Search NASA⌕ Search

Engineering topics

Weddle, Peter J.

Publications and source records attributed to Weddle, Peter J..

At least 19 records

Generating multi-scale Li-ion battery cathode particles with radial grain architectures using stereological generative adversarial networks

Abstract Understanding structure-property relationships of Li-ion battery cathodes is crucial for optimizing rate-performance and cycle-life resilience. However, correlating the morphology of cathode particles, such as in LiNi0.8Mn0.1Co0.1O2 (NMC811), and their inner grain architecture with electrode performance is challenging, particularly, due to the significant length-scale difference between grain and particle sizes. Experimentally, it is not feasible to image such a high number of particles with full granular detail. A second challenge is that sufficiently high-resolution 3D imaging techniques remain expensive and are sparsely available at research institutions. Here, we present a stereological generative adversarial network-based model fitting approach to tackle this, that generates representative 3D information from 2D data, enabling characterization of materials in 3D using cost-effective 2D data. Once calibrated, this multi-scale model can rapidly generate virtual cathode particles that are statistically similar to experimental data, and thus is suitable for virtual characterization and materials testing through numerical simulations. A large dataset of simulated particles with inner grain architecture has been made publicly available.

25 ENERGY STORAGE↗

PINN surrogate of Li-ion battery models for parameter inference, Part I: Implementation and multi-fidelity hierarchies for the single-particle model

To plan and optimize energy storage demands that account for Li-ion battery aging dynamics, techniques need to be developed to diagnose battery internal states accurately and rapidly. Here, this study seeks to reduce the computational resources needed to determine a battery's internal states by replacing physics-based Li-ion battery models - such as the single-particle model (SPM) and the pseudo-2D (P2D) model - with a physics-informed neural network (PINN) surrogate. The surrogate model makes high-throughput techniques, such as Bayesian calibration, tractable to determine battery internal parameters from voltage responses. This manuscript is the first of a two-part series that introduces PINN surrogates of Li-ion battery models for parameter inference (i.e., state-of-health diagnostics). In this first part, a method is presented for constructing a PINN surrogate of the SPM. A multi-fidelity hierarchical training, where several neural nets are trained with multiple physics-loss fidelities is shown to significantly improve the surrogate accuracy when only training on the governing equation residuals. The implementation is made available in a companion repository (https://github.com/NREL/PINNSTRIPES). The techniques used to develop a PINN surrogate of the SPM are extended in Part II for the PINN surrogate for the P2D battery model, and explore the Bayesian calibration capabilities of both surrogates.

25 ENERGY STORAGE↗

PINN surrogate of Li-ion battery models for parameter inference, Part II: Regularization and application of the pseudo-2D model

Bayesian parameter inference is useful to improve Li-ion battery diagnostics and can help formulate battery aging models. However, it is computationally intensive and cannot be easily repeated for multiple cycles, multiple operating conditions, or multiple replicate cells. To reduce the computational cost of Bayesian calibration, numerical solvers for physics-based models can be replaced with faster surrogates. A physics-informed neural network (PINN) is developed as a surrogate for the pseudo-2D (P2D) battery model calibration. For the P2D surrogate, additional training regularization was needed as compared to the PINN single-particle model (SPM) developed in Part I. Both the PINN SPM and P2D surrogate models are exercised for parameter inference and compared to data obtained from a direct numerical solution of the governing equations. A parameter inference study highlights the ability to use these PINNs to calibrate scaling parameters for the cathode Li diffusion and the anode exchange current density. By realizing computational speed-ups of ~2250x for the P2D model, as compared to using standard integrating methods, the PINN surrogates enable rapid state-of-health diagnostics. Finally, in the low-data availability scenario, the testing error was estimated to ~2 mV for the SPM surrogate and ~10 mV for the P2D surrogate which could be mitigated with additional data.

