Search NASA⌕ Search

Engineering topics

Xia, Yujian

Publications and source records attributed to Xia, Yujian.

Enhancing HT-WGS catalyst performance with stable monovalent copper species via electron supply from defect-induced MgO

Magnesium oxide (MgO) exhibits excellent synergy with cerium oxide (CeO2), serving as either textural or electronic promoters during catalytic reactions. However, achieving well-dispersed CeO2-MgO is technically challenging because they are known not to form solid solutions, and the crystal growth of CeO2 suppresses the structure formation of MgO, leading to MgO being in an inhomogeneous amorphous state within CeO2-MgO. For this reason, most of research groups have been struggling with synthesizing well-dispersed CeO2-MgO. This leads them to focusing on the interaction between the active metal and cerium, overlooking the true role of magnesium. In this study, we successfully synthesized well-dispersed CeO2-MgO via a spray pyrolysis-assisted evaporation-induced self-assembly method, followed by the impregnation of Cu. The location and dispersion of Cu nanoparticles were highly dependent on the MgO distribution. Additionally, we revealed that this significantly influenced the catalytic activity and stability towards the HTS reaction and furthermore supplies electrons to monovalent Cu species, helping maintain the stable electron structure and oxidation state of Cu species considered as active sites. These findings suggest that optimizing the MgO distribution in CeO2-MgO is a promising strategy for developing efficient catalysts for the HTS reaction, emphasizing the role of MgO in designing high-performance catalysts.

Kim, Min-Jae↗

Water-Surface Drag Coating: A New Route Toward High-Quality Conjugated Small-Molecule Thin Films with Enhanced Charge Transport Properties

Electronic properties of organic semiconductor (OSC) thin films are largely determined by their morphologies and crystallinities. However, solution-processed conjugated small-molecule OSC thin films usually exhibit abundant grain boundaries and impure grain orientations because of complex fluid dynamics during solution coating. Here, a novel methodology, water-surface drag coating, is demonstrated to fabricate high-quality OSC thin films with greatly enhanced charge transport properties. This method utilizes the water surface to alter the evaporation dynamics of solution to enlarge the grain size, and a unique drag-coating process to achieve the unidirectional growth of organic crystals. Furthermore, using 2,8-difluoro-5,11-bis(triethylsilylethynyl)anthradithiophene (Dif-TES-ADT) as an example, thin films with millimeter-sized single-crystal domains and pure crystallographic orientations are achieved, revealing a significant enhancement (4.7 times) of carrier mobility. More importantly, the resulting film can be directly transferred onto any desired flexible substrates, and flexible transistors based on the Dif-TES-ADT thin films show a mobility as high as 16.1 cm 2 V -1 s -1 , which represents the highest mobility value for the flexible transistors reported thus far. The method is general for the growth of various high-quality OSC thin films, thus opening up opportunities for high-performance organic flexible electronics.

36 MATERIALS SCIENCE↗

Real-time interface investigation on degradation mechanism of organic light-emitting diode by in-operando X-ray spectroscopies

Understanding the chemical evolution at the interface of organic light-emitting diodes (OLEDs) under working conditions is critical for addressing device failure and further improving performance. In this work, an in-operando approach was developed employing synchrotron-based X-ray absorption spectroscopy (XAS) to investigate the electronic structures and chemical degradation mechanisms of a model tris(8-hydroxyquinoline) aluminum (Alq 3 )-based OLED device under working condition. The results identify that Mg atoms from the electrode migrate into the Alq 3 organic layer under a potential bias and replace Al atom sites, forming the unstable Mgq 3 species which lead to device degradation. Here, the findings from the classic and simple model device elucidate the degradation mechanisms occurred at the interface of OLED devices, which may facilitate the development of more efficient and stable OLED devices with complex structures.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