NASA NTRS · 19700058276
Athermal plastic deformation in commercial purity titanium
Abstract
Commercial purity Ti athermal plastic deformation, showing anomalous behavior with temperature variations
Keep this discovery
Explore connections, maps & timelines
Monteiro, S. N., Reed-Hill, R. E., Santhanam, A. T.. 1970-01-01. Athermal plastic deformation in commercial purity titanium. https://ntrs.nasa.gov/citations/19700058276
Cite the original work for its findings. Save a collection to share your selection of sources.