25 ENERGY STORAGE↗

Cohesive phase-field chemo-mechanical simulations of inter- and trans- granular fractures in polycrystalline NMC cathodes via image-based 3D reconstruction

The optimal design and durable utilization of lithium-ion batteries necessitates an objective modeling approach to understand fracture and failure mechanisms. This paper presents a comprehensive chemo-mechanical modeling study focused on elucidating fracture-induced damage and degradation phenomena in the polycrystalline Li $\mathcal{x}$ Ni 0.5 Mn 0.3 Co 0.2 O 2 (NMC532) cathode. An innovative approach that utilizes image-based reconstructed 3D geometry as finite element (FE) mesh input is employed to enhance the precision in capturing the convoluted architecture and morphological features. For accurately representing the intricate crack configurations within the polycrystalline system, we adopted the cohesive phase-field fracture (CPF) model. Through the integration of advanced image-based geometry reconstruction technique and the promising CPF modeling approach, lithium (de)intercalation induced crack evolution (e.g., nucleation, propagation, branching and diverse modes including inter-/trans-(intra-) granular patterns) and the resulting chemical degradation can be precisely captured, which is also compared and validated with numerical predictions using a continuum damage model. In particular, this model predicts fracture induced degradation under varying fracture properties of grain boundaries and charging rates; the conclusion that NMC particles comprised of larger grains are predicted to have less degradation than those with smaller grains can also be drawn. This comprehensive analysis provides valuable insights into the fracture and degradation within polycrystalline NMC cathodes.

25 ENERGY STORAGE↗

Consequences of plane-strain and plane-stress assumptions in fully coupled chemo-mechanical Li-ion battery models

In Li-ion battery research, it is common to simulate chemo-mechanical phenomena in reduced dimensions (e.g., 2-D) as opposed to fully resolve these complex physics in 3-D. It is common to assume either (1) the out-of-plane strain is negligible (commonly referred to as plane-strain), or (2) the out-of-plane stress is negligible (commonly referred to as plane-stress). However, there is typically little consideration as to the quantitative consequences of these approximations. Furthermore, the influence of these out-of-plane assumptions can be compounded and convoluted when chemo-mechanics models implement so-called “fully coupled” formulations, where the local species concentrations influence the stress-state and the stress-state influences the local species fluxes. Here, the present manuscript explores the implications of using plane-stress and plane-strain assumptions in 2-D as compared to simulating a full 3-D electrode particle. This comparative study includes simulating both isotropic and anisotropic particle intercalation where the particles can be surrounded by either a liquid or solid electrolyte. Additionally, common Li-ion battery-model metrics such as the state-of-stress, intercalation fraction distribution, and specific capacity are compared, while also considering the effects of particle size and C-rate. As alternatives to the pure plane-strain and plane stress approximations, two modified plane-strain assumptions are found to better approximate the fully coupled chemo-mechanical 3-D behavior.

25 ENERGY STORAGE↗

Battery state-of-health diagnostics during fast cycling using physics-informed deep-learning

Rapid, in-situ Li-ion battery state-of-health (SOH) quantification is challenging. Li-ion battery aging can vary significantly with chemistry, operating conditions, cycling demands, electrode design, and operation history. As a cell ages, optimal and safe operating conditions need to be adapted to account for battery degradation by tracking critical aging modes such as loss-of-lithium-inventory (LLI), loss-of-active-material (LAM) in either electrode, and/or impedance rise. This manuscript describes a framework for identifying battery aging modes in-operando using fast-rate voltage charge/discharge responses. The framework uses a physically based Li-ion battery model to produce synthetic high-rate responses at aged states. The aging model is calibrated against experimental data from cells with different electrode loadings and cycled under a variety of fast-charging conditions (1 h, 15 min, 10 min, and 7 min charging). The synthetically generated high-rate responses at aged states are then used to train a deep-learning model to identify real cell state-of-health from fast charge/discharge battery voltage responses. The synthetically trained deep-learning model performance is validated by comparing to standard incremental capacity analysis and half-cell measurements. Finally, the framework demonstrates the benefits of using high-rate physics-based models to generate synthetic data for training deep-learning models.

