Effect of supersonic spraying impact velocity on opto-electric properties of transparent conducting flexible films consisting of silver nanowire, ITO, and polyimide multilayers

We demonstrate the use of supersonic spraying for the deposition of silver nanowires (AgNWs) on a flexible polyimide (PI) substrate for the formation of transparent and conducting films (TCF) as an alternative to nonflexible ITO (indium tin oxide). The self-fused intersections of the NWs resulted in films with a low sheet resistance (Rs = 31 ..omega../sq) and fairly high transmittance (Tr = 92%) on a glass substrate. The effect of the impact speed of the supersonically sprayed AgNWs on the opto-electric properties of the flexible TCF was evaluated by varying the spray coating conditions. The fabricated films were characterized by X-ray diffraction analysis, atomic force microscopy, ultraviolet-visible spectroscopy, and scanning electron microscopy. Finally, cyclic bending tests were performed on the PI/AgNW films as well as PI/ZnO/indium tin oxide/AgNW films, and the changes in their electrical properties with bending were compared.

36 MATERIALS SCIENCE↗

Supersonically Spray-Coated Colloidal Quantum Dot Ink Solar Cells

Controlling the thickness of quantum dot (QD) films is difficult using existing film formation techniques, which employ pre-ligand-exchanged PbS QD inks, because of several issues: 1) poor colloidal stability, 2) use of high-boiling-point solvents for QD dispersion, and 3) limitations associated with one-step deposition. Here in this paper, we suggest a new protocol for QD film deposition using electrical double-layered PbS QD inks, prepared by solution-phase ligand exchange using methyl ammonium lead iodide (MAPbI 3 ). The films are deposited by the supersonic spraying technique, which facilitates the rapid evaporation of the solvent and the subsequent deposition of the PbS QD ink without requiring a post-deposition annealing treatment for solvent removal. The film thickness could be readily controlled by varying the number of spraying sweeps made across the substrate. This spray deposition process yields high-quality n-type QD films quickly (within 1 min) while minimizing the amount of the PbS QD ink used to less than 5 mg for one device (300-nm-thick absorbing layer, 2.5 x 2.5 cm 2 ). Further, the formation of an additional p-layer by treatment with mercaptopropionic acid allows for facile hole extraction from the QD films, resulting in a power conversion efficiency of 3.7% under 1.5 AM illumination.

14 SOLAR ENERGY↗