Search NASA⌕ Search

Engineering topics

Xie, Qiang

Publications and source records attributed to Xie, Qiang.

Ethylene Carbonate–Free Electrolytes for Stable, Safer High–Nickel Lithium–Ion Batteries

Ethylene carbonate (EC) is an important component in state-of-the-art electrolytes for lithium-ion batteries (LIBs). However, EC is highly susceptible to oxidation on the surface of high-nickel layered oxide cathodes, making it undesirable for next-generation high-energy-density LIBs. In this study, a simple, yet effective, EC-free electrolyte (20F1.5M-1TDI) is presented by adding 20 wt% fluoroethylene carbonate (FEC) and 1 wt% lithium 4,5-dicyano-2-(trifluoromethyl)imidazole (LiTDI) into 1.5 M LiPF 6 in an ethyl methyl carbonate (EMC) electrolyte. The 20F1.5M-1TDI electrolyte is found to efficiently passivate the graphite anode and stabilize high-nickel cathodes by a synergistic decomposition of FEC and LiTDI. The LiNi 0.9 Mn 0.05 Al 0.05 O 2 (NMA90)/graphite full cell with the 20F1.5M-1TDI electrolyte, therefore, exhibits an enhanced cycling stability and a suppressed voltage hysteresis growth compared to that with an EC-containing baseline electrolyte (1 M LiPF 6 in EC:EMC, 3:7 in weight, with 2 wt% vinyl carbonate). Advanced analytical tools, such as time-of-flight secondary ion mass spectrometry and X-ray photoelectron spectroscopy, are employed to understand the underlying working mechanism of the EC-free electrolyte. Furthermore, the present study clearly showcases the great potential of EC-free electrolytes as a straightforward, practical approach for LIBs with high-nickel cathodes.

electrode/electrolyte interface↗

A Cobalt– and Manganese–Free High–Nickel Layered Oxide Cathode for Long–Life, Safer Lithium–Ion Batteries

High-nickel LiNi 1–x–y Mn x Co y O 2 and LiNi 1–x–y Co x Al y O 2 cathodes are receiving growing attention due to the burgeoning demands on high-energy-density lithium-ion batteries. The presence of both cobalt and manganese in them, however, triggers multiple issues, including high cost, high toxicity, rapid surface deterioration, and severe transition-metal dissolution. Herein, a Co- and Mn-free ultrahigh-nickel LiNi 0.93 Al 0.05 Ti 0.01 Mg 0.01 O 2 (NATM) cathode that exhibits 82% capacity retention over 800 deep cycles in full cells, outperforming two representative high-Ni cathodes LiNi 0.94 Co 0.06 O 2 (NC, 52%) and LiNi 0.90 Mn 0.05 Co 0.05 O 2 (NMC, 60%) is presented. It is demonstrated that a titanium-enriched surface along with aluminum and magnesium as the stabilizing ions in NATM not only ameliorates unwanted side reactions with the electrolyte and structural disintegrity, but also mitigates transition-metal dissolution and active lithium loss on the graphite anode. As a result, the graphite anode paired with NATM displays an ultrathin (≈8 nm), monolayer anode-electrolyte interphase architecture after extensive cycling. Furthermore, NATM displays considerably enhanced thermal stability with an elevated exothermic temperature (213 °C for NATM vs 180 and 190 °C for NC and NMC, respectively) and remarkably reduced heat release. This work sheds light on rational compositional design to adopt ultrahigh-Ni cathodes in lithium-based batteries with low cost, long service life, and improved thermal stability.

