Search NASA⌕ Search

Engineering topics

Wood, David L.

Publications and source records attributed to Wood, David L..

At least 19 records

Understanding slurry formulations to guide solution-processing of solid electrolytes

Scalable processing of thin solid electrolytes is crucial for engineering solid-state batteries with practical energy densities. To leverage existing battery production infrastructure, pathways for solution processing of solid electrolyte films must be investigated. Here, roll-to-roll compatible film preparation of aluminum-doped lithium lanthanum zirconate oxide was studied. Four slurry configurations accounting for different solvent properties and solid loadings were evaluated to investigate the ternary interactions within the dispersions. Rheological and coating stability analyses were carried out on the processed slurries. The analysis and characterization indicated that improved component interactions within the ethanol/toluene system result in homogenized distribution of the particles, binder, and plasticizer, and enable the extraction of free-standing thin films with thicknesses of 20 μm and large area (>15 in. 2 ). The drawbacks and opportunities of several protocols for high temperature sintering of the dried green films were investigated. This study highlights the importance of engineering dispersions during the development of processing protocols for solid electrolytes and provides guidelines for the best practices that can be leveraged for solution processing–based fabrications for a wide range of solid electrolyte materials.

25 ENERGY STORAGE↗

Review—Electrospun Inorganic Solid-State Electrolyte Fibers for Battery Applications

Inorganic solid-state electrolytes (SSEs), especially Li 7 La 3 Zr 2 O 12 (LLZO), are promising candidates for all solid-state batteries. Generally, SSEs are synthesized by solid-state reactions at high temperatures. The high temperature required to synthesize useful polymorphs (e.g., cubic phase, in the case of LLZO) increases their production cost. To lower the synthesis temperature, several approaches, including doping and crystallite size control via sol-gel processes, have been explored. Recently, electrospinning was used to synthesize the inorganic SSE fibers to control the crystallite size and lower the calcination temperature. Several publications followed that investigated the properties of fibers and demonstrated the use of these fibers in inorganic-polymer composite SSEs. This paper presents a concise discussion of electrospinning, the parameters that control fiber morphology, the synthesis of inorganic SSE fibers, the effect of sintering conditions on the fiber morphology and composition, and the recent use of these fibers in making composite SSEs and other battery applications. Additionally, most of the discussion focuses on LLZO, but this paper also discusses applications of other types of electrospun inorganic electrolyte fibers, the challenges of using these fibers, and possible future directions in this research field.

25 ENERGY STORAGE↗

Nanostructured ligament and fiber Al–doped Li 7 La 3 Zr 2 O 12 scaffolds to mediate cathode-electrolyte interface chemistry

In this study, scaffold structures of electrospun aluminum–substituted lithium lanthanum zirconate Li 7 La 3 Zr 2 O 12 (Al-LLZO) were synthesized and used as an additive in a LiNi 0.6 Mn 0.2 Co 0.2 O 2 composite cathode. The scaffolds were crystalized in the cubic phase after calcination at 700 °C. The Al-LLZO scaffold morphology was dependent on the precursor formulation (aqueous and dimethylformamide. The aqueous precursors resulted in scaffolds of densely coalesced ligaments, whereas the dimethylformamide precursors resulted in high–aspect ratio nanofiber scaffolds. The long-term cycling stability and rate performance of the cells were found to depend on the Al-LLZO scaffold morphology. The uniformly dispersed Al-LLZO fibers resulted in a more stable cathode electrolyte interface formation through the reduced decomposition of the LiPF 6 salt during cycling, resulting in a better high-rate and long-term cycling performance.

