Search NASA⌕ Search

Engineering topics

Zhuang, H. D.

Publications and source records attributed to Zhuang, H. D..

First results of Ne shattered pellet injection for mitigating plasma disruption with full metal wall in EAST tokamak

Disruption mitigation poses a significant and unresolved challenge for ITER and future fusion reactor devices. To mitigate the effect of plasma disruption, a Shattered Pellet Injection (SPI) system has been developed and the first rapid shutdown experiments have been successfully performed in the Experimental Advanced Superconducting Tokamak with full metal wall. The experiments confirmed the system’s capability to inject 5 mm diameter neon (Ne) pellets at velocities ranging from 100 to 400 m s −1 , with a maximum injected quantity of 13.2 Pa m 3 . Compared to unmitigated disruptions, the total radiation power was significantly higher with the respective use of SPI and Massive Gas Injection (MGI). Additionally, the radiation distribution and divertor heat flux were compared between SPI and MGI methods. The results demonstrated that SPI exhibited shorter cooling time, stronger core radiation and more uniform poloidal radiation distribution compared to MGI, indicating deeper deposition using SPI. Furthermore, during plasma shutdown, the electron temperature and peak heat flux near outer divertor strike points were reduced by 40% and 50% respectively, with SPI, in comparison to MGI. These findings serve as a valuable reference for implementing SPI technology as the baseline approach for disruption mitigation in ITER.

EAST↗

Reduction of hydrogen content in deuterium plasma with mixed graphite and tungsten divertors in EAST

Reduction of hydrogen content in deuterium-fueled fusion plasmas is important not only to avoid diluting reacting core deuterons but also so as to allow the optimization of hydrogen-minority-heating efficiency in those fusion devices which employ ion-cyclotron-radio-frequency heating systems. In EAST, the amount of hydrogen released from plasma-facing components has been shown to depend strongly on both their composition and their temperature. In this paper, as measured by thermal desorption spectroscopy, the hydrogen inventory in graphite – used in EAST as lower divertor material – has been determined to be >25 times larger than that of tungsten which comprises the upper divertor. This difference in hydrogen inventory is attributed mostly to the intrinsically porous nature of bulk graphite. Thus the main source of hydrogen release into EAST discharges was identified as the graphite tiles used in the lower divertor. The hydrogen content in EAST plasmas were clearly reduced by first employing a high-temperature vacuum baking of all graphite tiles and then renewing a 100–200 μm thick SiC coating before an EAST experimental run campaign. Subsequent active surface conditioning of all wall components with elemental silicon and then with elemental lithium were seem to again reduce the plasma hydrogen content significantly – with lithium proving to be more effective than silicon. Combining these several techniques, H/(H + D) levels as low as ~3% have been achieved in EAST discharges. Additionally, the effects of lithium thickness on H surface implantation and retention has been re-examined semi-quantitatively using data from a previous run campaign. These data suggest that relatively thick Li films coated on the first wall can effectively isolate the rich source of hydrogen stored in the porous bulk of the underlying graphite from the deuterium-fueled plasma so as to minimize hydrogen release. In conclusion, an operational maneuver whereby a diverted plasma is repetitively switched from an upper single null configuration to a lower single null configuration is presented. This switching maneuver has been shown to suppress hydrogen influx into a 35s-long EAST discharge by alternately mitigating the rise in divertor temperature.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