25 ENERGY STORAGE↗

Long-life LiNi 0.5 Mn 1.5 O 4 /graphite lithium-ion cells with an artificial graphite-electrolyte interface

The high operating voltage of a spinel LiNi 0.5 Mn 1.5 O 4 (LNMO) cathode leads to electrolyte decomposition and accelerated deterioration of the electrode/electrolyte interface in lithium-ion cells. Aggressive side reactions prevent long-term cycling and hinder its practical application. Advanced characterization shows that the high-voltage operation makes the graphite anode react with the electrolyte, particularly with the lithium salt in the electrolyte, resulting in massive active lithium inventory loss and capacity fade. The side reactions at the graphite are identified as the main culprit for the LNMO/graphite full cell decay. Here, we demonstrate that an artificial solid-electrolyte interface layer consisting of an ultra-thin Al 2 O 3 film, generated via atomic layer deposition (ALD) at the graphite surface, can successfully isolate the graphite from the electrolyte and inhibit the undesired reactions. Consequently, the capacity and cycling stability of the LNMO/graphite cell are drastically improved. After 300 cycles, the capacity retention of LNMO/graphite cell increases from 57.7% to 98.6% with the ALD-coated graphite. Furthermore, our findings provide valuable insights into the LNMO/graphite cell degradation and suggest a simple and robust, yet highly effective, approach for the practical viability of high-voltage lithium-ion batteries.

25 ENERGY STORAGE↗

Unveiling the Stabilities of Nickel–Based Layered Oxide Cathodes at an Identical Degree of Delithiation in Lithium–Based Batteries

Bulk, surface, and interfacial instabilities that impact the cycle and thermal performances are the major challenges with high-energy-density LiNi 1–x–y Mn x Co y O 2 (NMC) cathodes with high nickel contents. It is generally believed that the instabilities and performance losses become exponentially aggravated as the nickel content increases. Disparate from this prevailing belief, it is herein demonstrated that NMC cathodes with higher Ni contents may imply better overall stability than “lower-Ni” cathodes under an identical degree of delithiation (charging) conditions. With two representative cathodes, LiNi 0.8 Mn 0.1 Co 0.1 O 2 and LiNiO 2 , a systematic investigation into their stabilities with control of the degree of delithiation is presented. Electrochemical tests indicate that LiNiO 2 displays better cyclability than LiNi 0.8 Mn 0.1 Co 0.1 O 2 at the same delithiation state. Comprehensive structural and interphase investigations unveil that the inferior cyclability of LiNi 0.8 Mn 0.1 Co 0.1 O 2 predominantly results from aggravated parasitic reactions, and the interphase stability may be more critical than lattice stability in dictating cyclability. Also, LiNiO 2 delivers similar or better thermal behavior than LiNi 0.8 Mn 0.1 Co 0.1 O 2 . Finally, the findings demonstrate a strong correlation of the stability of NMC cathodes to the degree of delithiation state rather than the Ni content itself, highlighting the importance of reassessing the true implications of Ni content and structural and interphasial tuning on the stabilities of NMC cathodes.

25 ENERGY STORAGE↗

Zinc-Doped High-Nickel, Low-Cobalt Layered Oxide Cathodes for High-Energy-Density Lithium-Ion Batteries

High-Ni layered oxides with Ni contents greater than 90% are promising cathode candidates for high-energy-density Li-ion batteries. However, drastic electrode-electrolyte reactions and mechanical degradation issues limit their cycle life and practical viability. We demonstrate here that LiNi 0.94 Co 0.04 Zn 0.02 O 1.99 (NCZ), obtained by incorporating 2 mol% Zn 2+ into an ultrahigh-Ni baseline cathode material LiNi 0.94 Co 0.06 O 2 (NC), delivers superior cell performance. NCZ retains 74% of the initial capacity after 500 cycles in full cell assembled with graphite anode, outperforming NC (62% retention). NCZ also possesses a higher average discharge voltage relative to NC with an outstanding average voltage retention of over 99% after 130 cycles in half cells. Bulk structural investigations unveil that Zn doping promotes a smoother phase transition, suppresses anisotropic lattice distortion, and maintains the mechanical integrity of cathode particles. Furthermore, NCZ shows an enhanced interphase stability after long-term cycling, in contrast to the seriously degraded surface chemistry in NC. Finally, this work provides a practically viable approach for designing higher-energy-density high-Ni layered oxide cathodes for lithium-ion batteries.