25 ENERGY STORAGE↗

Electrochemical Healing of Dendrites in Garnet-Based Solid Electrolytes

Garnet oxides are a promising material family for solid-state batteries (SSBs). Dendrite formation in solid electrolytes critically limits the applicability of SSBs because of limiting Coulombic efficiency and power capability. In this study, the authors report operando electrochemical healing of dendrites in a garnet-based solid electrolyte (SE). Dendrites were deliberately formed at high operational current density (2 mA cm –2 ) beyond the critical current density (0.55 mA cm –2 ) of the used garnet SE. Electrochemical impedance spectroscopy and scanning electron microscopy were used to confirm dendrite growth in the SE. Dendrites were subsequently healed electrochemically via plating and stripping at 20 and 1 μA cm –2 current densities. Removal of dendrites was shown by an increase in bulk and interfacial resistance and a progressive increase in polarization during galvanostatic plating and stripping. High local current density at the dendrite tips was identified as the mechanism for preferentially removing dendrites electrochemically. The dendrite detection and healing methods discussed here are crucial for extending the life of SSBs.

25 ENERGY STORAGE↗

Probing Thermal Stability of Li-Ion Battery Ni-Rich Layered Oxide Cathodes by means of Operando Gas Analysis and Neutron Diffraction

Thermal stability is a crucial parameter that must be considered within the overall performance metrics of Ni-rich layered oxide cathodes. While the intrinsic structural stability of the cathode materials under thermal conditions is important, it is also critical to consider their reaction with electrolytes. In this study, operando gas analysis, ex situ neutron diffraction, and differential scanning calorimetry were combined to give a broader picture of the thermal stability of Ni-rich NMC cathodes. Li 1– x Ni 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) composite materials with four different states of charge were investigated with and without the presence of an electrolyte. It has been found that electrolyte can greatly accelerate both the structural and thermal decomposition of the cathode materials. A higher state of charge will also make cathode materials more susceptible to thermal shock. Without an electrolyte, O 2 release inducing a structural change from layered to rock salt was the major observation during thermal runaway. However, all samples retained some levels of layered structure after annealing up to 300 °C without the electrolyte. In comparison, almost all the O3-type layered phase transformed to the rock-salt phase for the cathode materials heated with the electrolyte at the same experimental conditions. Moreover, the amount of CO 2 increased by nearly two orders of magnitude when annealing cathode materials with electrolyte in operando gas analysis experiments. More delithiated NMC811 samples released larger amounts of CO 2 at earlier onset temperatures, resonating well with the differential scanning calorimetry (DSC) results showing that more delithiated samples release more heat during thermal shock.

25 ENERGY STORAGE↗

Eutectic Synthesis of the P2-Type Na x Fe 1/2 Mn 1/2 O 2 Cathode with Improved Cell Design for Sodium-Ion Batteries

An engaging area of research in sodium-ion batteries (SIBs) has been focusing on discovery, design, and synthesis of high-capacity cathode materials in order to boost energy density to levels close enough to that of state-of-the-art lithium-ion batteries. Of particular interest, P2-type layered oxide, Na 2/3 Fe 1/2 Mn 1/2 O 2 , has been researched as a potential cathode in SIBs based on its high theoretical capacity of 260 mA h/g and use of noncritical materials. However, the reported synthesis methods are not only complex and energy-demanding but also often yield inhomogeneous and impure materials with capacities less than 200 mA h/g under impractical test conditions. Here, we report a novel synthesis route using low-temperature eutectic reaction to produce highly homogeneous, crystalline, and impurity-free P2-Na x Fe 1/2 Mn 1/2 O 2 with enhanced Na-ion diffusivity and kinetics. The overall electrochemical performances of the Na-ion cells have been improved by pairing the P2-cathode with presodiated hard carbon anodes, leading to reversible capacities in the range of 180 mA h/g. This new approach is a contribution toward the simplification of synthesis and scalability of sodium-based cathodes with high crystallinity and fine-tuned morphology and the realization of a sodium-ion battery system with lower cost and improved electrochemical performance.

