NASA NTRS · 19850062621
PM superalloys - A troubled adolescent?
Abstract
The history of powder metallurgy P/M superalloy technology is reviewed with a comment on the state of the art, and speculates on the technology's future potential growth and maturity.
Keep this discovery
Explore connections, maps & timelines
Dreshfield, R. L., Gray, H. R.. 1985-03-01. PM superalloys - A troubled adolescent?. https://ntrs.nasa.gov/citations/19850062621