25 ENERGY STORAGE↗

Voltage-Based Strategies for Preventing Battery Degradation under Diverse Fast-Charging Conditions

Maintaining safe operating conditions is a key challenge for high-performance lithium-ion battery applications. The lithium-plating reaction remains a risk during charging, but limited studies consider the highly variable charging conditions possible in commercial cells. Here we combine pseudo-2D electrochemical modeling with data visualization methods to reveal important relationships between the measurable cell voltage and difficult-to-predict Li-plating onset criteria. An extensively validated model is used to compute Li plating for thousands of multistep charging conditions spanning diverse rates, temperatures, states-of-charge, and cell aging. Here we observe an empirical cell operating voltage limit below which plating does not occur across all conditions, and this limit varies with the battery state-of-charge and aging. A model sensitivity analysis also indicates that, when comparing two charging voltage profiles, the capacity difference at 4.0 V correlates well with the difference in the plating onset capacity. These results encourage simple strategies for Li-plating prevention that are complementary to existing battery controls.

25 ENERGY STORAGE↗

Cell-Format-Dependent Mechanical Damage in Silicon Anodes

Strong binders can be counterproductive for silicon anodes. Here, we show that stresses from cycling Si-based electrodes can cause permanent stretching and wrinkling of the current collector. Furthermore, this deformation damages the electrode coating and accelerates cell aging due to the inactivation of Si domains and facilitation of Li plating. Interestingly, we demonstrate that the formation of wrinkles is size-dependent, being present in pouch cells but absent from coin cells. This size-dependent performance decay indicates that, in extreme cases, testing outcomes are highly dependent on scale and that the validation of battery materials may require testing at larger cell formats.

25 ENERGY STORAGE↗

Rational designs to enable 10-min fast charging and long cycle life in lithium-ion batteries

A daunting challenge in the design of lithium ion batteries (LiBs) is enabling 10-min extreme fast charging (XFC) while achieving appreciable charge acceptance and cycle life. This desirable outcome requires both a comprehensive understanding of LiB operation and aging behavior at different length scales and careful optimization. Lithium plating has been a critical bottleneck because, at XFC rates, it consumes cyclable lithium causing distinct aging and safety concerns even in moderate-loading LiBs. Here, we propose combining multiple solutions, including materials-to-electrode design-to-charging protocols, that are intended to overcome limitations in lithium-ion transport in the electrolyte phase, thus enabling 10-min XFC in LiBs. Some implemented strategies include cathode chemistry, optimized carbon binder domain in the cathode, dual layer anode design, improved separator and advanced electrolyte. Further, innovative charging protocols in moderately loading (~3 mAh/cm 2 anode/2.7 mAh/cm 2 cathode) single-layer pouch cells are proposed, together with demonstrated 10-min XFC with higher charge acceptance between 87.3 and 92.1% (or 2–2.1 mAh/cm 2 ) for 600 cycles without lithium plating. This methodical study with well-defined cells shows promise in combining multiple solution strategies to enable 10-min XFC, charting a pathway to achieve XFC in higher-loading energy-optimized LiBs.

25 ENERGY STORAGE↗

Dynamic In‐Plane Heterogeneous and Inverted Response of Graphite to Fast Charging and Discharging Conditions in Lithium‐Ion Pouch Cells

Solutions for improving fast charging of lithium‐ion batteries have largely focused on alleviating through‐plane lithiation gradients while little is understood about in‐plane heterogeneities and how to resolve them. Herein, high‐speed synchrotron X‐ray diffraction (XRD) resolves graphite lithiation spatially and temporally during 6 C charging and 2 C discharging. At every point during operation, considerable differences in the state of lithiation across the pouch cell are present. Some regions are more responsive to operation than others, reaching full lithiation early during charge and full delithiation during discharge. Other regions within the cell never fully delithiate during discharge, despite a prolonged voltage hold at 2.8 V. Using time‐resolved XRD data, the calculated local current density (mA cm −2 ) at the graphite surface shows an unexpected occurrence of local inverted current densities where regions of graphite are observed to delithiate during charging and lithiate during discharging. A pseudo‐3D model is developed for the graphite electrode with spatially varying microstructural tortuosity to show how microstructural heterogeneity could influence spatial charge dynamics. The model could not predict the complex in‐plane charge behavior observed within the cell. Consequently physics‐based charging protocols based on homogeneous electrode assumptions may underestimate the local variations in charge dynamics and occurrence of lithium plating.

