NASA NTRS · 19840008196
Surface analysis in composite bonding
Abstract
Surface analysis results for graphite fibers and for graphite reinforced composites prior to adhesive bonding and following fracture of lap shear samples are discussed.
Keep this discovery
Explore connections, maps & timelines
Messick, D. L., Wightman, J. P.. 1983-12-01. Surface analysis in composite bonding. https://searchnasa.com/record/nasa%3A19840008196/surface-analysis-in-composite-bonding