Lattice parameter variations during aging in nickel-base superalloys

Abstract

The importance of the state of coherency on measurements of gamma/gamma-prime lattice mismatch has been experimentally demonstrated during aging at 1000 C of specimens of an alloy with composition Ni-(8.6)Cr-(5.3)Al-(10.1)Co-(11.7)W-(1.2)Ti-(0.7)Mo (wt pct). Lattice parameter measurements are given as a function of aging time, and the corresponding sample microstructures are presented. The results show that changes of the two phases during aging did not influence the lattice parameter measurements, indicating that aging specimens to produce a semicoherent gamma/gamma-prime structure provides a good approximation of the true, unconstrained lattice mismatch.

Keep this discovery

Explore connections, maps & timelines

BibTeXRIS

Nathal, M. V., Mackay, R. A., Garlick, R. G.. 1988-09-01. Lattice parameter variations during aging in nickel-base superalloys. https://ntrs.nasa.gov/citations/19880064091

Cite the original work for its findings. Save a collection to share your selection of sources.