25 ENERGY STORAGE↗

Enabling Extreme Fast-Charging: Challenges at the Cathode and Mitigation Strategies

We report charging lithium-ion batteries (LiBs) in 10 to 15 min via extreme fast-charging (XFC) is important for the widespread adoption of electric vehicles (EVs). Lately, the battery research community has focused on identifying XFC bottlenecks and determining novel design solutions. Like other LiB components, cathodes can present XFC bottlenecks, especially when considering long-term battery life. Therefore, it is necessary to develop a comprehensive understanding of how XFC conditions degrade LiB cathodes. The present article reviews relevant cathode-focused studies and summarizes the current understanding regarding cathode performance and aging issues under XFC conditions. Dominant aging modes and mechanisms are identified at different length-scales with electrochemical correlations for LiNi x Mn y Co z O 2 (NMC)-based cathodes. A range of electrochemical techniques and models provide key insights into cathode performance and life issues. A suite of multimodal and multiscale microscopy and X-ray techniques is surveyed to quantify chemical, structural, and crystallographic NMC-cathode degradation. Cathode cycle-life is scaled to equivalent EV miles to illustrate how cathode degradation translates to real-world scenarios and quantifies cathode-related bottlenecks that hinder XFC adoption. Finally, the article discusses several cathode cycle-life aging mitigation strategies with example case studies and identifies remaining challenges.

25 ENERGY STORAGE↗

Quantifying Graphite Solid-Electrolyte Interphase Chemistry and its Impact on Fast Charging

The solid-electrolyte interphase (SEI) enables the remarkable capacity retention of lithium-ion batteries, yet a comprehensive quantitative description of the SEI composition remains elusive. Using a combination of differential electrochemical mass spectrometry and mass spectrometry titration, we quantify graphite SEI components formed under electrolytes of varying salt concentrations. We find that, regardless of salt concentration, a conversion of initially deposited lithium ethylene dicarbonate to monocarbonates (likely lithium ethylene monocarbonate) and noncarbonate species occurs, and the extent of this conversion increases with electrolyte aging. Here, we additionally demonstrate that as the concentration increases (up to 2.0 M LiPF6), the SEI becomes progressively thinner with more LiF and less solid carbonates deposited. Finally, we reveal that less dead lithium formation and less solid carbonate deposition occur during prolonged fast charging for higher-concentration electrolytes. Because of the advantages imparted by a thinner SEI, the onset state of charge for lithium plating for the 2.0 M electrolyte is later than that predicted by a standard electrochemical model, underscoring the importance of explicit SEI effects in future electrochemical models.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Laser ablation for structuring Li-ion electrodes for fast charging and its impact on material properties, rate capability, Li plating, and wetting

Laser ablation is a scalable technique for decreasing the effective tortuosity of electrodes by selectively removing material with high precision. Applied to ≈ 110 um thick electrode coatings, this work focuses on understanding the impact of laser ablation on electrode material properties at the beginning of life and synergistic impacts of ablated channels on cell performance throughout their cycle life. Post laser ablation, local changes in chemistry, crystallography, and morphology of the laser-impacted electrode regions are investigated. It is shown that femtosecond pulsed laser ablation can achieve high-rate material removal with minor material damage locally at the interface of the impacted zones. The capacity achieved during a 6C (10 min) constant-current constant-voltage charge to 4.2 V improved from 1 mAh cm -2 for the non-ablated electrodes to almost 2 mAh cm -2 for the ablated electrodes. This benefit is attributed to a synergistic effect of enhanced wetting and decreased electrode tortuosity. The benefit was maintained for over 120 cycles, and upon disassembly decreased Li-plating on the graphite anode was observed. Finally, multi-physics modeling in conjunction with wetting analyses showed that laser ablating either one of the electrodes led to substantial improvements in wetting and rate capability, indicating that substantial performance benefits can be achieved by ablating only the graphite anode as apposed to both electrodes.

