Wu, Y Q

Publications and source records attributed to Wu, Y Q.

Effective grain pinning revealed by nanoscale electron tomography

The grain pinning behavior of TiC particles in a rapidly solidified MRE-Fe-B (MRE = Nd + Y + Dy) nanocrystalline hard magnet was studied using electron tomography (ET). The 3D reconstruction overcomes the inherent 2D nature of conventional transmission electronmicroscopy (TEM) to reveal how this grain boundary phase controls the nanoscale structure in the rapidly solidified alloy. The 3D reconstruction was performed on the optimally annealed alloy (750 C/15 min) with hard magnetic properties of M{sub r} = 8.1 kGs, H{sub c} = 6.2 kOe, (BH){sub max} = 11.2 MGOe measured at 300 k. The sampled volume, 425 x 425 x 92.5 nm{sup 3}, contains more than 20 grains of the RE2-14-1 phase and more than 70 TiC nanoparticles. The TiC grains shapes depend on their sizes and locations along the grain boundary. Most of the TiC particles are oval or short rod like shapes and range from 5 nm to 10 nm. TiC particles less than 10 nm formed between adjacent 2-14-1 grains, while the largest ones formed at triple junctions. There are -1.7 x 10{sup 8} TiC particles within a 1 mm{sup 3} volume in the alloy. This accounts for the strong grain boundary pinning effect, which limits grain growth during annealing.

36 MATERIALS SCIENCE↗

The mechanism of magnetic properties improvement and microstructure refinement of Zr in Nd[subscript 2]Fe[subscript 14]B

In order to understand the role of Zr addition in Nd{sub 2}Fe{sub 14}B (2-14-1), a systematic study of Zr in Nd{sub 2}Fe{sub 14}B was done on a series of stoichiometric samples (Nd{sub 1-x}Zr{sub x}){sub 2}Fe{sub 14}B with 0 {le} x {le} 0.16. As-cast ingots formed significant amounts of Nd{sub 2}Fe{sub 17} starting at x = 0.06, while in the melt-spun ribbons, no Nd{sub 2}Fe{sub 17} was observed for the range studied. A monotonic decrease in lattice parameters for the 2-14-1 phase indicate Zr solubility in the melt-spun ribbons, but this is not observed in the ingots. Magnetic and thermal measurements on the ribbons showed that the saturated magnetization Ms (around 16 kG), the spin reorientation temperature (125 K), and the Curie temperature (583 K) do not depend on the Zr content, while the anisotropy field Ha slightly decreased as the Zr content increased. The energy product (BHmax) and the coercive force H{sub c} are highly dependent on the solidification and annealing process. Scanning electron microscopy and transmission electron microscopy on the as-melt spun alloys are consistent with x-ray diffraction showing Zr solubility in the 2-14-1 grains. After annealing, Zr diffuses to the grain boundaries to form Zr enriched compounds. Thus, while Zr may exhibit a metastable solubility in Nd{sub 2}Fe{sub 14}B, the enhanced magnetic behaviors observed in melt-spun ribbons are due to the refinement of the microstructure and enhanced grain-boundary pinning.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Multiple charge density wave transitions in Gd2Te5

Diffraction measurements performed via transmission electron microscopy and high resolution X-ray scattering reveal two distinct charge density wave transitions in Gd{sub 2}Te{sub 5} at T{sub c1} = 410(3) and T{sub c2} = 532(3) K, associated with the on-axis incommensurate lattice modulation and off-axis commensurate lattice modulation respectively. Analysis of the temperature dependence of the order parameters indicates a non-vanishing coupling between these two distinct CDW states.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Microstructure and properties of 17-4PH steel plasma nitrocarburized with a carrier gas containing rare earth elements

The effect of rare earth addition in the carrier gas on plasma nitrocarburizing of 17-4PH steel was studied. The microstructure and crystallographically of the phases in the surface layer as well as surface morphology of the nitrocarburized specimens were characterized by optical microscope, X-ray diffraction and scanning tunneling microscope, respectively. The hardness of the surface layer was measured by using a Vickers hardness test. The results show that the incorporation of rare earth elements in the carrier gas can increase the nitrocarburized layer thickness up to 55%, change the phase proportion in the nitrocarburized layer, refine the nitrides in surface layer, and increase the layer hardness above 100HV. The higher surface hardening effect after rare earth addition is caused by improvement in microstructure and change in the phase proportion of the nitrocarburized layer.