25 ENERGY STORAGE↗

Long-Term Cyclability of NCM-811 at High Voltages in Lithium-Ion Batteries: an In-Depth Diagnostic Study

High-nickel layered oxides, such as LiNi 0.8 Co 0.1 Mn 0.1 O 2 (NCM-811), offer higher energy density than their low-nickel counterparts at a given voltage and are gaining major traction in automotive lithium-ion batteries for electric vehicles. Besides high-Ni content, higher charging voltages above 4.3 V vs Li + /Li boost the energy and represent another focus in battery development. Here, we investigate the long-term cyclability of NCM-811 in graphite pouch cells over 1000 deep cycles between 2.5–4.2, 2.5–4.4, and 2.5–4.5 V through a suite of sensitive characterization techniques. The NCM-811 full cells show severely deteriorated cyclability with higher charging voltages, from 78% at 4.2 V to 52 and 32% at 4.4 and 4.5 V, respectively. At 4.2 V, minor parasitic electrolyte oxidation as well as cathode Li/Ni mixing and cracking are revealed after cycling, while transition-metal dissolution and surface reconstruction into rock-salt NiO are virtually undetectable. At 4.4 and 4.5 V, transition-metal dissolution and crossover to the anode become much more pronounced and a primary contributor to the capacity fade, while significant surface NiO formation causes substantial voltage polarization, which is less noticeable at 4.2 V. Meanwhile, more severe electrolyte oxidation, Li/Ni mixing, and particle pulverization exacerbate the voltage and capacity fade. Finally, these results outline distinct challenges for stable high-Ni layered oxide cathodes in high-voltage Li-ion batteries.

25 ENERGY STORAGE↗

Long-Life, Ultrahigh-Nickel Cathodes with Excellent Air Storage Stability for High-Energy Density Lithium-Based Batteries

With increased energy density and cost advantage, ultrahigh-nickel layered oxides (LiNi x M 1-x O 2 , x = 0.9 - 1.0) are becoming front-runner as cathodes for next-generation lithium-based batteries, yet their commercialization is blocked both by severe capacity fade and exponentially aggravated air degradation. Thus, it is imperative to find effective solutions to address these issues simultaneously. Here, a significant enhancement in both the cycling and air storage stability of the ultrahigh-Ni cathode LiNi 0.94 Co 0.06 O 2 is achieved via a distinctive phosphoric acid treatment strategy. The modified cathode displays remarkably improved capacity retention (from 36 % to 80 % after 1,000 cycles) and rate capability (from 0 to 105 mA h g -1 at 30C rate) in pouch cells. Impressively, the modified cathode, after air storage for 450 days, maintains the morphology and 92% of the initial capacity of the fresh sample with excellent cyclability. Comprehensive interphase and structural analyses reveal that the enhanced electrochemical performance is due to a highly stabilized electrode/electrolyte interphase that suppresses electrode corrosion and lattice reconstruction. The excellent air stability results from an adsorption-buffering effect enabled by phosphoric acid to air attack. Finally, the study demonstrates an engineering pathway to improve the cycling and air stability, facilitating the practical viability of high-capacity, affordable, ultrahigh-Ni cathodes in lithium-based batteries.

25 ENERGY STORAGE↗

Insights into Boron-Based Polyanion-Tuned High-Nickel Cathodes for High-Energy-Density Lithium-Ion Batteries

Ultrahigh-Ni layered oxide cathodes (Ni content > 90%) are at the forefront for potentially enabling higher-energy density lithium-ion batteries. Unfortunately, they suffer from rapid capacity fade, poor thermal stability, and increased air sensitivity. Introduction of boron-based polyanion into layered cathodes has been found to be effective in stabilizing high-Ni cathodes, but the mechanism behind it is not yet fully understood. To develop a better understanding, we present here an extensive characterization of the ultrahigh-Ni cathode LiNi 0.94 Co 0.06 O 2 (NC) and B 2 O 3 -LiNi 0.94 Co 0.06 O 2 (B-NC). The B-NC delivers a capacity of 223 mA h g -1 with 80% capacity retention after 400 cycles in full cells with graphite anodes, superior to 61% retention for NC. In-depth interphase investigations reveal that the improved cyclability is attributed to the development of a well-passivated boron/phosphorus-rich cathode-electrolyte interphase in B-NC. Moreover, B-NC demonstrates a considerably enhanced air-exposure and thermal stability. A 30-day air-stored B-NC delivers a discharge capacity of 125 mA h g -1 at 10C rate, in sharp contrast to 65 mA h g -1 for the stored NC. Finally, this work advances the understanding of the effect boron-based polyanion insertion into layered oxides has on battery performance and offers a viable strategy for developing practically viable ultra-high-Ni cathodes with high-energy density.

