The Effects of Water Vapor and Hydrogen on the High-Temperature Oxidation of Alloys

Essentially all alloys and coatings that are resistant to corrosion at high temperature require the formation of a protective (slowly-growing and adherent) oxide layer by a process known as selective oxidation. The fundamental understanding of this process has been developed over the years for exposure in pure oxygen or air. However, the atmospheres in most applications contain significant amounts of water vapor which can greatly modify the behavior of protective oxides. The development of oxy-fuel combustion systems in which fossil fuels are burned in a mixture of recirculated flue gas and oxygen, rather than in air, has caused renewed interest in the effects of water vapor and steam on alloy oxidation. The focus of this paper is on the ways the presence of water vapor can directly alter the selective oxidation process. The paper begins with a brief review of the fundamentals of selective oxidation followed by a description of recent experimental results regarding the effect of water vapor on the oxidation of a variety of chromia-forming alloys (Fe- and Ni-base) in the temperature range 600 to 700 °C. The atmospheres include air, air-H{sub 2}O, Ar-H{sub 2}O and Ar-H{sub 2}O-O{sub 2}. Then the behavior of alumina-forming alloys in H{sub 2}O-containing atmospheres is briefly described. As hydrogen is produced during oxidation of alloys in H{sub 2}O, it can be released back into the gas phase or injected into the metal (where it can diffuse through to the other side). Experiments in which hydrogen concentrations have been measured on both sides of thin specimens during oxidation by H{sub 2}O on only one side are described. Finally, it is attempted to catalogue the various experimental observations under a few general principles.

36 MATERIALS SCIENCE↗

Oxy-Combustion Environment Characterization: Fire- and Steam-Side Corrosion in Advanced Combustion

Oxy-fuel combustion is burning a fuel in oxygen rather than air. The low nitrogen flue gas that results is relatively easy to capture CO{sub 2} from for reuse or sequestration. Corrosion issues associated with the environment change (replacement of much of the N{sub 2} with CO{sub 2} and higher sulfur levels) from air- to oxy-firing were examined. Alloys studied included model Fe-Cr alloys and commercial ferritic steels, austenitic steels, and nickel base superalloys. The corrosion behavior is described in terms of corrosion rates, scale morphologies, and scale/ash interactions for the different environmental conditions. Additionally, the progress towards laboratory oxidation tests in advanced ultra-supercritical steam is updated.

20 FOSSIL-FUELED POWER PLANTS↗

GRH 12-01 Fireside Corrosion in Oxy-fuel Combustion Poster 0108

The goals are to: (1) Achieve 90% CO{sub 2} capture at no more than a 35% increase in levelized cost of electricity of post-combustion capture for new and existing conventional coal-fired power plants; (2) Provide high-temperature corrosion information to aid in materials development and selection for oxy-fuel combustion; and (3) Identify corrosion mechanism and behavior differences between air- and oxy-firing.

54 ENVIRONMENTAL SCIENCES↗

Fireside Corrosion in Oxy-fuel Combustion of Coal

Oxy-fuel combustion is burning a fuel in oxygen rather than air. The low nitrogen flue gas that results is relatively easy to capture CO{sub 2} from for reuse or sequestration. Corrosion issues associated with the environment change (replacement of much of the N{sub 2} with CO{sub 2} and higher sulfur levels) from air- to oxy-firing were examined. Alloys studied included model Fe-Cr alloys and commercial ferritic steels, austenitic steels, and nickel base superalloys. The corrosion behavior is described in terms of corrosion rates, scale morphologies, and scale/ash interactions for the different environmental conditions.

01 COAL, LIGNITE, AND PEAT↗

Fireside Corrosion in Oxy-Fuel Combustion of Coal

The goal is to develop technologies for pulverized coal boilers with >90% CO{sub 2} capture and sequestration and <35% increase in the cost of electricity. Air-fired power plant experience shows a corrosion loss max at 680-700 C. Low melting point alkali metal trisulfates, such as (K,Na){sub 3}Fe(SO{sub 4}){sub 3}, become thermally unstable above this temperature range. Some overall conclusions are: (1) CO{sub 2} + 30% H{sub 2}O more corrosive than Ar + 30% H{sub 2}O; (2) Excess O{sub 2} in H{sub 2}O can, in some cases, greatly increase oxidation; (3) Coal ash is generally innocuous without SO{sub 3}3 in gas phase; and (4) Long-term exposures are starting to establish differences between air-firing and oxy-firing conditions.

01 COAL, LIGNITE, AND PEAT↗

Materials Performance in USC Steam

Materials Performance in USC Steam: (1) pressure effects on steam oxidation - unique capability coming on-line; (2) hydrogen evolution - hydrogen permeability apparatus to determine where hydrogen goes during steam oxidation; and (3) NETL materials development - steam oxidation resource for NETL developed materials.

08 HYDROGEN↗