Development of explosive welding procedures to fabricate channeled nozzle structures
Abstract
Research was conducted to demonstrate the feasibility of fabricating a large contoured structure with complex internal channeling by explosive welding procedures. Structures or nozzles of this nature for wind tunnel applications were designed. Such nozzles vary widely in their complexity. However, in their simplest form, they consist of a grooved base section to which a cover sheet is attached to form a series of internal cooling passages. The cover sheet attachment can be accomplished in various ways: fusion welding, brazing, and diffusion welding. The cover sheet has also been electroformed in place. Of these fabrication methods, brazing has proved most successful in producing nozzles with complex contoured surfaces and a multiplicity of internal channels.
Keep this discovery
Explore connections, maps & timelines
Pattee, H. E., Linse, V. D.. 1976-03-02. Development of explosive welding procedures to fabricate channeled nozzle structures. https://ntrs.nasa.gov/citations/19760021467
Cite the original work for its findings. Save a collection to share your selection of sources.