25 ENERGY STORAGE↗

Ethylene Carbonate–Free Electrolytes for High–Nickel Layered Oxide Cathodes in Lithium–Ion Batteries

Layered lithium nickel oxide (LiNiO 2 ) can provide very high energy density among intercalation cathode materials for lithium-ion batteries, but suffers from poor cycle life and thermal-abuse tolerance with large lithium utilization. In addition to stabilization of the active cathode material, a concurrent development of electrolyte systems of better compatibility is critical to overcome these limitations for practical applications. Here, with nonaqueous electrolytes based on exclusively aprotic acyclic carbonates free of ethylene carbonate (EC), superior electrochemical and thermal characteristics are obtained with an ultrahigh-nickel cathode (LiNi 0.94 Co 0.06 O 2 ), capable of reaching a 235 mA h g –1 specific capacity. Pouch-type graphite | LiNi 0.94 Co 0.06 O 2 cells in EC-free electrolytes withstand several hundred charge–discharge cycles with minor degradation at both ambient and elevated temperatures. In thermal-abuse tests, the cathode at full charge, while reacting aggressively with EC-based electrolytes below 200 °C, shows suppressed self-heating without EC. Through 3D chemical and structural analyses, the intriguing impact of EC is visualized in aggravating unwanted surface parasitic reactions and irreversible bulk structural degradation of the cathode at high voltages. Finally, these results provide important insights in designing high-energy electrodes for long-lasting and reliable lithium-ion batteries.

25 ENERGY STORAGE↗

Collapse of LiNi 1– x–y Co x Mn y O 2 Lattice at Deep Charge Irrespective of Nickel Content in Lithium-Ion Batteries

Volume variation and the associated mechanical fracture of electrode materials upon Li extraction/insertion are a main cause limiting lifetime performance of lithium-ion batteries. For LiNi 1-x-y Co x Mn y O 2 (NCM) cathodes, abrupt anisotropic collapse of the layered lattice structure at deep charge is generally considered characteristic to high Ni content and can be effectively suppressed by elemental substitution. Herein, we demonstrate the lattice collapse is a universal phenomenon almost entirely dependent on Li utilization, and not Ni content, of NCM cathodes upon delithiation. With Li removal nearing 80 mol%, very similar c-axis lattice shrinkage of around 5% occurs concurrently for NCMs synthesized in-house regardless of nickel content (90, 70, 50, or 33 mol%); meanwhile, the a-axis lattice contracts for high-Ni NCM, but it expands for low-Ni NCM. We further reveal Co-Mn co-substitution in NCM barely, if at all, affects several key structural aspects governing the lattice distortion upon delithiation. Finally, our results highlight the importance of evaluating true implications of compositional tuning on high-Ni layered oxide cathode materials to maximize their charge-storage capacities for next-generation high-energy Li-ion batteries.

