Abstract

The role of the interfacial region in determining the bond strength and durability of composite bonds is discussed. The characterization of a variety of carbon fibers including Celion 6000 using both scanning electron microscopy and X-ray photoelectron spectroscopy is discussed. The emphasis is on composite bonding, that is, the adhesive bonding between composites in contrast to fiber-matrix interaction. The primary objective of the research is the characterization of composite surfaces before adhesive bonding and after fracture of bonded specimens. Work done on the analysis of composite samples pretreated in a number of ways prior to bonding is detailed.