36 MATERIALS SCIENCE↗

Correlation of the energy product with evolution of the nanostructure in Y,Dy,Nd-(Fe,Co)-B magnetic alloy

The devitrification behavior of nanocrystalline MRE{sub 2}(Fe,Co){sub 14}B+ZrC (MRE = Nd+Y+Dy) was studied using differential scanning calorimetry (DSC), synchrotron high temperature x-ray diffraction, and analytical transmission electron microscopy (TEM) techniques. Alloy ribbons were melt spun at 25 m/s to obtain an amorphous structure. Optimum hard magnetic properties (B{sub r} = 7.2 kG, H{sub c} = 12.7 kOe and (BH){sub max} = 10.8 MG Oe) were obtained in ribbons annealed at 750 C for 15 min. A reduced annealing temperature of 638 C and holding time from 0 to 11 min were chosen based on DSC analysis. Large changes in both microstructure and hard magnetic properties were found in a narrow window of annealing time, 4.5-6 min, resulting in a dramatic increase in energy product, remanence and coercivity: 0.96 MG Oe, 5.2 kG, 2.7 kOe to 5.7 MG Oe, 7.2 kG, 8.5 kOe for (BH){sub max}, B{sub r} and H{sub c}, respectively. Energy dispersive x-ray spectroscopy and energy filtered TEM analyses indicate that Zr- and C-rich particles ({approx} 5 nm) and thin grain boundary layers (1-2 nm thick) are formed surrounding 2-14-1 hard phase grains when the annealing time is over 6 min. Further annealing resulted in a more distinct hard phase surrounded by a nonmagnetic grain boundary phase {approx} 1 nm in thickness. The thin grain boundary layer phase starts to disappear with annealing time over 11 min. The partitioning behavior of various elements at different annealing conditions appears to be associated with significant changes in magnetic properties, leading to an improved optimum microstructure.

36 MATERIALS SCIENCE↗

Charge Density Wave Formation in R(2)Te(5) (R=Nd, Sm, And Gd)

The rare earth (R) tellurides R{sub 2}Te{sub 5} have a crystal structure intermediate between that of RTe{sub 2} and RTe{sub 3}, consisting of alternating single and double Te planes sandwiched between RTe block layers. We have successfully grown single crystals of Nd{sub 2}Te{sub 5}, Sm{sub 2}Te{sub 5}, and Gd{sub 2}Te{sub 5} from a self-flux and we describe here evidence for charge density wave formation in these materials. The superlattice patterns for all three compounds are relatively complex, consisting at room temperature of at least two independent wave vectors. Consideration of the electronic structure indicates that, to a large extent, these wave vectors are separately associated with sheets of the Fermi surface which are principally derived from the single and double Te layers.

36 MATERIALS SCIENCE↗

Magnetic properties and microstructure of gas atomized MRE2(Fe, Co)14B powder with ZrC addition (MRE=Nd + Y + Dy)

Gas atomization powder with Zr substitutions for the MRE and ZrC additions were systematically studied. The results show that the partial substitutions of Zr and the ZrC additions effectively improved glass formability in the alloys. Scanning electron microscopy (SEM) revealed that the as-atomized powder with a particle size of less than 32 {micro}m is predominately uniform equiaxed grains with an average grain size of 1.5 {micro}m. X-ray diffraction and differential thermal analysis measurements detected very tiny amounts of amorphous phase. After annealing at 700 C for 15 min, the SEM grain microstructure exhibits a minor change, but magnetic properties are substantially improved. M versus T measurements reveal that the phase composition evolved from 2:14:1 plus a small amount of 2:17 phases to a single 2:14:1 phase during the annealing process. The sieve analysis of the powders showed a particle size distribution with 90 wt % of the powder less than 45 {micro}m. The magnetic properties of the annealed powder varied with particle size. (BH){sub max} first increases with increasing particle size from 5 {micro}m, reaches the peak value in the size range of 20-25 {micro}m, and then decreases with increasing particle size. For the 20-25 {micro}m powder sample annealed at 700 C for 15 min, the (BH){sub max} of 9.6 MG Oe at room temperature and 5.6 MG Oe at 200 C were obtained, respectively.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Plasma synthesized boron nano-sized powder: The effect of processing conditions on the crystallographic and microstructural properties