25 ENERGY STORAGE↗

A Mg-Doped High-Nickel Layered Oxide Cathode Enabling Safer, High-Energy-Density Li-Ion Batteries

High-nickel layered oxide cathodes with a Ni content of > 90% show substantial potential for next-generation lithium-ion batteries (LIBs) due to their high capacity and lower cost. However, they are plagued by rapid capacity decay and poor thermal stability, which hamper their practical viability. Here we present Li 0.98 Mg 0.02 Ni 0.94 Co 0.06 O 2 (NC-Mg) with 2% Mg doping, aiming to provide a strategic guideline for solving the issues. The Mg 2+ ions occupy the lithium layer and are pro-posed to act as pillar ions, which substantially enhances the structural reversibility and reduces the anisotropic lattice distortion upon cycling, thereby greatly improving the electrochemical and thermal stability of NC-Mg compared to the undoped LiNi 0.94 Co 0.06 O 2 (NC). Specifically, NC-Mg delivers 214 mA h g -1 with a capacity retention of 80.1% after 500 cycles in pouch-type full cells, much higher than the retention of NC (56.3%). A discharge capacity of 158 mA h g -1 at 10C rate demonstrates its remarkable rate capability. Additionally, the Mg doping significantly elevates the exothermic peak tem-perature of NC-Mg to 211 °C, in sharp contrast to 177 °C for NC, highlighting the improved thermal stability of NC-Mg. Collectively, the superior performance of NC-Mg demonstrates a feasible alternative strategy for developing safer, high-energy-density LIBs.

25 ENERGY STORAGE↗

Extending the limits of powder diffraction analysis: diffraction parameter space, occupancy defects, and atomic form factors

Although the determination of site occupancies is often a major goal in Rietveld refinement studies, the accurate refinement of site occupancies is exceptionally challenging due to the many correlations and systematic errors that have a hidden impact on the final refined occupancy parameters. Through the comparison of results independently obtained from neutron and synchrotron powder diffraction, improved approaches capable of detecting occupancy defects with an exceptional sensitivity of 0.1% (absolute) in the class of layered NMC Li-ion battery cathode materials have been developed. A new method of visualizing the diffraction parameter space associated with crystallographic site scattering power through the use of f* diagrams is described and this method is broadly applicable to ternary compounds. The f* diagrams allow the global minimum fit to be easily identified and also permit a robust determination of the number and type of occupancy defects within a structure. Through a comparison of neutron and X-ray diffraction results, a systematic error in the synchrotron results was identified using f* diagrams for a series of NMC compounds. Using neutron diffraction data as a reference, this error was shown to specifically result from problems associated with the neutral oxygen X-ray atomic form factor and could be eliminated by using the ionic O 2- form factor for this anion while retaining the neutral form factors for cationic species. The f* diagram method offers a new opportunity to experimentally assess the quality of atomic form factors through powder diffraction studies on chemically related multi-component compounds.

25 ENERGY STORAGE↗

Sensitization of cancer cells to radiation by selenadiazole derivatives by regulation of ROS-mediated DNA damage and ERK and AKT pathways

Highlights: • Selenadiazole derivatives could be used as an effective and low toxic sensitizer for radiotherapy. • Selenadiazole derivatives enhances radiation-induced growth inhibition on A375 cells through induction of G2/M arrest. • ROS-mediated signaling pathways play important roles in radiosensitization of selenadiazole derivatives. - Abstract: X-ray-based radiotherapy represents one of the most effective ways in treating human cancers. However, radioresistance and side effect remain as the most challenging issue. This study describes the design and application of novel selenadiazole derivatives as radiotherapy sensitizers to enhance X-ray-induced inhibitory effects on A375 human melanoma and Hela human cervical carcinoma cells. The results showed that, pretreatment of the cells with selenadiazole derivatives dramatically enhance X-ray-induced growth inhibition and colony formation. Flow cytometry analysis indicates that the sensitization by selenadiazole derivatives was mainly caused by induction of G2/M cell cycle arrest. Results of Western blotting demonstrated that the combined treatment-induced A375 cells growth inhibition was achieved by triggering reactive oxygen species-mediated DNA damage involving inactivation of AKT and MAPKs. Further investigation revealed that selenadiazole derivative in combination with X-ray could synergistically inhibit the activity of thioredoxin reductase-1 in A375 cells. Taken together, these results suggest that selenadiazole derivatives can act as novel radiosensitizer with potential application in combating human cancers.

60 APPLIED LIFE SCIENCES↗