Lanthanum sulfides as high temperature thermoelectric materials
Abstract
Thermoelectric property measurements have been made for the nonstoichiometric lanthanum sulfides, LaS(R) with R in the range 1.33-1.50. The Seebeck coefficients and electrical resistivities increase with temperature from 200 to 1100 C. Power factors (defined as Seebeck coefficient squared divided by electrical resistivity) generally increase both as the temperature is increased and as the compound composition is varied from LaS(1.48) to LaS(1.35). The power factor values combined with estimates of thermal conductivities for LaS(1.38) and LaS(1.4) yield figures of merit greater than 0.0005 at 1000 C.
Keep this discovery
Explore connections, maps & timelines
Danielson, L. R., Matsuda, S., Raag, V.. 1984-01-01. Lanthanum sulfides as high temperature thermoelectric materials. https://ntrs.nasa.gov/citations/19850063349