25 ENERGY STORAGE↗

Effect of formation protocol: Cells containing Si-Graphite composite electrodes

The effect of formation protocol was observed in tests using small pouch cells containing silicon-graphite/Li(Ni 0.5 Mn 0.3 Co 0.2 )O 2 chemistry. The time for the formation protocol was either 13.2 or 186 h for the tested cells. It is demonstrated that the “fast” formation protocol produces cells with similar performance characteristics to that of the “slow” protocol. Moreover, the solid-electrolyte interface layers from both formation protocols are stable and function analogously, albeit with different chemistry. The fast formation protocol may thus allow a more economical route to cell fabrication.

25 ENERGY STORAGE↗

Drying Temperature and Capillarity-Driven Crack Formation in Aqueous Processing of Li-Ion Battery Electrodes

Unlike conventional electrode processing for Li-ion batteries, which uses the expensive and highly toxic organic N -methyl-2-pyrrolidone (NMP) solvent, aqueous processing simply employs deionized water as the solvent. Yet, thick aqueous processed cathodes have been found to crack during drying. Here, the influence of electrode drying temperature and thickness on cracking was investigated. LiNi 1/3 Mn 1/3 Co 1/3 O 2 cathodes prepared with a hydrophilic binder, modified styrene–butadiene rubber (SBR), were coated at various thicknesses and dried at temperatures ranging from 20 to 70 °C. Experiments revealed cracking worsens with increased electrode thickness and elevated drying temperatures. Cracks were formed during the capillarity-driven phase during drying. Strong evaporation and weak diffusion played a critical role in the nonuniform distribution of the inactive phase. Images of electrode surfaces were processed to quantify crack dimensions and crack intensity factor (CIF). The average crack length and width, as well as CIF, increased with drying temperature and electrode thickness. Electrochemical performance revealed a strong and negative correlation between the crack density and performance in terms of specific capacity. Transport limitations associated with the presence of cracks adversely affect the advantage of high volume ratio of active materials in the thick electrodes.

25 ENERGY STORAGE↗

Effect of overcharge on lithium-ion cells: Silicon/graphite anodes

Small pouch cells containing Si/graphite electrodes were systematically charged to 100, 120, 140, 160, 180 and 250% state of charge. Description of the Si/graphite electrode after the overcharge showed some features similar to those found in a pure graphite electrode. Since the amount of silicon in the electrode was ~15 wt%, this was not unexpected. The effect of silicon was observed in the composition of the SEI layer and the trends in two components of the SEI layer.

25 ENERGY STORAGE↗

Analysis of electrolyte imbibition through lithium-ion battery electrodes

A quantitative measurement of wettability between the porous electrode and the electrolyte in lithium-ion batteries can greatly improve our understanding of wetting behavior. Although the wetting balance method is widely used to measure the electrolyte transport rate in the porous electrodes, it suffers from several drawbacks and has limited accuracy. We here presented a combined experimental and theoretical investigation of the dynamics of electrolyte imbibition through electrodes. We suggested a novel method to accurately measure the electrolyte imbibition rate. Excellent agreement between the experimental data and the developed analytical model is obtained. The coefficient of penetrance (COP) and the solid permeability coefficient (SPC) are identified as important parameters, i.e., the electrolyte with higher COP value wets faster into an electrode, whereas for an electrolyte, the electrode with higher SPC value is more amenable to be impregnated. The effect of electrolyte salt concentration and electrolyte solvent has been studied in detail. The result implies that increasing salt concentration adversely influences electrolyte wetting rate, whereas switching from EC-DEC system to EC-EMC system improves electrolyte wetting rate. Moreover, for the electrolytes tested in this study, the imbibition into the uncalendered graphite anode is much faster than that into the uncalendered NMC532 cathode.