25 ENERGY STORAGE↗

A Comprehensive Understanding of the Aging Effects of Extreme Fast Charging on High Ni NMC Cathode

As the battery industry shifts toward high Ni content cathodes, such as LiNi 0.8 Mn 0.1 Co 0.1 O 2 [NMC811], a complete understanding of the degradation mechanisms of NMC811 under extreme fast charging (XFC) (XFC, ≤10–15 min charging) conditions is needed. Such comprehensive understanding would identify the most critical materials gaps that need to be addressed for enabling XFC long-life cells for electric vehicles. This study maps out the key aging mechanisms for NMC811 cycled at different XFC conditions (between 1C and 9C) for up to 1000 cycles. To acquire a fundamental understanding of utilization and degradation, cells are evaluated using a range of electrochemical techniques, and multimodal and multiscale microscopy techniques to quantify chemical, structural, and crystallographic degradation as a function of cycling conditions for the NMC cathode. When comparing NMC811 to NMC532, it is observed that NMC811 has a greater subsurface crystallographic degradation and displays a similar magnitude of subparticle cracking. However, the NMC811 maintains superior performance despite those advanced degradations. Here, the superior cycle life performance is attributed to the NMC811 particles having radially oriented grains and improved transport properties. NMC811 shows between 4.6× and 3.15× reduction in capacity fade than NMC532 for charging rates between 4C (e.g., 15-min charging) and 6C (10-min charging).

25 ENERGY STORAGE↗

Developing extreme fast charge battery protocols – A review spanning materials to systems

Extreme fast charging (XFC) has become a focal research point in the lithium-battery community over the last several years. As adoption of electric vehicles increases, fast charging has become a key driver in enhancing consumer recharge experience. Recently, the research community has made significant improvements in developing charge protocols to support XFC. New charge protocol designs derived using a combination of advanced, physically derived models, and electrochemical and secondary characterization methods, increase charge acceptance and decrease aging. By coordinating these methods and modifying protocols to account for different material constraints, including lithium plating and cathode particle degradation, novel charge protocols have increased the energy accepted during charging by over 25% in 10 min and increased the charge acceptance prior to a constant-voltage step by approximately 3x. Here, we review several charge-protocol advances, aging factors which are enhanced by XFC and advances which will enable adoption of XFC capable vehicles. These advances include implementing machine learning and other detection algorithms to reduce and classify lithium plating, which is known to significantly degrade cell performance and reduce cell life. The review concludes by discussing full-system fast charge requirements, including electric vehicle service equipment needs for implementing XFC protocols.

25 ENERGY STORAGE↗

Quantifying the Influence of Charge Rate and Cathode-Particle Architectures on Degradation of Li-Ion Cells Through 3D Continuum-Level Damage Models

In this article, we develop a 3D, continuum-level damage model implemented on statistically generated LiNi 0.5 Mn 0.3 Co 0.2 O (NMC 532) secondary cathode particles. The primary motivation of the particle-level model is to inform cathode-particle design through detailed exploration of the influence of secondary and primary particle sizes on the damage predicted during operation, and determine charging profiles that reduce cathode fracture. The model considers NMC 532 secondary particles containing an agglomeration of anisotropic, randomly oriented grains. These brittle, Ni-based cathodes are prone to mechanical degradation, which reduces overall battery cycle life. The model predicts that secondary-particle fracture is primarily due to non-ideal grain interactions and high-rate charge demands. The model predicts that small secondary-particles with large grains develop significantly less damage than larger secondary particles with small grains. The model predicts most of the chemo-mechanical damage accumulates in the first few cycles. The chemo-mechanical model predicts monotonically increasing capacity fade with cycling and rate. Comparing to experimental results, the model is well suited for capturing initial capacity fade mechanisms, but additional physics is required to capture long-term capacity fade effects.

25 ENERGY STORAGE↗