNi 0.33 Mn 0.33 Co 0.33 O 2 (NMC111) and LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cathodes by using both single-solvent model electrolytes and the mixed solvents used in commercial cells. While NMC111 exhibits similar parasitic currents with EC-containing and EC-free electrolytes during high voltage holds in NMC/Li 4 Ti 5 O 12 (LTO) cells, this is not the case for NMC811. Online gas analysis reveals that the solvent-dependent reactivity for Ni-rich cathodes is related to the extent of lattice oxygen release and accompanying electrolyte decomposition, which is higher for EC-containing than EC-free electrolytes. Combined findings from electrochemical impedance spectroscopy (EIS), TEM, solution NMR, ICP, and XPS reveal that the electrolyte solvent has a profound impact on the degradation of the Ni-rich cathode and the electrolyte. Higher lattice oxygen release with EC-containing electrolytes is coupled with higher cathode interfacial impedance, a thicker oxygen-deficient rock-salt surface reconstruction layer, more electrolyte solvent and salt breakdown, and higher amounts of transition metal dissolution. These processes are suppressed in the EC-free electrolyte, highlighting the incompatibility between Ni-rich cathodes and conventional electrolyte solvents. Finally, new mechanistic insights into the chemical oxidation pathways of electrolyte solvents and, critically, the knock-on chemical and electrochemical reactions that further degrade the electrolyte and electrodes curtailing battery lifetime are provided.

25 ENERGY STORAGE↗