Thermoelectric Properties of Au- Containing Type-I Clathrates Ba8AuxGa16-3xGe30+2x

Type I clathrates, with compositions based on Ba8Ga16Ge30, are a class of promising thermoelectric materials due to their intrinsically low thermal conductivity. It has been demonstrated previously that the thermoelectric performance can be improved by transition metal substitution of the framework atoms. In this study, the effects of Au substitution for Ga/Ge on thermal and electrical transport properties of type I clathrate compounds have been investigated. Polycrystalline samples with a large range of Au content have been synthesized using conventional solid state techniques with the actual compositions of resulting materials approximately following Zintl-Klemm rules. The charge carrier type changes from electrons (n) to holes (p) as the Au content increases. The Seebeck coefficient (S) and power factor (S2/ where is the electrical resistivity) were improved by Au substitution and the resulting overall thermoelectric properties were enhanced by Au substitution with a thermoelectric figure of merit ZT ~ 0.63 at temperature T = 740 K for the composition Ba8Au5.47Ge39.96. The results presented herein show that Au-containing type I clathrates are promising p-type thermoelectric materials for high temperature applications.

Clathrates↗

The effect of structural vacancies on the thermoelectric properties of (Cu₂Te){sub 1–x}(Ga₂Te₃) x

We have studied the effects of structural vacancies on the thermoelectric properties of the ternary compounds (Cu₂Te) 1–x (Ga₂Te₃) x (x=0.5, 0.55, 0.571, 0.6, 0.625, 0.667 and 0.75), which are solid solutions found in the pseudo-binary phase diagram for Cu₂Te and Ga₂Te₃, and possesses tunable structural vacancy concentrations. This materials system is not suitable due to the cost and scarcity of the constituent elements, but the vacancy behavior is well understood and will provide a valuable test case for other systems more suitable from the standpoint of cost and abundance of raw materials, which also possesses these vacancy features, but whose structural characterization is lacking at this stage. We find that the nominally defect free phase CuGaTe₂ possess the highest ZT (ZT=S²T/ρκ, where S is the Seebeck coefficient and ρ is the electrical resistivity κ is the thermal conductivity and T is the absolute temperature) which approaches 1 at 840 K and seems to continuously increase above this temperature. This result is due to the unexpectedly low thermal conductivity found for this material at high temperature. The low thermal conductivity was caused by strong Umklapp (thermally resistive scattering processes involving three phonons) phonon scattering. We find that due to the coincidentally strong scattering of carriers by the structural defects that higher concentrations of these features lead to poor electrical transport properties and decreased ZT. - Graphical abstract: Thermal conductivity and zT as a function of temperature for a series of compounds of the type (Cu₂Te) 1–x (Ga₂Te₃)x (x=0.5, 0.55, 0.571, 0.6, 0.625, 0.667 and 0.75). Highlights: • All the samples show p-type semiconducting behavior in the temperature dependence of the Seebeck and Hall coefficients. • The increased carrier concentration and the introduction of vacancies diminish the carrier mobility and power factor. • The low temperature k decreases significantly as the Ga₂Te₃ content increases due to increasing point defects. • The highest ZT ~ 1.0 at 840 K among the samples in this study was found in CuGaTe₂, which contains no vacancies.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Thermal to Electrical Energy Conversion of Skutterudite-Based Thermoelectric Modules

The performance of thermoelectric (TE) materials has improved tremendously over the past decade. The intrinsic thermal and electrical properties of state-of-the-art TE materials demonstrate that the potential for widespread practical TE applications is very large and includes TE generators (TEGs) for automotive waste heat recovery. TE materials for automotive TEG applications must have good intrinsic performance, be thermomechanically compatible, and be chemically stable in the 400 K to 850 K temperature range. Both n-type and p-type varieties must be available at low cost, easily fabricated, and durable. They must also form robust junctions and develop good interfaces with other materials to permit efficient flows of electrical and thermal energy. Among the TE materials of interest for automotive waste heat recovery systems are the skutterudite compounds, which are the antimony-based transition-metal compounds RTE4Sb12, where R can be an alkali metal (e.g., Na, K), alkaline earth (e.g., Ba), or rare earth (e.g., La, Ce, Yb), and TE can be a transition metal (e.g., Co, Fe). We synthesized a considerable quantity of n-type and p-type skutterudites, fabricated TE modules, incorporated these modules into a prototype TEG, and tested the TEG on a production General Motors (GM) vehicle. We discuss our progress on skutterudite TE module fabrication and present module performance data for electrical power output under simulated operating conditions for automotive waste heat recovery systems. We also present preliminary durability results on our skutterudite modules.

module↗

Improved Thermoelectric Performance of p-type Skutterudite YbxFe4-yPtySb12 (0.8 x 1, y = 1 and 0.5)

Thermoelectric performance of p-type skutterudites currently lags that of the corresponding n-type materials and improvement of this important class of materials have become the focus of considerable research effort world-wide. Recent calculations find promising band structural features in p-type skutterudite materials of the type AeFe3NiSb12 ( Ae = Ca, Sr, or Ba) which could potentially lead to excellent thermoelectric properties. Recent work on the Yb- filled analog of the these formulations (YbFe3NiSb12) however finds that the onset of intrinsic conduction at lower than expected temperatures deteriorates the performance above 500 K leading to poor performance in the temperature range of interest for automotive waste heat recovery applications. We therefore seek a way to increase the band gap in order to find a way to minimize the deleterious effects of intrinsic conduction. Here we present ab initio band structure calculations and the synthesis and thermoelectric properties of YbxFe4-yPtySb12 (0.8 x 1, y = 1 and 0.5). Ab initio calculations find that the band gap increases for YbFe3PtSb12 as compared to the Ni-containing analog, though no such increase in the band gap energy was found for as compared to YbFe3.5Ni0.5Sb12. The y = 1 samples shows a characteristic transition to intrinsic conduction with a decrease in the Seebeck coefficient at temperatures above 700 K. The increased carrier concentration in y = 0.5 virtually eliminates any evidence of intrinsic conduction and the Seebeck coefficients for these samples increase monotonically up to 750 K, resulting in power factors approaching 27 W/cm K2 at 750 K. These power factors combined with low thermal conductivity result in a ZT = 0.9 at 750 K for Yb0.95Fe3.5Pt0.5Sb12.

skutterudite↗

Thermoelectric Properties of P-type Skutterudites YbxFe3.5Ni0.5Sb12 (0.8 x 1)

P-type skutterudites, with nominal compositions YbxFe3.5Ni0.5Sb12 (0.8 x 1), have been synthesized by induction melting with subsequent annealing, and their thermoelectric properties evaluated from 3.5 K to 745 K to assess their suitability for thermoelectric based waste heat recovery applications. We report results for the synthesis and measurements of Seebeck coefficient (S), electrical resistivity ( ), thermal conductivity ( ), Hall coefficient (RH), and effective mass (m*/m0) of YbxFe3.5Ni0.5Sb12 (0.8 x 1). Powder x-ray diffraction and electron probe microanalysis (EPMA) show that this system has a narrow filling fraction range of x ~ 0.84 to 0.86 for Yb in the crystallographic voids. All samples show positive RH for the entire temperature range studied with carrier concentrations ranging from 9.6 1020 to 2.8 1021 cm-3 at room temperature. Relatively high values of S result in high power factors up to 17 Wcm-1K-2 at room temperature. However, large values of and a sharp reduction in the S at high temperature due to bipolar conduction prevent the attainment of high thermoelectric figure of merit.

36 MATERIALS SCIENCE↗