25 ENERGY STORAGE↗

Unveiling the Role of Al 2 O 3 in Preventing Surface Reconstruction During High-Voltage Cycling of Lithium-Ion Batteries

Recent achievements in high-energy batteries have been made by using Ni-rich NMC cathodes (LiNi x Mn y Co 1–x–y O 2 with x > 0.5) in conjunction with higher cell voltages. However, these gains have come at a cost of fast capacity fade and poor rate performace. In our previous study, we showed that Al 2 O 3 ALD coatings on LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) and LiNi 0.8 Co 0.15 Al 0.05 O 2 (NCA) cathodes prevented surface phase transitions, reduced impedance, and extended cycle life in high voltage cells. In this work, neutron diffraction (ND), X-ray photoelectron spectroscopy (XPS), and electron energy loss spectroscopy (EELS) are used to fully investigate the mechanism by which ALD surface coatings mitigate NMC811 cathode degredation. Refinement of ND patterns indicated no changes in the bulk crystal structure of cycled cathodes with or without the Al 2 O 3 coating. Rather, the improved performance of ALD-coated cathodes is clearly due to surface stabilization. EELS established that all three transition metal oxidation states were reduced at the surface of the uncoated cathode after cycling, whereas the coated cathode showed no changes in surface oxidation states relative to the bulk. The surface coatings also prevented transition metal dissolution and crossover. XPS analysis of the anode harvested from cycled cells with uncoated cathodes showed significant amounts of Mn deposited within the SEI. In contrast, no Mn could be detected on the anodes cycled with coated cathodes. These results affirm that ALD coatings can effectively reduce the reactivity of the NMC surface and prevent detrimental side reactions that shorten battery cycle life.

25 ENERGY STORAGE↗

Balancing formation time and electrochemical performance of high energy lithium-ion batteries

Most lithium-ion batteries still rely on intercalation-type graphite materials for anodes, and the formation process for them typically takes several days or even more to provide a stable solid electrolyte interphase (SEI). The slow formation step results in lower LIB production rates, requires a large number of battery cyclers, and constitutes the second highest cost during battery manufacturing. In an effort to decrease the high manufacturing cost associated with long formation times, here we studied five different formation protocols in nickel-rich LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811)/graphite cells where the total formation time varied from 10 to 86 h. Electrochemical characterization and post mortem analysis show that very long formation time do not necessarily improve long-term performance while very short formation protocols result in lithium plating and poorer electrochemical performance. Finally, we find the optimum formation cycling protocol is intermediate in length to minimize impedance growth, improve capacity retention, and avoid lithium plating.

25 ENERGY STORAGE↗

Si Oxidation and H 2 Gassing During Aqueous Slurry Preparation for Li-Ion Battery Anodes

Si has the possibility to greatly increase the energy density of Li-ion battery anodes, though it is not without its problems. One issue often overlooked is the decomposition of Si during large scale slurry formulation and battery fabrication. Here, we investigate the mechanism of H 2 production to understand the role of different slurry components and their impact on the Si oxidation and surface chemistry. Mass spectrometry and in situ pressure monitoring identifies that carbon black plays a major role in promoting the oxidation of Si and generation of H 2 . Si oxidation also occurs through atmospheric O 2 consumption. Both pathways, along with solvent choice, impact the surface silanol chemistry, as analyzed by 1 H– 29 Si cross-polarization magic angle spinning nuclear magnetic resonance (MAS NMR) and attenuated total reflectance Fourier transform infrared spectroscopy (ATR FTIR). An understanding of the oxidation of Si, during slurry processing, provides a pathway toward improving the manufacturing of Si based anodes by maximizing its capacity and minimizing safety hazards.

25 ENERGY STORAGE↗

Effect of overcharge on Li(Ni 0.5 Mn 0.3 Co 0.2 )O 2 /Graphite lithium ion cells with poly(vinylidene fluoride) binder. I - Microstructural changes in the anode

Cells based on NMC/graphite, containing poly(vinylidene difluoride) (PVDF) binders in the positive and negative electrodes, were systematically overcharged to 100, 120, 140, 160, 180, and 250% state-of-charge (SOC). At 250% SOC the cell vented. Scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS) of the anodes showed several state-of-overcharge-dependent trends. Starting at 120% SOC, dendrites appeared and increased in concentration as the SOC increased. Dendrite morphology appeared to be dependent on whether the active material was on the “dull” or “shiny” side of the copper collector. Significantly more delamination of the active material from the collector was seen on the “shiny” side of the collector particularly at 180 and 250% SOC. Transition metals were detected at 120% SOC and increased in concentration as the SOC increased. Finally, there was considerable spatial heterogeneity in the microstructures across each laminate with several regions displaying complex layered structures.

