Search NASA⌕ Search

Engineering topics

Zhou, Feng

Publications and source records attributed to Zhou, Feng.

57 records · Page 4

Preliminary Design of a Bunching System for the CLIC Polarized Electron Source

Major parameters of the CLIC and ILC electron sources are given in Table I. It is shown that the CLIC source needs to provide 312 15-ps-long 2-GHz microbunches. There are two approaches to achieve the time structure [2]: one is to develop a 2-GHz optical pulse train, and the other to develop a 156-ns-long CW optical pulse and use an RF bunching system to generate 312 2-GHz microbunches. The former scheme may ease the RF bunching system but still need it to bunch 100-ps of microbunch down to 15-ps level. Otherwise, a huge amount of energy spread is accumulated when the beam is accelerated through downstream 2-GHz accelerator. In addition, in the former scheme, the space charge is high and surface charge is not yet proven in the parameter regime and 2-GHz mode locked laser is challenging. The latter scheme needs a high-efficiency bunching system to generate 312 15-ps microbunches with 2-GHz repetition rate but it has some notable advantages: a 156-ns CW laser technique is matured, and the charge limit behavior in the scheme is better characterized than that in the former case, as listed in the table. This note presents a design and modeling of the bunching system for the latter scheme to convert a 156-ns CW pulse to 312 15-ps long 2-GHz microbunches.

43 PARTICLE ACCELERATORS↗

Analysis of Phase Separation in Czochralski Grown Single Crystal Ilmenite

Ilmenite (FeTiOs) is a wide bandgap semiconductor with an energy gap of 2.58 eV. Ilmenite has properties suited for radiation tolerant applications, as well as a variety of other electronic applications. Single crystal ilmenite has been grown from the melt using the Czochralski method. Growth conditions have a profound effect on the microstructure of the samples. Here we present data from a variety of analytical techniques which indicate that some grown crystals exhibit distinct phase separation during growth. This phase separation is apparent for both post-growth annealed and unannealed samples. Under optical microscopy, there appear two distinct areas forming a matrix with an array of dots on order of 5 pm diameter. While appearing bright in the optical micrograph, atomic force microscope (AFM) shows the dots to be shallow pits on the surface. Magnetic force microscope (MFM) shows the dots to be magnetic. Phase identification via electron microprobe analysis (EMPA) indicates two major phases in the unannealed samples and four in the annealed samples, where the dots appear to be almost pure iron. This is consistent with micrographs taken with a scanning probe microscope used in the magnetic force mode. Samples that do not exhibit the phase separation have little or no discernible magnetic structure detectable by the MFM.

Wilkins, R.↗