Boron nano-sized powders (doped and undoped) were synthesized by the reaction of boron trichloride, BCl{sub 3}, and hydrogen, H{sub 2}, in a plasma. The gases were mixed and injected into an argon RF plasma where they combined and formed boron powder via gas phase nucleation. Methane gas, CH{sub 4}, was added in the case of carbon-doped powder. These powders were found to be suitable for the fabrication of high performance superconducting magnesium diboride (MgB{sub 2}) wires. Plasma synthesized boron particles typically had the shape of low aspect ratio spheroids that tended to form open, lacy agglomerates. Particle sizes ranged from 10 to 250 nm. A typical batch of boron powder contained a mixture of amorphous and crystalline material. In this study, the effects of plasma power and carbon dopant addition on the crystallinity, particle size, and microstructure of boron nanopowder were investigated using powder x-ray diffraction (XRD), scanning electron microscopy (SEM), transmission electron microscopy (TEM), and selected area electron diffraction (SAD). Particle size distribution was measured using SEM and TEM images. SAD patterns showed the characteristic halo of an amorphous material, but single crystal reflections were observed as well. Wires made from these powders attained 60,000 A/cm{sup 2} at 5 K and 5 Tesla and attained 25,000 A/cm{sup 2} at 20 K and 3 Tesla.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Charge density wave formation in R2Te5 (R=Nd, Sm, and Gd)

The rare earth (R) tellurides R{sub 2}Te{sub 5} have a crystal structure intermediate between that of RTe{sub 2} and RTe{sub 3}, consisting of alternating single and double Te planes sandwiched between RTe block layers. We have successfully grown single crystals of Nd{sub 2}Te{sub 5}, Sm{sub 2}Te{sub 5}, and Gd{sub 2}Te{sub 5} from a self-flux and we describe here evidence for charge density wave formation in these materials. The superlattice patterns for all three compounds are relatively complex, consisting at room temperature of at least two independent wave vectors. Consideration of the electronic structure indicates that, to a large extent, these wave vectors are separately associated with sheets of the Fermi surface which are principally derived from the single and double Te layers.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

High thermal stability of carbon-coated L10-FePt nanoparticles prepared by salt-matrix annealing

Monodisperse L1{sub 0}-FePt nanoparticles with size ranging from 3 to 8 nm were prepared by the salt-matrix annealing method. It was observed that the annealed particles have high thermal stability - no sintering occurred even when the particles were heated at 1100 C for an hour. This high thermal stability resulted from carbon coating of the particles during salt-matrix annealing as consequence of decomposition of surfactants.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Microstructure analysis of a SmCo/Fe exchange spring bilayer.

The microstructure of a magnetron sputtered Cr(20 nm)/Sm-Co(20 nm)/Fe(20 nm)/Cr(5 nm) exchange spring magnet was studied using an advanced analytical transmission electron microscopy to better understand the relationship between its chemistry and structure to enhance the energy product. It is shown that the Fe atoms diffuse into the well textured Sm-Co layer, causing a transition from the stoichiometric Sm{sub 2}Co{sub 7} near the Sm-Co/Cr interface to a defected Sm(Co,Fe){sub 5} in the Sm-Co-Fe intermixed area. The graded intermixed layer between Sm-Co and pure Fe gives rise to a compositionally enhanced energy product.

36 MATERIALS SCIENCE↗