25 ENERGY STORAGE↗

What makes lithium substituted polyacrylic acid a better binder than polyacrylic acid for silicon-graphite composite anodes?

Lithium substituted polyacrylic acid (LiPAA) has previously been demonstrated as a superior binder over polyacrylic acid (PAA) for Si anodes, but from where does this enhanced performance arise? In this paper, full cells are assembled with PAA and LiPAA based Si-graphite composite anodes that dried at temperatures from 100 °C to 200 °C. The performance of full cells containing PAA based Si-graphite anodes largely depend on the secondary drying temperature, as decomposition of the binder is correlated to increased electrode moisture and a rise in cell impedance. Full cells containing LiPAA based Si-graphite composite electrodes display better Coulombic efficiency than those with PAA, because of the electrochemical reduction of the PAA binder. This is identified by attenuated total reflectance Fourier transform infrared spectrometry and observed gassing during the electrochemical reaction. Finally, Coulombic losses from the PAA and Si SEI, along with depletion of the Si capacity in the anode results in progressive underutilization of the cathode and full cell capacity loss.

25 ENERGY STORAGE↗

Effect of overcharge on Li(Ni 0.5 Mn 0.3 Co 0.2 )O 2 cathodes: NMP-soluble binder. II — Chemical changes in the anode

For this study, cells based on nickel manganese cobalt oxide (NMC)/graphite electrodes, which contained polyvinylidene difluoride (PVDF) binders in the electrodes, were systematically charged to 100, 120, 140, 160, 180, and 250% state of charge (SOC). Characterization of the anodes by inductively-coupled-plasma mass spectrometry (ICP-MS), X-ray photoelectron spectroscopy (XPS), and high-performance liquid chromatography coupled with electrospray ionization mass spectrometry (HPLC-ESI-MS) showed several extent-of-overcharge-dependent trends. The concentrations (by wt) of nickel, manganese, and cobalt in the negative electrode increased with SOC, but the metals remained in the same ratio as that of the positive. Electrolyte reaction products, such as LiF:LiPO 3 , increased with overcharge, as expected. Three organic products were found by HPLC-ESI-MS. From an analysis of the mass spectra, two of these compounds seem to be organophosphates, which were formed by the reaction of polymerized electrolyte decomposition products and PF 3 or O=PF 3 . Their concentration tended to reach a constant ratio. The third was seen at 250% SOC only.

25 ENERGY STORAGE↗

Effect of overcharge on Li(Ni 0.5 Mn 0.3 Co 0.2 )O 2 /graphite lithium ion cells with poly(vinylidene fluoride) binder. III — Chemical changes in the cathode

Here, 1.5 Ah pouch cells based on Li(Ni 0.5 Mn 0.3 Co 0.2 )O 2 cathodes and graphite anodes, both containing poly (vinylidene fluoride) (PVDF) binders, were systematically overcharged to 100, 120, 140, 160, 180, and 250% state of charge (SOC), at which point they vented. The cells were subsequently discharged to 0% SOC and disassembled under an inert atmosphere for characterization. A combination of X-ray photoelectron spectroscopy (XPS), scanning-electron microscopy (SEM), energy-dispersive spectroscopy (EDS), 6 Li SSNMR, and X-ray diffraction (XRD) analysis of the NMC532 cathodes indicates the formation of a thin C- and O-rich cathode electrolyte interphase layer, progressive Li loss above 140% SOC, and retention of the bulk crystal structure at all states of charge.

25 ENERGY STORAGE↗