Search NASA⌕ Search

Engineering topics

Yeddala, Munaiah

Publications and source records attributed to Yeddala, Munaiah.

Electrolyte Design for NMC811||SiO x -Gr Lithium-Ion Batteries with Excellent Low-Temperature and High-Rate Performance

The use of high-nickel NMC811 cathode and SiO x -Gr anode can greatly improve the overall energy densities of lithium-ion batteries. However, the unfavorable solid electrolyte interphase (SEI) layer generated from the decomposition of EC-based electrolytes lead to the poor cycling stability of NMC811||SiO x -Gr cells. Here we report an electrolyte design of 1.5 M LiPF 6 dissolved in FEC/MA/BN 2:2:6 by volume, which can form thin, robust, and homogeneous SEI layer to greatly improve the charge transfer at the electrode-electrolyte interface. Importantly, the designed electrolyte shows an outstanding low temperature performance that it can deliver a capacity of 123.3 mAh g –1 after 50 cycles at −20 °C with a current density of 0.5 C, overwhelming the standard EC-based electrolyte (1.2 M LiPF 6 EC/EMC 3:7 by volume) with a capacity of 35.7 mAh g –1 . The electrolyte also has a superior rate performance that it achieves a capacity of 122.5 mAh g −1 at a high current density of 10 C. Moreover, the LTE electrolyte holds the great potential of extreme fast-charging ability because of the large part of CC contribution in the CCCV charging model at high charging current densities.

Electrochemistry↗

Speciation of Transition Metal Dissolution in Electrolyte from Common Cathode Materials

Abstract Significant capacity loss has been observed across extended cycling of lithium‐ion batteries cycled to high potential. One of the sources of capacity fade is transition metal dissolution from the cathode active material, ion migration through the electrolyte, and deposition on the solid‐electrolyte interphase on the anode. While much research has been conducted on the oxidation state of the transition metal in the cathode active material or deposited on the anode, there have been limited investigations of the oxidation state of the transition metal ions dissolved in the electrolyte. In this work, X‐ray absorption spectroscopy has been performed on electrolytes extracted from cells built with four different cathode active materials (LiMn 2 O 4 (LMO), LiNi 0.5 Mn 1.5 O 4 (LNMO), LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811), and (x Li 2 MnO 3 *(1‐x) LiNi a Mn b Co c O 2 , with a+b+ c =1) (LMRNMC)) that were cycled at either high or standard potentials to determine the oxidation state of Mn and Ni in solution. Inductively coupled plasma‐mass spectrometry has been performed on the anodes from these cells to determine the concentration of deposited transition metal ions. While transition metal ions were found dissolved in all electrolytes, the oxidation state(s) of Mn and Ni were determined to be dependent on the cathode material and independent of cycling potential.

Rynearson, Leah↗

Speciation of Transition Metal Dissolution in Electrolyte from Common Cathode Materials

Significant capacity loss has been observed across extended cycling of lithium-ion batteries cycled to high potential. One of the sources of capacity fade is transition metal dissolution from the cathode active material, ion migration through the electrolyte, and deposition on the solid-electrolyte interphase on the anode. While much research has been conducted on the oxidation state of the transition metal in the cathode active material or deposited on the anode, there have been limited investigations of the oxidation state of the transition metal ions dissolved in the electrolyte. Here, in this work, X-ray absorption spectroscopy has been performed on electrolytes extracted from cells built with four different cathode active materials (LiMn 2 O 4 (LMO), LiNi 0.5 Mn 1.5 O 4 (LNMO), LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811), and (x Li 2 MnO 3 *(1-x) LiNi a Mn b Co c O 2 , with a+b+c=1) (LMRNMC)) that were cycled at either high or standard potentials to determine the oxidation state of Mn and Ni in solution. Inductively coupled plasma-mass spectrometry has been performed on the anodes from these cells to determine the concentration of deposited transition metal ions. While transition metal ions were found dissolved in all electrolytes, the oxidation state(s) of Mn and Ni were determined to be dependent on the cathode material and independent of cycling potential.

25 ENERGY STORAGE↗

Improved Performance of Silicon-Containing Anodes with Organic Solvent-Solubilized Lithium Nitrate

Three different organic solvents (dimethylacetamide (DMAc), dimethylformamide (DMF), and dimethyl sulfoxide (DMSO)) were used to improve the solubility of LiNO 3 in a standard carbonate-based electrolyte with lithium difluoro(oxalato)borate (LiDFOB) as the salt. Together, the LiDFOB and organic-solvent solubilized LiNO 3 preferentially reduce on the surface of silicon-containing anodes to create an SEI rich in oxalates, nitrate decomposition species, and B-F species. The improved stability of the SEI throughout the first 100 cycles results in silicon and silicon/graphite composite anodes with better capacity retention than observed with standard electrolytes or fluoroethylene carbonate (FEC) containing electrolytes. This study demonstrates the feasibility of the use of non-traditional electrolyte solvents in the improvement and optimization of lithium ion-battery electrolytes.

25 ENERGY STORAGE↗