Search NASA⌕ Search

Engineering topics

Young, Travis R.

Publications and source records attributed to Young, Travis R..

Stabilization of ferroelectric phase of Hf 0.6 Zr 0.4 O 2 on NbN and Nb [slides]

This work demonstrated both NbN and Nb make good electrodes for stabilizing orthorhombic phase of Hf 0.6 Zr 0.4 O 2 ferroelectric films. Wake up are < 100 cycles. P r can be as high as 30 µC/cm 2 - respectively 14 and 18 µC/cm 2 here. Further, capacitance suggests an orthorhombic phase can be stabilized. Addition of a linear dielectric under modest thickness can tune the P r and reduce leakage.

36 MATERIALS SCIENCE↗

Al 0.68 Sc 0.32 N Lamb wave resonators with electromechanical coupling coefficients near 10.28%

Aluminum scandium nitride (Al 1-x Sc x N/AlScN) (x = 0.32) Lamb wave resonators (LWR) have been fabricated and tested to demonstrate electromechanical coupling coefficients (k t 2 ) in excess of 10%. The resonators exhibited an average k t 2 and unloaded quality factor (Q u ) of 10.28% and 711, respectively, when calculated from the measured data. Applying the Butterworth Van-Dyke (BVD) model to the measured data enabled the extraction of the resonator's lumped element parameters to calculate the motional quality factor (Q m ), which neglects the contributions of the electrical traces. For the best measured resonator response, results from the BVD model showed a Q m of 1184 and a resulting figure-of-merit (FOM = K 2 ·Q m ) of 100. Comparing the response of similar AlScN and AlN resonators shows that the AlScN LWR has a significantly lower motional resistance (R m ), suggesting that AlScN has a strong potential for use in piezoelectric microelectromechanical oscillators.

42 ENGINEERING↗

ScAlN etch mask for highly selective silicon etching

Here, this work reports the utilization of a recently developed film, ScAlN, as a silicon etch mask offering significant improvements in high etch selectivity to silicon. Utilization of ScAlN as a fluorine chemistry based deep reactive ion etch mask demonstrated etch selectivity at 23 550:1, four times better than AlN, 11 times better than Al 2 O 3 , and 148 times better than silicon dioxide with significantly less resputtering at high bias voltage than either Al 2 O 3 or AlN. Ellipsometry film thickness measurements show less than 0.3 nm/min mask erosion rates for ScAlN. Micromasking of resputtered Al for Al 2 O 3 , AlN, and ScAlN etch masks is also reported here, utilizing cross-sectional scanning electron microscope and confocal microscope roughness measurements. With lower etch bias, the reduced etch rate can be optimized to achieve a trench bottom surface roughness that is comparable to SiO 2 etch masks. Etch mask selectivity enabled by ScAlN is likely to make significant improvements in microelectromechanical systems, wafer level packaging, and plasma dicing of silicon.

36 MATERIALS SCIENCE↗