Search NASA⌕ Search

Engineering topics

Yelton, William Graham

Publications and source records attributed to Yelton, William Graham.

At least 19 records

Direct observation of electrothermal instability structures in the skin layer of an intensely Ohmically heated conductor

Magnetically driven implosions (MDIs) on the Z Facility assemble high-energy-density plasmas for radiation effects and ICF experiments. MDIs are hampered by the Magneto-Rayleigh-Taylor (MRT) instability, which can grow to large amplitude from a small seed perturbation, limiting achievable stagnation pressures and temperatures. The metallic liners used in Magnetized Liner Inertial Fusion (MagLIF) experiments include astonishingly small (-10 nm RMS) initial surface roughness perturbations; nevertheless, unexpectedly large MRT amplitudes are observed in experiments. An electrothermal instability (ETI) may provide a perturbation which exceeds the initial surface roughness. For a condensed metal resistivity increases with temperature. Locations of higher resistivity undergo increased Ohmic heating, resulting in locally higher temperature, and thus still higher resistivity. Such unstable temperature (and pressure) growth produces density perturbations when the locally overheated metal changes phase, providing the seed perturbation for MRT growth. ETI seeding of MRT on thick conductors carrying current in a skin layer has thus far only been inferred by evaluating MRT amplitude late in the experiment. A direct observation of ETI is vital to ensure our simulation tools are accurately representing the seed of the deleterious MRT instability. In this LDRD project, ETI growth was directly observed on the surface of 1.0-mm-diameter solid Al rods which were pulsed with 1 MA of current in 100 ns. Fine structures resulting from ETI-driven temperature variations were observed directly through high resolution gated optical imaging. Data from two Aluminum alloys (6061 and 5N) and a variety fabrication techniques (conventional machining, single-point diamond turned, electropolished) enable evaluation of which imperfections provide a seed for ETI growth and subsequent plasma initiation. Data is relevant to the early stages of MagLIF liner implosions, when the ETI seed of MRT may be initiated, and provides a fundamentally new dataset with which to test our state-of-the-art simulation tools.

42 ENGINEERING↗

Nuclear radiation-warning detector that measures impedance

This invention is a nuclear radiation-warning detector that measures impedance of silver-silver halide on an interdigitated electrode to detect light or radiation comprised of alpha particles, beta particles, gamma rays, X rays, and/or neutrons. The detector is comprised of an interdigitated electrode covered by a layer of silver halide. After exposure to alpha particles, beta particles, X rays, gamma rays, neutron radiation, or light, the silver halide is reduced to silver in the presence of a reducing solution. The change from the high electrical resistance (impedance) of silver halide to the low resistance of silver provides the radiation warning that detected radiation levels exceed a predetermined radiation dose threshold.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Understanding and Predicting Metallic Whisker Growth and its Effects on Reliability (LDRD Final Report)

Tin (Sn) whiskers are conductive Sn filaments that grow from Sn-plated surfaces, such as surface finishes on electronic packages. The phenomenon of Sn whiskering has become a concern in recent years due to requirements for lead (Pb)-free soldering and surface finishes in commercial electronics. Pure Sn finishes are more prone to whisker growth than their Sn-Pb counterparts and high profile failures due to whisker formation (causing short circuits) in space applications have been documented. At Sandia, Sn whiskers are of interest due to increased use of Pb-free commercial off-the-shelf (COTS) parts and possible future requirements for Pb-free solders and surface finishes in high-reliability microelectronics. Lead-free solders and surface finishes are currently being used or considered for several Sandia applications. Despite the long history of Sn whisker research and the recently renewed interest in this topic, a comprehensive understanding of whisker growth remains elusive. This report describes recent research on characterization of Sn whiskers with the aim of understanding the underlying whisker growth mechanism(s). The report is divided into four sections and an Appendix. In Section 1, the Sn plating process is summarized. Specifically, the Sn plating parameters that were successful in producing samples with whiskers will be reviewed. In Section 2, the scanning electron microscopy (SEM) of Sn whiskers and time-lapse SEM studies of whisker growth will be discussed. This discussion includes the characterization of straight as well as kinked whiskers. In Section 3, a detailed discussion is given of SEM/EBSD (electron backscatter diffraction) techniques developed to determine the crystallography of Sn whiskers. In Section 4, these SEM/EBSD methods are employed to determine the crystallography of Sn whiskers, with a statistically significant number of whiskers analyzed. This is the largest study of Sn whisker crystallography ever reported. This section includes a review of previous literature on Sn whisker crystallography. The overall texture of the Sn films was also analyzed by EBSD. Finally, a short Appendix is included at the end of this report, in which the X-Ray diffraction (XRD) results are discussed and compared to the EBSD analyses of the overall textures of the Sn films. Sections 2, 3, and 4 have been or will be submitted as stand-alone papers in peer-reviewed technical journals. A bibliography of recent Sandia Sn whisker publications and presentations is included at the end of the report.

36 MATERIALS SCIENCE↗