Nasa developments in cobalt-base superalloys

Abstract

Chemical, mechanical and physical properties of cobalt-refractory-metal superalloys for high temperature aerospace applications

Explore related subjects

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Ashbrook, R. L., Freche, J. C., Sandrock, G. D.. 1964-10-05. Nasa developments in cobalt-base superalloys. https://ntrs.nasa.gov/citations/19650019794

Cite the original work for its findings. Save a collection to share your selection of sources.

KEEP EXPLORING

Related reports

Development of high temperature nickel-base alloys for jet engine turbine bucket applications

A program has been initiated to develop a material with superior properties at elevated temperatures for utilization in turbine blade applications. A nickel-base superalloy can provide the necessary high temperature strength by using the maximum capability of the three available strengthening mechanisms - intermetallic gamma prime precipitation (Ni3Al), solid solution strengthening with refractory and precious metals, and stable carbide formations through the addition of strong carbide forming elements. A stress rupture test at 2000 deg F and 15,000 psi was formulated to approximate the desired properties. By adding varying amounts of refractory metals (Mo, W and Ta) it was possible to statistically analyze the effects of each in a basic superalloy composition containing fixed amounts of Co, Cr, C, B, Sr, and Ni at three separate levels of AL and Ta. Metallographic analysis correlated with the mechanical properties of the alloys; those with few strengthening phases were weak and ductile and those with excessive amounts of intermetallic phases present in undesirable morphologies were brittle.

SUPERALLOY↗

Progress in superalloys

Strength and workability of high temperature nickel-base, cobalt-base, and cobalt-refractory metal superalloys

SUPERALLOY↗