A new diffusion-inhibited oxidation-resistant coating for superalloys

Abstract

(Previously announced in STAR as N81-33273)

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Gedwill, M. A., Glasgow, T. K., Levine, S. R.. 1982-01-01. A new diffusion-inhibited oxidation-resistant coating for superalloys. https://ntrs.nasa.gov/citations/19830029081