In search for mild corrosive, 14 different salt solutions screened in alternate-immersion tests on 3 aluminum alloys. Best results were obtained with NaCl/MgCl2 solution and with synthetic seawater (contains nearly same proportions of NaCl and MgCl2 along with precise, minute amounts of eight other salts). Because solution is less expensive than artificial seawater, it is probably preferred for future stress-corrosion-cracking (SCC) testing.